Green Preparation of Thermochromic Starch-Based Fibers through a Wet-Spinning Process AITranslate
Abstract AITranslate
A starch-graft-poly(butyl acrylate/styrene) (St-g-PBAS) copolymer was synthesized via grafting butyl acrylate (BA) and styrene (S) monomers onto starch by radical polymerization, and ammonium persulfate (APS) was used as an initiator. Thermochromic St-g-PBAS fibers with a full core structure were achieved through a wet-spinning process via coagulating a dope-dyed St-g-PBAS/dimethylacetamide (DMAc) solution in water. The effects of spinning conditions such as temperature and the drawing rate in a coagulation bath, drawing and stretching multiples of the primary fiber in hot water, thermal setting temperature, and time on the finished fiber mechanical performances were examined. The St-g-PBAS copolymer was analyzed by Fourier transform infrared spectra (FT-IR), solid-state nuclear magnetic resonance (13C NMR), thermal gravimetric analysis (TG), and X-ray photoelectron spectroscopy (XPS). The fiber performances were characterized by a scanning electron microscope (SEM), X-ray diffraction (XRD), and a fiber mechanical determinator. The results showed that the substitution degree of starch was 0.51, and the obtained St-g-PBAS fiber had the full core structure and excellent mechanical performances with high breaking strength (up to 2.11 cN·dtex–1), thermal stability, and elasticity (breaking elongation of up to 88.2%). The fiber color changes repeatedly between purple and pink as the temperature increases and then decreases to 31 °C.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01194
Chinese Library Classification Number:
Citation Information:
A starch-graft-poly(butyl acrylate/styrene) (St-g-PBAS) copolymer was synthesized via grafting butyl acrylate (BA) and styrene (S) monomers onto starch by radical polymerization, and ammonium persulfate (APS) was used as an initiator. Thermochromic St-g-PBAS fibers with a full core structure were achieved through a wet-spinning process via coagulating a dope-dyed St-g-PBAS/dimethylacetamide (DMAc) solution in water. The effects of spinning conditions such as temperature and the drawing rate in a coagulation bath, drawing and stretching multiples of the primary fiber in hot water, thermal setting temperature, and time on the finished fiber mechanical performances were examined. The St-g-PBAS copolymer was analyzed by Fourier transform infrared spectra (FT-IR), solid-state nuclear magnetic resonance (13C NMR), thermal gravimetric analysis (TG), and X-ray photoelectron spectroscopy (XPS). The fiber performances were characterized by a scanning electron microscope (SEM), X-ray diffraction (XRD), and a fiber mechanical determinator. The results showed that the substitution degree of starch was 0.51, and the obtained St-g-PBAS fiber had the full core structure and excellent mechanical performances with high breaking strength (up to 2.11 cN·dtex–1), thermal stability, and elasticity (breaking elongation of up to 88.2%). The fiber color changes repeatedly between purple and pink as the temperature increases and then decreases to 31 °C.
quote
| GB/T 7714-2015 | [1] Linlin Chang, Fangjun Wang, Yanzhu Guo, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01194. |
| MLA | [1] Linlin Chang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01194. |
| APA | [1] Linlin Chang, Fangjun Wang, Yanzhu Guo, Jiawen Li, Yumei Gong, & Qiang Shi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01194 |
| IEEE | [1] Linlin Chang, Fangjun Wang, Yanzhu Guo, Jiawen Li, Yumei Gong, and Qiang Shi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01194. keywords: {starchgraftbutyl acrylate/styrene;thermochromic biomass fiber;wet spinning;green preparation;starchbased fiber} |