All-Polymeric Thin-Film Nanocomposite Membrane for Organic Solvent Nanofiltration AITranslate
Abstract AITranslate
The fabrication of chemically stable and high-permeance polymeric membranes, compatible with both polar and nonpolar solvents, for use in solvent filtration is reported. Herein, poly(divinylbenzene-co-perfluorodecyl acrylate) (poly(DVB-co-PFDA) nanoparticles (NPs) are synthesized and integrated into the active layer of a thin-film composite membrane, constructing a thin-film nanocomposite (TFN) membrane. The TFN membranes demonstrate stability in organic solvent and exhibit permeance in the range 13.7 L/(m2 h bar) for acetonitrile, with a molecular weight cutoff of ∼328 Da for the solute. The use of polymeric NPs, compatible with the polyamide layer of the membranes, is the main reason behind the improved performance.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01291
Chinese Library Classification Number:
Citation Information:
The fabrication of chemically stable and high-permeance polymeric membranes, compatible with both polar and nonpolar solvents, for use in solvent filtration is reported. Herein, poly(divinylbenzene-co-perfluorodecyl acrylate) (poly(DVB-co-PFDA) nanoparticles (NPs) are synthesized and integrated into the active layer of a thin-film composite membrane, constructing a thin-film nanocomposite (TFN) membrane. The TFN membranes demonstrate stability in organic solvent and exhibit permeance in the range 13.7 L/(m2 h bar) for acetonitrile, with a molecular weight cutoff of ∼328 Da for the solute. The use of polymeric NPs, compatible with the polyamide layer of the membranes, is the main reason behind the improved performance.
quote
| GB/T 7714-2015 | [1] Syed Ibrahim Gnani Peer Mohamed, Siamak Nejati, Mona Bavarian. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01291. |
| MLA | [1] Syed Ibrahim Gnani Peer Mohamed, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01291. |
| APA | [1] Syed Ibrahim Gnani Peer Mohamed, Siamak Nejati, & Mona Bavarian. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01291 |
| IEEE | [1] Syed Ibrahim Gnani Peer Mohamed, Siamak Nejati, and Mona Bavarian, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01291. keywords: {hydrophobic;polymer nanoparticles;thinfilm composite;solvent;free radical precipitation polymerization} |