daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Abrasive Wear Resistance of Ultra-fine Structured WC-12Co Coating Deposited by HVOF AITranslate

Chongyi Zhangyuan Tungsten Co.,Ltd.;Jiangxi Institute of Tungstenand Rare Earth;Institute of Engineering &Research,Jiangxi Universityof Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using spherical shell shaped WC-12 Co composite powder prepared by spray conversion as raw materials,ultra-fine structured WC-12 Co coating was prepared on 45#steel substrate by high velocity oxygen-fuel(HVOF)spray.The microhardness and fracture toughness of the coating were investigated.The phases,microstructure and wear resistance of the coating were analyzed by XRD,SEM and wear testing machine.The results indicate that moderate decarbonization reaction of WC-12 Co composite powder with porous spherical shell occurs during HVOF spraying.The coating contains not only WC and W2C phases,but also a small amount of W phase.The coating is highly densified and shows rock stratum structure,with average microhardness HV0.3 and fracture toughness of 1 205.5 and 4.96 MPa·m^1/2,respectively.During wearing,the binding phase of the coating is ploughed by SiO2 to form discrete grooves,and the fine WC grains from stripping and cracking of WC grains become new abrasives,which grind coarse grains or accumulate in cracks to aggravate cracking.

KeyWords AITranslate

spherical shell shaped WC-12 Co composite powder HVOF coating abrasive wear

1裴延波,陈浩,王长江,战晓溪.WC-Co涂层的发展现状与展望[J].石油化工腐蚀与防护,2011,28(1):1-4. 被引量:24

2路阳,丁明辉,王智平,王玉波,杨效田,周晶晶.超音速火焰喷涂研究与应用[J].材料导报,2011,25(19):127-130. 被引量:22

3鲍君峰,崔颖,侯玉柏,张康.超音速热喷涂技术的发展与现状[J].热喷涂技术,2011,3(4):18-21. 被引量:22

4周克崧,邓春明,刘敏.超音速火焰喷涂WC涂层替代电镀硬铬:疲劳和摩擦磨损性能[J].中国工程科学,2009,11(10):48-54. 被引量:25

5羊建高,吕健,朱二涛,陈颢,郭圣达.连续还原碳化法制备纳米WC-Co复合粉研究[J].有色金属科学与工程,2013,4(5):23-27. 被引量:24

6羊求民,羊建高,苏伟,陈丽勇,陈颢,郭圣达.纳米/超细晶WC-Co类硬质合金的研究进展[J].稀有金属与硬质合金,2018,46(1):76-83. 被引量:18

7文彦,张钦英,郭圣达,苏伟,黄柱,陈颢.WC-6Co硬质合金SPS烧结工艺[J].有色金属科学与工程,2017,8(3):74-78. 被引量:11

8郭圣达,鲍瑞,刘亮,杨平,易健宏,羊建高,陈颢.原位合成复合粉制备超细WC-Co硬质合金[J].稀有金属材料与工程,2017,46(12):3977-3982. 被引量:7

9吴杰,王忠华,尚根峰,羊建高,刘芳,吕健.喷雾转换法制备超细晶WC-12Co复合粉末HVOF涂层性能研究[J].稀有金属与硬质合金,2017,45(2):39-44. 被引量:2

10李松林,向锦涛,周伍喜,李玉玺,陈文.超音速火焰喷涂WC-10Co4Cr涂层的耐滑动磨损行为[J].中国有色金属学报,2012,22(5):1371-1376. 被引量:24

1易健宏,郭圣达,鲍瑞,张家敏,羊建高.超细晶碳化钨-钴复合粉短流程制备工艺研究[J].硬质合金,2018,35(5):305-314.

2宋娓娓,蒲家飞,刘胜荣,汪洪峰.6082铝合金磨损性能分析[J].邵阳学院学报:自然科学版,2019,16(4):52-56. 被引量:3

3杨宁,李立凯.激光熔覆(V2O5+WO3+C)/Ni60涂层的磨损性能研究[J].稀有金属与硬质合金,2019,47(4):54-57.

4张建龙,刘雪梅,宋晓艳,王海滨,刘兴伟,侯超.纳米及亚微米复合粉添加对超粗晶硬质合金晶粒长大的影响及机制[J].稀有金属材料与工程,2019,48(2):552-558. 被引量:7

5聂荣国,蔡明杰,毛良杰,何军,郑莉.钻井液中纳米SiO2含量对套管摩擦学性能的影响[J].机械设计与研究,2019,35(4):163-167. 被引量:4

6王玉香,文小强,袁德林.共沉淀-喷雾干燥法制备超细WC-Co复合粉的研究[J].世界有色金属,2019,0(6):174-175. 被引量:1

7金一兰.浅谈初中语文非连续文本阅读指导研究[J].新智慧,2019,0(15):128-128. 被引量:1

8王大锋,马冰,陈东高,马良超,刘红伟,吴进明.WC晶体结构特征对HVOF喷涂纳米结构WC-CoCr涂层组织及性能的影响[J].中国表面工程,2019,32(1):88-97. 被引量:8

9闫岸如,刘学胜,王智勇,贺定勇.W含量对选区激光熔化W-Cu组织与热物性的影响[J].中国激光,2019,46(7):125-135.

10丁述宇,马国政,丁发军,王海斗,吴治永,徐滨士.等离子喷涂过程基体温度场分布的数值模拟[J].中国表面工程,2019,32(2):98-108. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG154.5[金属学及工艺—热处理]

Citation Information:

Using spherical shell shaped WC-12 Co composite powder prepared by spray conversion as raw materials,ultra-fine structured WC-12 Co coating was prepared on 45#steel substrate by high velocity oxygen-fuel(HVOF)spray.The microhardness and fracture toughness of the coating were investigated.The phases,microstructure and wear resistance of the coating were analyzed by XRD,SEM and wear testing machine.The results indicate that moderate decarbonization reaction of WC-12 Co composite powder with porous spherical shell occurs during HVOF spraying.The coating contains not only WC and W2C phases,but also a small amount of W phase.The coating is highly densified and shows rock stratum structure,with average microhardness HV0.3 and fracture toughness of 1 205.5 and 4.96 MPa·m^1/2,respectively.During wearing,the binding phase of the coating is ploughed by SiO2 to form discrete grooves,and the fine WC grains from stripping and cracking of WC grains become new abrasives,which grind coarse grains or accumulate in cracks to aggravate cracking.

quote

GB/T 7714-2015 [1] WU Jie, WANG Zhong-hua, LV Jian. Abrasive Wear Resistance of Ultra-fine Structured WC-12Co Coating Deposited by HVOF[J]. Rare Metals and Cemented Carbides, 2019(4): 24-29.
MLA [1] WU Jie, et al., "Abrasive Wear Resistance of Ultra-fine Structured WC-12Co Coating Deposited by HVOF." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 24-29.
APA [1] WU Jie, WANG Zhong-hua, & LV Jian. (2019). Abrasive Wear Resistance of Ultra-fine Structured WC-12Co Coating Deposited by HVOF. Rare Metals and Cemented Carbides(4), 24-29.
IEEE [1] WU Jie, WANG Zhong-hua, and LV Jian, "Abrasive Wear Resistance of Ultra-fine Structured WC-12Co Coating Deposited by HVOF," Rare Metals and Cemented Carbides, no. 4, pp. 24-29, 2019. keywords: {spherical shell shaped WC-12 Co composite powder;HVOF;coating;abrasive wear}