Experimental Process and Kinetics Research of Silicon Extraction from the Residue after Titanium Extraction by Alkali Leaching AITranslate
Abstract AITranslate
A large amount of silicon exists in the residue after titanium extraction from titanium-rich residue by ammonium bisulfate roasting.The effects of various parameters in the experimental process of extracting silicon from the residue after caustic alkali leaching are systematically studied.The results show that SiO2 extraction rate can reach 78.4%under the experimental conditions of reaction temperature of 220℃,mass ratio of caustic alkali to residue of 3.5∶1,liquid-solid ratio of 5.5∶1,reaction time of 50 min and stirring speed of 400 r/min.The alkali leaching kinetic analysis results show that the reaction process is controlled by internal diffusion.The apparent activation energy of the reaction is 24.047 kJ/mol,and the kinetics equation can be expressed as 1+2(1-x)-3(1-x)^2/3=2.415 exp[-24 047/(RT)]·t.
KeyWords AITranslate
1隋丽丽,翟玉春.浓硫酸焙烧钛渣提钛后的滤渣提硅实验研究[J].稀有金属与硬质合金,2016,44(4):28-31. 被引量:3
2牟文宁,陆修远,崔富晖,罗绍华,翟玉春.低品位红土镍矿预焙烧-碱浸过程中硅的转化和浸出动力学(英文)[J].中国有色金属学报:英文版,2018,28(1):169-176. 被引量:12
3朱晓波,管学茂,李望.赤泥酸浸提钛实验研究[J].稀有金属与硬质合金,2015,43(2):11-13. 被引量:22
4戚海平,张印民,张永锋,孙俊民,郝志飞.微硅粉碱溶脱硅及其反应动力学[J].环境工程学报,2017,11(4):2475-2480. 被引量:3
5贺实月,李会泉,李少鹏,李勇辉,解强.煤粉炉高铝粉煤灰碱溶脱硅反应动力学[J].中国有色金属学报,2014,24(7):1888-1894. 被引量:20
6李海兰,李娜丽.钛渣综合利用研究进展[J].贵阳学院学报:自然科学版,2017,12(4):56-59. 被引量:1
7朱晓波,李望,管学茂.柠檬酸助浸提取赤泥中钛的动力学(英文)[J].中国有色金属学报:英文版,2015,25(9):3139-3145. 被引量:10
1张永禄,尹飞,揭晓武,阮书锋,王振文.碱循环浸出法分离废旧锂离子电池中铝的研究[J].有色金属:冶炼部分,2018(12):22-26. 被引量:9
2熊庆丰,范兴祥,余宇楠,刘琼,刘振楠,姚春玲.用氢氧化钠从银渣中浸出硒碲试验研究[J].湿法冶金,2017,36(4):281-284. 被引量:2
3刘燕,肖付刚,谢文佳,薄尤优.预制肉中硝酸盐亚硝酸盐测定方法优化研究[J].食品与营养科学,2019,8(1):95-102.
4姚夏妍,鲁兴武,程亮,李俞良,李彦龙,李守荣,郁青春.氧化碱浸分离黑铜泥中砷的研究[J].有色金属工程,2019,9(6):43-47. 被引量:7
5Xufei Fang.裂纹前应力辅助晶界氧化机理的修正[J].钢铁译文集,2019,0(1):24-27.
6任娜,孙慧,王聪慧,赵卓,魏微.中孔炭对葡萄叶中白藜芦醇静态吸附性能的研究[J].应用化工,2019,48(8):1795-1799.
7孙玉成,董佳佳.阐释、描述与呈现:人类学语境下的动画实践[J].当代电影,2019(9):19-22. 被引量:2
8刘红玲.空气预热器腐蚀积灰问题探讨[J].能源研究与管理,2019,0(3):33-35. 被引量:7
9王洪亮,尹亚平.锌浸出渣回转窑处理尾气吸收剂的选择[J].世界有色金属,2019,0(11):7-8.
10王佳敏,魏剑,陈甜甜,张昊.一步法合成银纳米线及应用进展[J].功能材料,2019,50(8):8001-8008.
Basic Information:
DOI:
Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]
Citation Information:
A large amount of silicon exists in the residue after titanium extraction from titanium-rich residue by ammonium bisulfate roasting.The effects of various parameters in the experimental process of extracting silicon from the residue after caustic alkali leaching are systematically studied.The results show that SiO2 extraction rate can reach 78.4%under the experimental conditions of reaction temperature of 220℃,mass ratio of caustic alkali to residue of 3.5∶1,liquid-solid ratio of 5.5∶1,reaction time of 50 min and stirring speed of 400 r/min.The alkali leaching kinetic analysis results show that the reaction process is controlled by internal diffusion.The apparent activation energy of the reaction is 24.047 kJ/mol,and the kinetics equation can be expressed as 1+2(1-x)-3(1-x)^2/3=2.415 exp[-24 047/(RT)]·t.
quote
| GB/T 7714-2015 | [1] XU Li-shuang, SUI Li-li, GE Xin, et al. Experimental Process and Kinetics Research of Silicon Extraction from the Residue after Titanium Extraction by Alkali Leaching[J]. Rare Metals and Cemented Carbides, 2019(4): 20-23. |
| MLA | [1] XU Li-shuang, et al., "Experimental Process and Kinetics Research of Silicon Extraction from the Residue after Titanium Extraction by Alkali Leaching." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 20-23. |
| APA | [1] XU Li-shuang, SUI Li-li, GE Xin, ZHAI Yu-chun, & SHAO Shuang. (2019). Experimental Process and Kinetics Research of Silicon Extraction from the Residue after Titanium Extraction by Alkali Leaching. Rare Metals and Cemented Carbides(4), 20-23. |
| IEEE | [1] XU Li-shuang, SUI Li-li, GE Xin, ZHAI Yu-chun, and SHAO Shuang, "Experimental Process and Kinetics Research of Silicon Extraction from the Residue after Titanium Extraction by Alkali Leaching," Rare Metals and Cemented Carbides, no. 4, pp. 20-23, 2019. keywords: {titanium-rich residue;caustic alkali leaching;silicon extraction;kinetics;internal diffusion;process condition} |