Effects of Sintering Process on Microstructure and Properties of Coarse Grained Cemented Carbide AITranslate

Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

WC-12%Co coarse grained cemented carbides were prepared by vacuum sintering and low pressure sintering with coarse grained WC as the raw material.The microstructure and properties of the coarse grained cemented carbides prepared by different processes were investigated by using scanning electron microscopy,optical metallographic microscopy,and microhardness,coercive force and bending strength tests.The results show that compared with vacuum sintering,low pressure sintering can improve the comprehensive performance of the coarse grained cemented carbide.As the inert gas pressure in the furnace increases from 2 MPa to 5 MPa,all the density,coercive force,hardness,flexural strength and impact toughness of the coarse grained cemented carbide have no obvious change.

KeyWords AITranslate

coarse grained cemented carbide vacuum sintering low pressure sintering microstructure property

1Sandvik Hard Materials.Technical info\understanding cemented carbide grain size. http://www.sandvik.com . 2004

1秦琴,王楠,颜子镒,田金欣,唐诗佳,杨昊栋,黄泰博.WC粗晶硬质合金摩擦性能影响因素分析[J].稀有金属与硬质合金,2021,49(5):82-86. 被引量:2

2蒋俊鹏,欧阳水林,钟志强,邱联昌,郭圣达,谭卓鹏,陈颢.不同氮气压力烧结对WC-TiC-NbC-Co硬质合金表面结构和性能的影响[J].有色金属科学与工程,2021,12(6):57-63. 被引量:1

1曹瑞军,李开深,李腾飞,何盛亚.金刚石含量对金刚石强化硬质合金耐磨性影响[J].硬质合金,2022,39(3):165-171. 被引量:1

2张云龙,牛楚涵,牛广津,张宇民,李启荣,高志杨,张唯一.La_(2)O_(3)掺杂量对WC-12Co硬质合金微观结构和硬度的影响[J].中国钨业,2022,37(2):53-59.

3曾湘华,汤昌仁,梁瑜,刘恒嵩,鄢志刚,林森.烧结碳气氛对CVD涂层刀片基体脱β层厚度的影响[J].中国钨业,2023,38(1):37-43.

1杨胜,顾金宝,廖军,陈洪霞.烧结压力对WC-12%Co粗晶硬质合金组织及性能的影响[J].稀有金属与硬质合金,2015,43(2):54-58.

2吴迪,熊志翔,白英龙,果世驹,杨霞,徐红霞.铸造碳化钨反应烧结制备粗晶硬质合金[J].粉末冶金材料科学与工程,2011,16(4):471-477. 被引量:3

3聂洪波.超粗晶WC-Co硬质合金的制备方法与机理及性能研究[J].中国钨业,2016,31(4):51-57. 被引量:10

4郭圣达,羊建高,黄海平,许方,胡咏梅,郑彪华.粗晶硬质合金硬度和强度影响因素的分析研究[J].稀有金属与硬质合金,2012,40(4):56-58. 被引量:10

5谢宏,肖逸锋,贺跃辉,丰平,黄自谦.低压烧结对硬质合金组织和性能的影响[J].中国钨业,2006,21(6):27-31. 被引量:25

6李勇,谢淑华.WC粗晶硬质合金的研究进展[J].材料研究与应用,2009,3(2):77-80. 被引量:12

7罗斌辉,张华明.生产优质粗颗粒WC的工艺研究[J].稀有金属与硬质合金,2008,36(1):38-41. 被引量:1

8程鑫,张立.热处理对粗晶WC-Co硬质合金力学性能的影响[J].稀有金属与硬质合金,2012,40(2):45-47. 被引量:8

9陈芃,李海坤.硬质合金高温处理回收工艺研究[J].硬质合金,2001,18(4):201-203. 被引量:13

10张立,程鑫,陈述,马鋆,吴厚平,熊湘君.Cr、V、RE添加剂对特粗晶与超粗晶硬质合金微观组织与性能的影响[J].中国有色金属学报,2012,22(9):2620-2625. 被引量:9

Basic Information:

DOI:

Chinese Library Classification Number:TF124.5[冶金工程—粉末冶金]

Citation Information:

WC-12%Co coarse grained cemented carbides were prepared by vacuum sintering and low pressure sintering with coarse grained WC as the raw material.The microstructure and properties of the coarse grained cemented carbides prepared by different processes were investigated by using scanning electron microscopy,optical metallographic microscopy,and microhardness,coercive force and bending strength tests.The results show that compared with vacuum sintering,low pressure sintering can improve the comprehensive performance of the coarse grained cemented carbide.As the inert gas pressure in the furnace increases from 2 MPa to 5 MPa,all the density,coercive force,hardness,flexural strength and impact toughness of the coarse grained cemented carbide have no obvious change.

quote

GB/T 7714-2015 [1] CHEN Hong-xia, XUE Lin, GU Jin-bao, et al. Effects of Sintering Process on Microstructure and Properties of Coarse Grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2015(5): 64-67 71.
MLA [1] CHEN Hong-xia, et al., "Effects of Sintering Process on Microstructure and Properties of Coarse Grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 5, 2015, pp. 64-67 71.
APA [1] CHEN Hong-xia, XUE Lin, GU Jin-bao, YANG Sheng, & YUAN Ming-jian. (2015). Effects of Sintering Process on Microstructure and Properties of Coarse Grained Cemented Carbide. Rare Metals and Cemented Carbides(5), 64-67 71.
IEEE [1] CHEN Hong-xia, XUE Lin, GU Jin-bao, YANG Sheng, and YUAN Ming-jian, "Effects of Sintering Process on Microstructure and Properties of Coarse Grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 5, pp. 64-67 71, 2015. keywords: {coarse grained cemented carbide;vacuum sintering;low pressure sintering;microstructure;property}