Study on Environment-friendly Vanadium Extraction Process by Roasting with Composite Additives and Leaching with Dilute Acid AITranslate
Abstract AITranslate
Vanadium was extracted by roasting with composite additives and leaching with dilute acid.Impacts were investigated of composite additive dosage,roasting temperature,roasting duration,sulfuric acid dosage,leaching duration,leaching temperature and liquid-solid ratio on vanadium leaching rate.The results show that under the conditions of composite additive dosage 6%,roasting temperature 800 ℃,roasting duration 3h,sulfuric acid dosage 3%,leaching duration 3h,leaching temperature 60℃and liquid-solid ratio 3∶1,the vanadium leaching rate of the above process is85.6%,increased by 13.4%compared with that of calcification roasting process.This technology has a good application prospect as an environment-friendly process with less off-gas pollution during roasting and substantially improved vanadium leaching rate.
KeyWords AITranslate
1余唐霞,曹婧,温婧,孙红艳,姜涛.钒渣钙化焙烧添加剂选择及工艺优化[J].材料与冶金学报,2020,19(3):176-184. 被引量:5
2邱玉超,石俊杰,余彬,肖攀,赵斐,马文远,李建中,刘常升.转炉钒渣提钒技术研究现状及展望[J].化工进展,2021,40(10):5281-5292.
1邱玉超,石俊杰,余彬,肖攀,赵斐,马文远,李建中,刘常升.转炉钒渣提钒技术研究现状及展望[J].化工进展,2021,40(10):5281-5292.
2高慧阳,张杰.响应曲面法优化钒渣微波钙化焙烧提钒工艺[J].盐城工学院学报:自然科学版,2021,34(4):1-6.
3余唐霞,温婧,孙红艳,李芳芳,姜涛.不同钙含量钒渣的物相结构对钙化提钒的影响[J].钢铁钒钛,2021,42(5):18-23. 被引量:1
4赵笑益,王望泊,程倩,王勇,宁新霞,王思颖.石煤高温熟化-柱浸提钒工艺研究[J].稀有金属与硬质合金,2022,50(4):1-6.
5胡可,韩慧果,吴潘,何坚,蒋炜,刘长军,梁斌.胺萃取耦合CO_(2)矿化分离钒渣钙化焙烧酸浸液中钒锰[J].钢铁钒钛,2023,44(3):9-15.
1刘志强,朱薇,陈怀杰.从含稀有金属炉渣中富集稀有金属的研究[J].有色金属:冶炼部分,2015(3):41-43.
2李兰杰,陈东辉,白瑞国,刘雅健,王少伟,陈育红.钒渣空白焙烧高效清洁提钒技术[J].河北冶金,2014(12):29-33. 被引量:10
3林海玲,范必威,庾化龙,张云.石煤中影响钒转浸率的主要因素研究[J].成都理工学院学报,1999,26(3):317-320. 被引量:19
4狄聚才.锌冶炼系统处理炼铅含镉烟尘的生产实践[J].中国有色冶金,2010,39(5):25-27. 被引量:11
5畅永锋,翟秀静,符岩,张廷安.稀酸浸出还原焙烧红土矿时铁还原度对浸出的影响[J].东北大学学报:自然科学版,2008,29(12):1738-1741. 被引量:3
6赵富平,李春雷.阜康冶炼厂浸铜后渣加压浸出工艺探讨[J].新疆有色金属,2003,26(S2):43-44. 被引量:2
7专利信息[J].黄金科学技术,2009,17(3):70-70.
8郑诗礼,杜浩,王少娜,张懿,陈东辉,白瑞国.亚熔盐法钒渣高效清洁提钒技术[J].钢铁钒钛,2012,33(1):15-19. 被引量:33
9余德麒,施正伦,肖文丁,李戈跃,骆仲泱,岑可法.石煤灰渣二次焙烧稀酸浸出提钒工艺条件[J].过程工程学报,2010,10(4):673-678. 被引量:10
10蔡晋强,龚加齐,郑越,姚玉梅.硫酸铵焙烧法从石煤钒矿中提取钒和铝的试验研究[J].稀有金属与硬质合金,2013,41(4):1-4. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Vanadium was extracted by roasting with composite additives and leaching with dilute acid.Impacts were investigated of composite additive dosage,roasting temperature,roasting duration,sulfuric acid dosage,leaching duration,leaching temperature and liquid-solid ratio on vanadium leaching rate.The results show that under the conditions of composite additive dosage 6%,roasting temperature 800 ℃,roasting duration 3h,sulfuric acid dosage 3%,leaching duration 3h,leaching temperature 60℃and liquid-solid ratio 3∶1,the vanadium leaching rate of the above process is85.6%,increased by 13.4%compared with that of calcification roasting process.This technology has a good application prospect as an environment-friendly process with less off-gas pollution during roasting and substantially improved vanadium leaching rate.
quote
| GB/T 7714-2015 | [1] CAI Jun, YAN Wen-bin, HUA Jun, et al. Study on Environment-friendly Vanadium Extraction Process by Roasting with Composite Additives and Leaching with Dilute Acid[J]. Rare Metals and Cemented Carbides, 2015(4): 10-12 33. |
| MLA | [1] CAI Jun, et al., "Study on Environment-friendly Vanadium Extraction Process by Roasting with Composite Additives and Leaching with Dilute Acid." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 10-12 33. |
| APA | [1] CAI Jun, YAN Wen-bin, HUA Jun, GAO Feng, YI Jing, & HE Xin-bo. (2015). Study on Environment-friendly Vanadium Extraction Process by Roasting with Composite Additives and Leaching with Dilute Acid. Rare Metals and Cemented Carbides(4), 10-12 33. |
| IEEE | [1] CAI Jun, YAN Wen-bin, HUA Jun, GAO Feng, YI Jing, and HE Xin-bo, "Study on Environment-friendly Vanadium Extraction Process by Roasting with Composite Additives and Leaching with Dilute Acid," Rare Metals and Cemented Carbides, no. 4, pp. 10-12 33, 2015. keywords: {environment-friendly vanadium extraction;composite additive;roasting;acid leaching} |