Study on Influence of Fe3+ on Spodumene Flotation and its Mechanism AITranslate
Abstract AITranslate
Influences of Fe3+on spodumene flotation and its mechanism were systematically studied through flotation tests of pure spodumene,measurement of electric potential,infrared spectrum test and Fe3+solution chemical analysis.The results indicate that the flotation recovery of spodumene is significantly increased with the addition of Fe3+.The surface potential of spodumene significantly shifts after activated by Fe3+and then interacting with the collector,proving that Fe3+is absorbed strongly on the surface of spodumene.IR characteristic absorption peaks of oleic in spodumene are remarkably enhanced after activated by Fe3+and then interacting with the collector,indicating that the addition of Fe3+contributes to the adsorption of oleic acid on spodumene surface.
KeyWords AITranslate
1闻 辂等编著.矿物红外光谱学[M]. 重庆出版社, 1989
2WANG Yu-hua YU Fu-shun.Effects of Metallic Ions on the Flotation of Spodumene and Beryl[J].中国矿业大学学报:英文版,2007,17(1):35-39. 被引量:27
1闫克勤.贵州某锂辉石矿石选矿试验[J].金属矿山,2018,47(11):95-97. 被引量:2
2李金林,刘丹,王伊杰,文书明,夏节.锂辉石浮选机理研究现状[J].硅酸盐通报,2016,35(8):2400-2406. 被引量:14
3李慧,何廷树,王宇斌,王真,袁航.铁离子对辉钼矿表面性质及可浮性的影响机理研究[J].有色金属工程,2018,8(1):89-92. 被引量:5
4巫侯琴,方帅,徐龙华,田佳,陈海焱.伟晶岩型锂辉石矿石浮选药剂及工艺研究现状[J].金属矿山,2018,47(7):1-6. 被引量:6
5董栋,程宏伟,郭保万,何兰军.锂辉石选矿技术现状及展望[J].矿产保护与利用,2018,38(4):130-134. 被引量:17
6郑海涛,王毓华,赵悦豪,朱广丽,卢东方,郑霞裕.NaOH和机械搅拌对锂辉石表面及浮选行为的影响[J].有色金属工程,2019,9(6):61-68. 被引量:3
7徐龙华,方帅,巫侯琴.氧化矿表面改性调控浮选分离的研究综述[J].贵州大学学报:自然科学版,2020,37(2):1-6. 被引量:7
8冯海强,王毓华.锂辉石浮选捕收剂及其构效关系研究综述[J].稀有金属,2022,46(8):1083-1096. 被引量:1
1He-Peng Zhou,Jie Hu,Yong-Bing Zhang,Yi-Jun Cao,Xian-Ping Luo,Xue-Kun Tang.Effectively enhancing recovery of fine spodumene via aggregation flotation[J].稀有金属:英文版,2020,0(3):316-326. 被引量:4
2蒋双宇,曹浩然,李祖龙.川西地区锂资源的工业应用及开发利用探讨[J].内蒙古石油化工,2020(12):1-4.
3程仁举,李成秀,刘星,王昌良,徐莺.川西某低品位锂辉石矿分选试验研究[J].有色金属:选矿部分,2017(5):42-45. 被引量:15
4刘若华,孙伟,冯木,梅志,金娇.新型捕收剂浮选锂辉石的作用机理研究[J].有色金属:选矿部分,2018(2):87-90. 被引量:11
5董栋,程宏伟,郭保万,何兰军.锂辉石选矿技术现状及展望[J].矿产保护与利用,2018,38(4):130-134. 被引量:17
6马倩倩.金属阳离子在锂辉石浮选中的影响[J].中国粉体工业,2019,0(1):4-7.
7郑海涛,王毓华,赵悦豪,朱广丽,卢东方,郑霞裕.NaOH和机械搅拌对锂辉石表面及浮选行为的影响[J].有色金属工程,2019,9(6):61-68. 被引量:3
8袁航,何廷树,李慧,王宇斌.Ca2+在粗细粒辉钼矿表面吸附及对可浮性影响[J].有色金属工程,2019,9(8):59-65. 被引量:2
9朱一民,周菁.2018年浮选药剂的进展[J].矿产综合利用,2019,0(4):1-10. 被引量:7
10陈勇,常宝乾,李恒,阳建国.澳大利亚某锂辉石矿石浮选试验[J].金属矿山,2019,0(9):87-91. 被引量:1
1徐振洪,李溪.起泡剂对水-煤界面性质的影响[J].煤炭科学技术,1998,26(12):31-33.
2代小云,张文军,罗顺发,李强,王雪伟.浮选水质硬度对煤泥润湿性及电动电位的影响[J].煤炭工程,2016,48(9):137-141. 被引量:4
3梁冰,尹小波,赵礼兵,张锦瑞.助磨剂对微细粒贫赤铁矿磨矿作用机理研究[J].水泥助磨剂与混凝土外加剂,2016,0(1):62-66.
4赵晴,闵凡飞,刘峰.石英颗粒表面电动电位影响因素及变化规律?[J].中国科技博览,2014(3):453-454.
5冯博,卢毅屏,冯其明.绿泥石/蛇纹石聚集分散及抑制行为研究[J].稀有金属,2016,40(2):167-171. 被引量:5
6谢广元,施秀屏,欧泽深,高敏.高效MN-5阳离子絮凝剂及其特性研究[J].煤炭学报,1998,23(3):332-336.
7闵凡飞,赵晴,李宏亮,彭陈亮.煤泥水中高岭土颗粒表面荷电特性研究[J].中国矿业大学学报,2013,42(2):284-290. 被引量:34
8荣葵一,彭长琪.祁连温石棉性能及利用方向[J].非金属矿,1997(2):40-43.
9李桂芹.分散剂在铁矿石细磨矿浆中分散力的测定及其作用机理[J].中国矿业,1996,5(6):49-53. 被引量:13
10袁世泉,张洪恩.菱镁矿、白云石表面电性研究[J].矿冶工程,1990,10(4):19-23. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TD923[矿业工程—选矿];TD955[矿业工程—选矿]
Citation Information:
Influences of Fe3+on spodumene flotation and its mechanism were systematically studied through flotation tests of pure spodumene,measurement of electric potential,infrared spectrum test and Fe3+solution chemical analysis.The results indicate that the flotation recovery of spodumene is significantly increased with the addition of Fe3+.The surface potential of spodumene significantly shifts after activated by Fe3+and then interacting with the collector,proving that Fe3+is absorbed strongly on the surface of spodumene.IR characteristic absorption peaks of oleic in spodumene are remarkably enhanced after activated by Fe3+and then interacting with the collector,indicating that the addition of Fe3+contributes to the adsorption of oleic acid on spodumene surface.
quote
| GB/T 7714-2015 | [1] SHI Hai-lan, ZHU Wen-long. Study on Influence of Fe3+ on Spodumene Flotation and its Mechanism[J]. Rare Metals and Cemented Carbides, 2015(4): 5-9. |
| MLA | [1] SHI Hai-lan, and ZHU Wen-long. "Study on Influence of Fe3+ on Spodumene Flotation and its Mechanism." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 5-9. |
| APA | [1] SHI Hai-lan, & ZHU Wen-long. (2015). Study on Influence of Fe3+ on Spodumene Flotation and its Mechanism. Rare Metals and Cemented Carbides(4), 5-9. |
| IEEE | [1] SHI Hai-lan and ZHU Wen-long, "Study on Influence of Fe3+ on Spodumene Flotation and its Mechanism," Rare Metals and Cemented Carbides, no. 4, pp. 5-9, 2015. keywords: {spodumene;flotation;Fe3+;electric potential;infrared spectrum} |