daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tough Polymeric Hydrogels Formed by Natural Glycyrrhetinic Acid-Tailored Host–Guest Macro-Cross-Linking toward Biocompatible Materials AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; PSL University Paris
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Host–guest polymeric hydrogels often suffer from poor biocompatibility and weak mechanical strength owing to the low complexation degree between host and guest polymers. In contrast to reported works, here a biocompatible host–guest macro-cross-linker (HGMC) was synthesized beforehand by complexation of poly(β-cyclodextrin) with natural glycyrrhetinic acid-derivative functionalized with acrylates at two extremities. After cross-linking polyacrylamide, three polymeric hydrogels were obtained, the swelling ratios and micropore sizes of which could be adjusted effectively by HGMC content. Moreover, they exhibited robust anticompressing and elastic features. These biocompatible tough polymeric hydrogels hold promise for potential applications as biomaterials.

KeyWords AITranslate

polymeric hydrogel host−guest pairs cyclodextrins glycyrrhetinic acid natural product
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00723

Chinese Library Classification Number:

Citation Information:

Host–guest polymeric hydrogels often suffer from poor biocompatibility and weak mechanical strength owing to the low complexation degree between host and guest polymers. In contrast to reported works, here a biocompatible host–guest macro-cross-linker (HGMC) was synthesized beforehand by complexation of poly(β-cyclodextrin) with natural glycyrrhetinic acid-derivative functionalized with acrylates at two extremities. After cross-linking polyacrylamide, three polymeric hydrogels were obtained, the swelling ratios and micropore sizes of which could be adjusted effectively by HGMC content. Moreover, they exhibited robust anticompressing and elastic features. These biocompatible tough polymeric hydrogels hold promise for potential applications as biomaterials.

quote

GB/T 7714-2015 [1] Ge Xu, Jiawei Li, Jianqiao Wu, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00723.
MLA [1] Ge Xu, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00723.
APA [1] Ge Xu, Jiawei Li, Jianqiao Wu, Hao Zhang, Jun Hu, & MinHui Li. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00723
IEEE [1] Ge Xu, Jiawei Li, Jianqiao Wu, Hao Zhang, Jun Hu, and MinHui Li, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00723. keywords: {polymeric hydrogel;host−guest pairs;cyclodextrins;glycyrrhetinic acid;natural product}