Cell-Laden Particulate-Composite Hydrogels with Tunable Mechanical Properties Constructed with Gradient-Interface Hydrogel Particles AITranslate
Abstract AITranslate
Hydrogels have long been studied as cell encapsulants for engineered tissue, yet diffusive limitations, suboptimal mechanical properties, and poor cell distribution limit the use of single-phase hydrogels for complex tissues scaffolds. Here, a composite hydrogel structure is presented to overcome these limitations. It is shown that oxygen inhibition during chain-growth photopolymerization of microgel particles can be used to directly manipulate the interfacial bond strength between two hydrogel interfaces in the particulate-composite hydrogels. Using this principle, a cell-laden particulate-composite hydrogel is fabricated that overcomes the low cell viability of a single-phase hydrogel, while allowing the stiffness to be arbitrarily tuned.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00606
Chinese Library Classification Number:
Citation Information:
Hydrogels have long been studied as cell encapsulants for engineered tissue, yet diffusive limitations, suboptimal mechanical properties, and poor cell distribution limit the use of single-phase hydrogels for complex tissues scaffolds. Here, a composite hydrogel structure is presented to overcome these limitations. It is shown that oxygen inhibition during chain-growth photopolymerization of microgel particles can be used to directly manipulate the interfacial bond strength between two hydrogel interfaces in the particulate-composite hydrogels. Using this principle, a cell-laden particulate-composite hydrogel is fabricated that overcomes the low cell viability of a single-phase hydrogel, while allowing the stiffness to be arbitrarily tuned.
quote
| GB/T 7714-2015 | [1] Rajib Krishna Shaha, Zhongliang Jiang, Carl P. Frick, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00606. |
| MLA | [1] Rajib Krishna Shaha, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00606. |
| APA | [1] Rajib Krishna Shaha, Zhongliang Jiang, Carl P. Frick, & John Oakey. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00606 |
| IEEE | [1] Rajib Krishna Shaha, Zhongliang Jiang, Carl P. Frick, and John Oakey, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00606. keywords: {particulatecomposite hydrogel;tissue scaffold;photopolymerization;oxygen inhibition;interfacial bonding;cell encapsulation} |