The Effects of Dual-temperature Heat Treatment on Microstructure and Mechanical Properties of Ti-Al-Cr Alloys AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of dual-temperature heat treatment on microstructure and mechanical properties of Ti-Al-Cr alloys have been studied.The results show that dual-temperature heat treatment resulted in the fine uniform duplex microstructure,ideal mechanical properties are obtained with σ b=547 MPa,σ 0.2 =632 MPa,δ=3 5%under the heat treatment at 1 290 ℃,4 h,FC→1 240 ℃,4 h,FC+900 ℃,24 h,FC.

KeyWords AITranslate

Ti-Al-Cr dual-temperature heat treatment alloy microstructure mechanical properties

1蒲忠杰,祝东,朱静,蔡其巩,邹敦叙.TiAl基金属间化合物的塑性变形行为[J].科学通报,1990,35(6):469-471. 被引量:2

1陈付时.Cr在γ—基Ti—Al—Cr合金中促进保护氧化铝成形成的作用[J].钛合金信息,1997(6):11-12.

2贺跃辉,刘业翔,黄伯云,孔高宁,曲选辉,雷长明.TiAl基合金双温热处理的研究[J].高技术通讯,1994,4(12):26-30. 被引量:7

3贺跃辉,黄伯云,陈小群,刘业翔,徐强.双温热处理TiAl基合金显微组织和相结构分析[J].电子显微学报,1997,16(1):31-38. 被引量:1

4周春根,杨颖,宫声凯,徐惠彬.Cr在Ti-Al-Cr合金抗高温氧化过程中的作用研究[J].航空学报,2001,22(1):73-77. 被引量:4

5彭超群,黄伯云,贺跃辉.热处理对TiAl基合金相变和显微组织的影响[J].材料科学与工艺,2002,10(3):331-336. 被引量:5

6孙涛,王清,耿明,孙东立,武高辉.TiAl合金片层组织的形成与细化工艺及其机理研究[J].材料热处理学报,2009,30(2):96-100. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料];TG166.5[金属学及工艺—热处理]

Citation Information:

The effects of dual-temperature heat treatment on microstructure and mechanical properties of Ti-Al-Cr alloys have been studied.The results show that dual-temperature heat treatment resulted in the fine uniform duplex microstructure,ideal mechanical properties are obtained with σ b=547 MPa,σ 0.2 =632 MPa,δ=3 5%under the heat treatment at 1 290 ℃,4 h,FC→1 240 ℃,4 h,FC+900 ℃,24 h,FC.

quote

GB/T 7714-2015 [1] ZHANG Yong-hong, HUANG Bo-yun, HE Yue-hui. The Effects of Dual-temperature Heat Treatment on Microstructure and Mechanical Properties of Ti-Al-Cr Alloys[J]. Rare Metals and Cemented Carbides, 2002(3): 1-3.
MLA [1] ZHANG Yong-hong, et al., "The Effects of Dual-temperature Heat Treatment on Microstructure and Mechanical Properties of Ti-Al-Cr Alloys." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 1-3.
APA [1] ZHANG Yong-hong, HUANG Bo-yun, & HE Yue-hui. (2002). The Effects of Dual-temperature Heat Treatment on Microstructure and Mechanical Properties of Ti-Al-Cr Alloys. Rare Metals and Cemented Carbides(3), 1-3.
IEEE [1] ZHANG Yong-hong, HUANG Bo-yun, and HE Yue-hui, "The Effects of Dual-temperature Heat Treatment on Microstructure and Mechanical Properties of Ti-Al-Cr Alloys," Rare Metals and Cemented Carbides, no. 3, pp. 1-3, 2002. keywords: {Ti-Al-Cr;dual-temperature heat treatment;alloy microstructure;mechanical properties}