Effect of Solid Solution Treatment on Mechanical Properties of Beryllium Material AITranslate

Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Effects of solid solution treatment on mechanical properties of the vacuum-hot-pressed(HP) beryllium material and the cold-hot-isostatic(HIP)beryllium material have been studied by impact grinding of the beryllium powders with stable low-oxygen air.It is shown that the mechanical properties of beryllium materials as solution are lower than that of as-pressed Be by both hot press and HIP.The lower mechanical property of solid-solution hot-pressed Be material is caused mainly by BeO aggregation due to Be 2SO 4 precipitate and also the lower Fe content in the feed,resulting in non-effective solid solution strengthening.

KeyWords AITranslate

beryllium solid solution treatment mechanical property

1[1]Carrabine J A,et al.The effects of AlFeBe4 on mechanical properties of fabricated polycrystalline beryllium[A].In:Schetki L M eds.Beryllium Technology[C].Philadephia:Gordon and Breach Science Publishers,INC,1966.1:239.

2[2]Moore A,et al.Precipitation-ageing and improved mechanical properties in commercially pure beryllium and beryllium alloys[A].In:The Institute of Metals ed.The Metallurgy of Beryllium[C].London:Chapman and Hall Ltd,1963.112.

1张青来,A.B.Bondarev,V.A.Andreev,王粒粒,胡永学.时效处理对金属铍剩余电阻比的影响[J].中国有色金属学报,2007,17(7):1124-1128. 被引量:1

2张青来,Bondarev A B,Andreev V A,王粒粒,胡永学.不同纯度金属铍热处理时剩余电阻的变化[J].稀有金属材料与工程,2007,36(8):1354-1357.

3康慧灵,何力军,许德美,钟景明,王战宏,孙本双,刘霄霞.粉末冶金多晶态铍室温断裂行为的研究进展[J].材料导报,2013,27(15):94-97. 被引量:1

4张延宾,郑侠,戴天舒.大型铍材一次脱气真空炉的研制[J].真空,2016,53(6):74-77. 被引量:1

5郑莉芳,刘新宇,鲍帅平,张健康,钟景明,丁玉龙.稀有金属铍的性能研究进展[J].稀有金属,2023,47(2):292-302.

1周民杰,罗炳池,李恺,张继成,李佳,吴卫东.Cu掺杂对Be薄膜微结构的影响(英文)[J].中国有色金属学报:英文版,2012,22(5):1151-1155.

2刘军,孙洪涛,李晖,王志萍,陈红,李娜.电感耦合等离子体原子发射光谱法测定铍中氧化铍的含量[J].理化检验:化学分册,2019,55(12):1452-1454. 被引量:3

3张乃禄,陈媛.基于模糊PID的稀有金属真空脱气温度控制系统[J].工业仪表与自动化装置,2021(6):13-16. 被引量:2

1钟景明,闵学仁,聂大钧,高洪季,付晓旭,夏洪先,王零森.冲击研磨铍粉及其材料性能[J].稀有金属材料与工程,1999,28(6):386-389. 被引量:3

2王零森,钟景明,付晓旭,王战宏,聂大钧,王学泽.晶粒尺寸对等静压铍材力学性能的影响[J].中南工业大学学报,1999,30(4):395-397. 被引量:8

3武永丽.BeO压铸模的设计[J].机械工人:热加工,1992,16(8):12-13.

4康慧灵,何力军,许德美,钟景明,王战宏,孙本双,刘霄霞.粉末冶金多晶态铍室温断裂行为的研究进展[J].材料导报,2013,27(15):94-97. 被引量:1

5张文华,李宗理,翟惠民.铍材和铍粉的X射线照相法[J].无损检测,2000,22(1):28-32. 被引量:3

6许德美,秦高梧,李峰,王东新,夏洪先,任玉平,裴文利.BeO杂质形态与分布对金属铍力学性能的影响[J].中国有色金属学报,2011,21(4):769-776. 被引量:17

7马玲,冯婷,焦旗,赵双群.粉末冶金铍铝合金的铍铝界面结构[J].热加工工艺,2013,42(4):100-102. 被引量:5

8吴梅柏,郭喜平.铌硅化物基超高温合金与石墨坩埚氧化物涂层反应的热力学分析[J].稀有金属与硬质合金,2007,35(1):5-9. 被引量:2

9谭佳梅,张鹏程,谌继明,周上祺.Be与CuCrZr中温热等静压扩散连接研究[J].核动力工程,2007(z1):61-64.

10曾小勤,王渠东,吕宜振,朱燕萍,丁文江.阻燃镁合金研究[J].铸造,1999(6):4-7. 被引量:19

Basic Information:

DOI:

Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料];TG166.7[金属学及工艺—热处理]

Citation Information:

Effects of solid solution treatment on mechanical properties of the vacuum-hot-pressed(HP) beryllium material and the cold-hot-isostatic(HIP)beryllium material have been studied by impact grinding of the beryllium powders with stable low-oxygen air.It is shown that the mechanical properties of beryllium materials as solution are lower than that of as-pressed Be by both hot press and HIP.The lower mechanical property of solid-solution hot-pressed Be material is caused mainly by BeO aggregation due to Be 2SO 4 precipitate and also the lower Fe content in the feed,resulting in non-effective solid solution strengthening.

quote

GB/T 7714-2015 [1] ZHONG Jing-ming, WANG Xue-ze, WANG Dong-xin, et al. Effect of Solid Solution Treatment on Mechanical Properties of Beryllium Material[J]. Rare Metals and Cemented Carbides, 2002(3): 4-7.
MLA [1] ZHONG Jing-ming, et al., "Effect of Solid Solution Treatment on Mechanical Properties of Beryllium Material." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 4-7.
APA [1] ZHONG Jing-ming, WANG Xue-ze, WANG Dong-xin, FU Xiao-xu, & WANG Ling-sen. (2002). Effect of Solid Solution Treatment on Mechanical Properties of Beryllium Material. Rare Metals and Cemented Carbides(3), 4-7.
IEEE [1] ZHONG Jing-ming, WANG Xue-ze, WANG Dong-xin, FU Xiao-xu, and WANG Ling-sen, "Effect of Solid Solution Treatment on Mechanical Properties of Beryllium Material," Rare Metals and Cemented Carbides, no. 3, pp. 4-7, 2002. keywords: {beryllium;solid solution treatment;mechanical property}