Determination of Isothermal Section of Ni-Ti-Si Ternary System at 1 173 K AITranslate
Abstract AITranslate
The phase equilibria in the Ni-Ti-Si ternary system at 1 173 K was investigated by using diffusion triple technique and electron microprobe analysis (EMPA).The experimental results indicate that seven diffusion layers, which are TiSi 2, TiSi, Ti 5Si 4, Ti 5Si 3, Ti 3Si, Nb 5Si 3 and NbSi 2,exist in the Ni-Ti-Si ternary system at 1 173 K,and no ternary compound was observed in the diffusion triple.A tentative isothermal section of this system at 1 173 K was constructed based on the experimental data.The isothermal section consists of six three-phase regions.
KeyWords AITranslate
1张岳兰,刘华山,金展鹏.Nb-Ti-Si 三元系相平衡的热力学计算[J].中南工业大学学报,1998,29(4):370-373. 被引量:5
1王日初,柳春雷,王冲,金展鹏.Nb-Ti-Si三元系1473K等温截面的测定[J].稀有金属材料与工程,2002,31(5):337-340.
2王日初,刘立斌.Nb—Ti—Si三元系1373K等温截面的测定[J].矿冶工程,1999,19(2):66-68.
3王日初,刘立斌,金展鹏,崔予文.Ni-Re- Ta 三元系1 473 K 等温截面的测定[J].稀有金属材料与工程,1999,28(4):222-224.
4王日初,王冲,金展鹏.Ni-Re-Ta三元系1373K等温截面的测定[J].矿冶工程,2002,22(1):82-84.
5王日初,金展鹏,柳春雷.Nb-Ti-Si三元系中化合物的形成序列[J].中南工业大学学报,2002,33(4):385-388. 被引量:2
6乔亮,苏轩,陶汪,陈彦宾,熊俊,付忠奎,鄢江武,陈建平.TC4钛合金不同焊接工艺下组织性能对比[J].热加工工艺,2016,45(3):19-22. 被引量:5
7肖来荣,李威,许谅亮,蔡圳阳,毛海军,殷傲宇.铌合金表面硅化物涂层的界面结构[J].粉末冶金材料科学与工程,2011,16(6):843-848. 被引量:8
8王日初,王冲,金展鹏.三元扩散偶中的相区分布与四相平衡的关系[J].中国有色金属学报,2002,12(4):643-647. 被引量:3
9王日初,柳春雷,王冲,金展鹏.Ni-Ta-Hf三元系等温截面的研究[J].矿冶工程,2002,22(3):120-122.
10张岳兰,刘华山,金展鹏.Nb-Ti-Si 三元系相平衡的热力学计算[J].中南工业大学学报,1998,29(4):370-373. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
The phase equilibria in the Ni-Ti-Si ternary system at 1 173 K was investigated by using diffusion triple technique and electron microprobe analysis (EMPA).The experimental results indicate that seven diffusion layers, which are TiSi 2, TiSi, Ti 5Si 4, Ti 5Si 3, Ti 3Si, Nb 5Si 3 and NbSi 2,exist in the Ni-Ti-Si ternary system at 1 173 K,and no ternary compound was observed in the diffusion triple.A tentative isothermal section of this system at 1 173 K was constructed based on the experimental data.The isothermal section consists of six three-phase regions.
quote
| GB/T 7714-2015 | [1] WANG Ri-chu, QUE Ji-rong, LIU Chun-lei, et al. Determination of Isothermal Section of Ni-Ti-Si Ternary System at 1 173 K[J]. Rare Metals and Cemented Carbides, 2002(3): 8-10. |
| MLA | [1] WANG Ri-chu, et al., "Determination of Isothermal Section of Ni-Ti-Si Ternary System at 1 173 K." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 8-10. |
| APA | [1] WANG Ri-chu, QUE Ji-rong, LIU Chun-lei, & JIN Zhan-peng. (2002). Determination of Isothermal Section of Ni-Ti-Si Ternary System at 1 173 K. Rare Metals and Cemented Carbides(3), 8-10. |
| IEEE | [1] WANG Ri-chu, QUE Ji-rong, LIU Chun-lei, and JIN Zhan-peng, "Determination of Isothermal Section of Ni-Ti-Si Ternary System at 1 173 K," Rare Metals and Cemented Carbides, no. 3, pp. 8-10, 2002. keywords: {diffusion pair;Nb-Ti-Si ternary system;tie line;phase equilibria;isothermal section} |