daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

FeSe2 Graphite Intercalation Compound as Anode Materials for Sodium Ion Batteries FeSe2 Graphite Intercalation Compound as Anode Materials for Sodium Ion Batteries AITranslate

Fujian Normal University; Haixi Institute; Haixi Institute; Haixi Institute; Haixi Institute; Fujian Normal University; Fujian Normal University; Haixi Institute; Haixi Institute; Haixi Institute; Haixi Institute; Haixi Institute
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on theoretical calculations, the molecule predominantly generated by the combination of sodium with graphite is identified as NaC186. Consequently, this compound has a relatively limited capacity for sodium storage, amounting to only 36 mA h g–1. In this study, we construct FeSe2 graphite intercalation compounds (FeSe2-GIC) by in situ inserting FeSe2 between the graphite interlayers by a hydrothermal process. The resulting FeSe2-GIC material is then subjected to ball milling to form the FeSe2-GIC-BM. The FeSe2 material was found to be tightly intercalated within the graphite layers, resulting in a limited volume expansion and improved electrical conductivity. The electrochemical test results indicate that the FeSe2-GIC-BM anode exhibits a remarkable electrochemical performance. It exhibits an initial specific discharge capacity of 676.2 mA h g–1 at a current density of 0.1 A g–1 and a specific discharge capacity of 425.0 mA h g–1 at a current density of 5 A g–1. After 1200 cycles, the observed reversible capacity remains at 182.9 mA h g–1. The exceptional storage and cycling characteristics can be attributed to the distinctive layered structure.

KeyWords AITranslate

hydrothermal synthesis ball milling graphite intercalation compound intercalated structure FeSe2
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01355

Chinese Library Classification Number:

Citation Information:

Based on theoretical calculations, the molecule predominantly generated by the combination of sodium with graphite is identified as NaC186. Consequently, this compound has a relatively limited capacity for sodium storage, amounting to only 36 mA h g–1. In this study, we construct FeSe2 graphite intercalation compounds (FeSe2-GIC) by in situ inserting FeSe2 between the graphite interlayers by a hydrothermal process. The resulting FeSe2-GIC material is then subjected to ball milling to form the FeSe2-GIC-BM. The FeSe2 material was found to be tightly intercalated within the graphite layers, resulting in a limited volume expansion and improved electrical conductivity. The electrochemical test results indicate that the FeSe2-GIC-BM anode exhibits a remarkable electrochemical performance. It exhibits an initial specific discharge capacity of 676.2 mA h g–1 at a current density of 0.1 A g–1 and a specific discharge capacity of 425.0 mA h g–1 at a current density of 5 A g–1. After 1200 cycles, the observed reversible capacity remains at 182.9 mA h g–1. The exceptional storage and cycling characteristics can be attributed to the distinctive layered structure.

quote

GB/T 7714-2015 [1] Haodong Wang, Kai Zhang, Jun Zheng, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01355.
MLA [1] Haodong Wang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01355.
APA [1] Haodong Wang, Kai Zhang, Jun Zheng, Gang Wang, Wenwu Fu, Yaowei Hao, Yafang Zhao, Xiaocao Cao, Zhiguang Lin, Jiayi Liu, Ming Zhang, & Zhongrong Shen. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01355
IEEE [1] Haodong Wang, Kai Zhang, Jun Zheng, Gang Wang, Wenwu Fu, Yaowei Hao, Yafang Zhao, Xiaocao Cao, Zhiguang Lin, Jiayi Liu, Ming Zhang, and Zhongrong Shen, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01355. keywords: {hydrothermal synthesis ball milling graphite intercalation compound intercalated structure FeSe2}