Topological Data Analysis of Nanoscale Roughness of Layer-by-Layer Polyelectrolyte Samples Using Machine Learning Topological Data Analysis of Nanoscale Roughness of Layer-by-Layer Polyelectrolyte Samples Using Machine Learning AITranslate

ITMO University; ITMO University; ITMO University; ITMO University; ITMO University;NT-MDT BV, Hoenderparkweg 96 b; University of Wisconsin Milwaukee; ITMO University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The surface roughness of layer-by-layer (LbL) polyelectrolytes is studied by atomic force microscopy (AFM) and analyzed with novel methods including topological data analysis (TDA) and machine learning (ML) to correlate multiscale roughness with the number of bilayers and to recognize the types of polyelectrolytes (PEs). LbL PEs composed of one to four bilayers of (1) polyethylenimine (PEI)/poly(sodium 4-styrenesulfonate) (PSS), (2) PEI/poly(acrylic acid) (PAA), and (3) PEI/MXene rigid flakes are deposited on a smooth silicon wafer. With a growing number of bilayers, the roughness changes from a smooth surface to an equilibrium rough profile. The AFM study of the surface morphology demonstrates that surface roughness is multiscale, with smaller features imposed on larger ones. Roughness data is filtered from measurement resolution artifacts, and several methods are applied: correlation length, statistics of the distribution of extremes in trimmed images, and TDA barcodes and persistence diagrams of simplexes in 8D data space. An ML algorithm is used to determine the number of bilayers in a PE. Roughness analysis indicates a gradual transition from a smooth to a rough surface with saturation at three to four bilayers and the existence of multiscale roughness invariance.

KeyWords AITranslate

polyelectrolytes MXene topological data analysis atomic force microscopy machine learning
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01358

Chinese Library Classification Number:

Citation Information:

The surface roughness of layer-by-layer (LbL) polyelectrolytes is studied by atomic force microscopy (AFM) and analyzed with novel methods including topological data analysis (TDA) and machine learning (ML) to correlate multiscale roughness with the number of bilayers and to recognize the types of polyelectrolytes (PEs). LbL PEs composed of one to four bilayers of (1) polyethylenimine (PEI)/poly(sodium 4-styrenesulfonate) (PSS), (2) PEI/poly(acrylic acid) (PAA), and (3) PEI/MXene rigid flakes are deposited on a smooth silicon wafer. With a growing number of bilayers, the roughness changes from a smooth surface to an equilibrium rough profile. The AFM study of the surface morphology demonstrates that surface roughness is multiscale, with smaller features imposed on larger ones. Roughness data is filtered from measurement resolution artifacts, and several methods are applied: correlation length, statistics of the distribution of extremes in trimmed images, and TDA barcodes and persistence diagrams of simplexes in 8D data space. An ML algorithm is used to determine the number of bilayers in a PE. Roughness analysis indicates a gradual transition from a smooth to a rough surface with saturation at three to four bilayers and the existence of multiscale roughness invariance.

quote

GB/T 7714-2015 [1] Aleksandr S. Aglikov, Timur A. Aliev, Mikhail V. Zhukov, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01358.
MLA [1] Aleksandr S. Aglikov, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01358.
APA [1] Aleksandr S. Aglikov, Timur A. Aliev, Mikhail V. Zhukov, Anna A. Nikitina, Evgeny Smirnov, Dmitry A. Kozodaev, Michael I. Nosonovsky, & Ekaterina V. Skorb. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01358
IEEE [1] Aleksandr S. Aglikov, Timur A. Aliev, Mikhail V. Zhukov, Anna A. Nikitina, Evgeny Smirnov, Dmitry A. Kozodaev, Michael I. Nosonovsky, and Ekaterina V. Skorb, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01358. keywords: {polyelectrolytes MXene topological data analysis atomic force microscopy machine learning}