Bipolar Photoresponse of a Graphene Field-Effect Transistor Induced by Photochemical Reactions Bipolar Photoresponse of a Graphene Field-Effect Transistor Induced by Photochemical Reactions AITranslate

Sejong University; Sejong University; University of Education; New Uzbekistan University; University of Sargodha; Sejong University; Sejong University; Xinjiang University; Sejong University; Shenzhen University; Sejong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Graphene is an air-friendly material that can be easily p-doped by oxygen; therefore, a stable, defect-free, and efficient graphene n-doping technique should be developed for achieving high performance in electronic and optoelectronic devices. In this study, we present a unique method for n-type chemical doping of monolayer graphene grown through chemical vapor deposition. The doping process is thoroughly examined using X-ray photoelectron spectroscopy, Raman spectroscopy, and ultraviolet photoelectron spectroscopy. The findings demonstrate that the use of KBr solution is highly effective in achieving n-type doping in monolayer graphene, offering promising prospects for its practical application. Also, we fabricated graphene field-effect transistors and studied their electrical properties before (pristine) and after doping the graphene channel with different KBr concentrations (0, 0.05, 0.15, 0.20, and 0.25 M) in dark and under deep-ultraviolet (DUV) light conditions. During graphene doping in the dark environment, the charge neutrality point (CNP) shifted toward negative back gate voltages and then saturated at 0.25 M. After photochemical doping under DUV light, CNP further shifted toward negative gate voltages with improved carrier mobility at the same molar concentration of 0.25 M. Additionally, the photodetectors are fabricated from pristine and doped graphene which demonstrated bipolar photoresponse, thereby, a transition of negative photocurrent to a positive photocurrent when the concentration of the KBr solution reached 0.20 M. Moreover, their response time decreased from 8 to 3.5 s with increasing KBr concentration from 0 to 0.30 M. Finally, the gate voltage-dependent broadband photoresponsivity of doped graphene (0.25 M) was investigated at different wavelengths (220, 365, 530, and 850 nm). Thus, the controlled doping-induced bidirectional photoresponse can provide a facile route for logic gate applications.

KeyWords AITranslate

chemical doping KBr photoresponsivity fieldeffect carrier mobility charge neutrality point
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00851

Chinese Library Classification Number:

Citation Information:

Graphene is an air-friendly material that can be easily p-doped by oxygen; therefore, a stable, defect-free, and efficient graphene n-doping technique should be developed for achieving high performance in electronic and optoelectronic devices. In this study, we present a unique method for n-type chemical doping of monolayer graphene grown through chemical vapor deposition. The doping process is thoroughly examined using X-ray photoelectron spectroscopy, Raman spectroscopy, and ultraviolet photoelectron spectroscopy. The findings demonstrate that the use of KBr solution is highly effective in achieving n-type doping in monolayer graphene, offering promising prospects for its practical application. Also, we fabricated graphene field-effect transistors and studied their electrical properties before (pristine) and after doping the graphene channel with different KBr concentrations (0, 0.05, 0.15, 0.20, and 0.25 M) in dark and under deep-ultraviolet (DUV) light conditions. During graphene doping in the dark environment, the charge neutrality point (CNP) shifted toward negative back gate voltages and then saturated at 0.25 M. After photochemical doping under DUV light, CNP further shifted toward negative gate voltages with improved carrier mobility at the same molar concentration of 0.25 M. Additionally, the photodetectors are fabricated from pristine and doped graphene which demonstrated bipolar photoresponse, thereby, a transition of negative photocurrent to a positive photocurrent when the concentration of the KBr solution reached 0.20 M. Moreover, their response time decreased from 8 to 3.5 s with increasing KBr concentration from 0 to 0.30 M. Finally, the gate voltage-dependent broadband photoresponsivity of doped graphene (0.25 M) was investigated at different wavelengths (220, 365, 530, and 850 nm). Thus, the controlled doping-induced bidirectional photoresponse can provide a facile route for logic gate applications.

quote

GB/T 7714-2015 [1] Muhammad Farooq Khan, Ehsan Elahi, Najam Ul Hassan, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00851.
MLA [1] Muhammad Farooq Khan, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00851.
APA [1] Muhammad Farooq Khan, Ehsan Elahi, Najam Ul Hassan, Malik Abdul Rehman, H. M. Waseem Khalil, Muhammad Asghar Khan, Shania Rehman, Aize Hao, Hwayong Noh, Karim Khan, & Jonghwa Eom. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00851
IEEE [1] Muhammad Farooq Khan, Ehsan Elahi, Najam Ul Hassan, Malik Abdul Rehman, H. M. Waseem Khalil, Muhammad Asghar Khan, Shania Rehman, Aize Hao, Hwayong Noh, Karim Khan, and Jonghwa Eom, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00851. keywords: {chemical doping KBr photoresponsivity fieldeffect carrier mobility charge neutrality point}