Giant Surface Acoustic Wave Nonreciprocity with Low Magnetoacoustic Insertion Loss in CoFeB/Ru/CoFeB Synthetic Antiferromagnets Giant Surface Acoustic Wave Nonreciprocity with Low Magnetoacoustic Insertion Loss in CoFeB/Ru/CoFeB Synthetic Antiferromagnets AITranslate
Abstract AITranslate
In this study, we optimize the nonreciprocal transmission of surface acoustic waves (SAWs) in a piezoelectric/magnetic heterostructure loaded with a CoFeB(dA)/Ru(0.55 nm)/CoFeB(dB) synthetic antiferromagnet (SAF). The SAF is composed of two ferromagnetic layers separated by a thin nonmagnetic Ru spacer layer, providing strong antiferromagnetic interlayer exchange coupling. The optical spin wave (SW) mode shows a large nonreciprocal dispersion relation in conjunction with a narrow line width. Therefore, for oppositely propagating SAWs, the SAW-SW resonances can become fully separated. For the optimized CoFeB(16 nm)/Ru(0.55 nm)/CoFeB(5 nm) SAF, we demonstrate both, a giant nonreciprocal SAW transmission of ΔS±/lf > 250 dB/mm and a very low magnetoacoustic insertion loss of ILΔ/lf < 1 dB/mm per length lf of the SAF in the acoustic path at frequencies above 5 GHz. These results yield the potential for the realization of novel microwave devices with nonreciprocal signal transmission, such as acoustic isolators. In addition, the experimental results are in excellent agreement with a phenomenological model that considers the dipolar fields of the SWs and takes the bilinear and biquadratic interlayer exchange coupling into account.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00844
Chinese Library Classification Number:
Citation Information:
In this study, we optimize the nonreciprocal transmission of surface acoustic waves (SAWs) in a piezoelectric/magnetic heterostructure loaded with a CoFeB(dA)/Ru(0.55 nm)/CoFeB(dB) synthetic antiferromagnet (SAF). The SAF is composed of two ferromagnetic layers separated by a thin nonmagnetic Ru spacer layer, providing strong antiferromagnetic interlayer exchange coupling. The optical spin wave (SW) mode shows a large nonreciprocal dispersion relation in conjunction with a narrow line width. Therefore, for oppositely propagating SAWs, the SAW-SW resonances can become fully separated. For the optimized CoFeB(16 nm)/Ru(0.55 nm)/CoFeB(5 nm) SAF, we demonstrate both, a giant nonreciprocal SAW transmission of ΔS±/lf > 250 dB/mm and a very low magnetoacoustic insertion loss of ILΔ/lf < 1 dB/mm per length lf of the SAF in the acoustic path at frequencies above 5 GHz. These results yield the potential for the realization of novel microwave devices with nonreciprocal signal transmission, such as acoustic isolators. In addition, the experimental results are in excellent agreement with a phenomenological model that considers the dipolar fields of the SWs and takes the bilinear and biquadratic interlayer exchange coupling into account.
quote
| GB/T 7714-2015 | [1] Matthias Küß, Stephan Glamsch, Yannik Kunz, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00844. |
| MLA | [1] Matthias Küß, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00844. |
| APA | [1] Matthias Küß, Stephan Glamsch, Yannik Kunz, Andreas Hörner, Mathias Weiler, & Manfred Albrecht. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00844 |
| IEEE | [1] Matthias Küß, Stephan Glamsch, Yannik Kunz, Andreas Hörner, Mathias Weiler, and Manfred Albrecht, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00844. keywords: {Nonreciprocity Surface acoustic waves Spin waves Magnetoacoustics Synthetic antiferromagnetic multilayers Acoustic isolator} |