daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Systematic Study of Vinyl Ether-Based Poly(Ethylene Oxide) Side-Chain Polymer Electrolytes AITranslate

Institute for Chemical Technology and Polymer Chemistry (ITCP);Helmholtz-Institute Münster;Helmholtz-Institute Münster; University of Münster; University of Münster; Soft Matter Synthesis Laboratory - Institute for Biological Interfaces III (IBG-3)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, we report on the synthesis of a systematic library of vinyl ether-based poly(ethylene oxide) (PEO) side-chain copolymers in order to reduce the crystallization of PEO. The influence of different grafted PEO side chain lengths, the grafting density, and the [Li+]:[EO] ratio after mixing with LiTFSI on the glass transition temperature (Tg), the crystallinity, and the resulting ionic conductivity was examined. Copolymers bearing longer PEO side chains and higher grafting densities show higher crystallization tendencies while their Tg is reduced at the same time. Furthermore, the addition of LiTFSI reduces crystallization but increases Tg. Because these effects are directly impacting the ionic conductivity, we demonstrate that the different parameters need to be carefully adjusted in order to balance their influence. In this way, a fundamental view that shows the potential of PEO side-chain copolymers for their applications as polymer electrolytes is provided.

KeyWords AITranslate

polymer electrolyte PEO architectures vinyl ether with PEO side chains “graftingto” thermal and electrochemical properties Li+ Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01398

Chinese Library Classification Number:

Citation Information:

Herein, we report on the synthesis of a systematic library of vinyl ether-based poly(ethylene oxide) (PEO) side-chain copolymers in order to reduce the crystallization of PEO. The influence of different grafted PEO side chain lengths, the grafting density, and the [Li+]:[EO] ratio after mixing with LiTFSI on the glass transition temperature (Tg), the crystallinity, and the resulting ionic conductivity was examined. Copolymers bearing longer PEO side chains and higher grafting densities show higher crystallization tendencies while their Tg is reduced at the same time. Furthermore, the addition of LiTFSI reduces crystallization but increases Tg. Because these effects are directly impacting the ionic conductivity, we demonstrate that the different parameters need to be carefully adjusted in order to balance their influence. In this way, a fundamental view that shows the potential of PEO side-chain copolymers for their applications as polymer electrolytes is provided.

quote

GB/T 7714-2015 [1] Andreas J. Butzelaar, Kun L. Liu, Philipp Röring, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01398.
MLA [1] Andreas J. Butzelaar, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01398.
APA [1] Andreas J. Butzelaar, Kun L. Liu, Philipp Röring, Gunther Brunklaus, Martin Winter, & Patrick Theato. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01398
IEEE [1] Andreas J. Butzelaar, Kun L. Liu, Philipp Röring, Gunther Brunklaus, Martin Winter, and Patrick Theato, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01398. keywords: {polymer electrolyte;PEO architectures;vinyl ether with PEO side chains;“graftingto”;thermal and electrochemical properties;Li+;Show More}