Research Progress on Gallium Extraction Technology in Hydrochloric Acid System AITranslate
Abstract AITranslate
The extraction and enrichment technologies of gallium in hydrochloric acid system were emphatically introduced,mainly including extraction,adsorption and molecular imprinting methods.The technical characteristics of the gallium extraction methods in hydrochloric acid system were analyzed.Finally,the problems and research and development directions of gallium extraction technology were pointed out,and reasonable suggestions were also proposed.
KeyWords AITranslate
1邱伟明,奚长生,丘秀珍,林滨钰,谭期,黄康利,林颖.从冶锌工业废渣中提取镓和铟[J].有色金属:冶炼部分,2017(5):28-32. 被引量:13
2刘建,闫英桃,邵海欣,陈长江.CL-TBP萃淋树脂吸附分离镓(Ga)研究[J].化学通报,2001,64(2):119-121. 被引量:10
3林建军,钟依均,陈建荣,许峰,胡建华.N503萃淋树脂吸附镓的研究[J].中国有色金属学报,1996,6(1):40-43. 被引量:6
4刘延红,郭昭华,池君洲,王永旺,陈东.镓回收方法与技术的研究与进展[J].稀有金属与硬质合金,2016,44(1):1-8. 被引量:15
5罗凡,董滨,毕研斌,谢加才.螯合树脂吸附金属阳离子的应用及其研究进展[J].水处理技术,2011,37(1):23-27. 被引量:24
6黄瑞成,刘芳,曹春华.聚氨酯泡沫塑料分离富集高盐溶液中镓的实验条件研究[J].资源环境与工程,2015,29(6):1041-1043. 被引量:3
7董学林,何海洋.泡沫塑料吸附分离富集-电感耦合等离子体质谱法测定稀土矿石中的镓[J].岩矿测试,2016,35(1):42-47. 被引量:9
8张朝晖,张华斌,胡宇芳,李艳杰,聂丽华.镓离子配合物印迹聚合物的研制及吸附性能研究[J].化学通报,2011,74(1):72-77. 被引量:11
1王丽萍,李超.粉煤灰资源化技术开发与利用研究进展[J].矿产保护与利用,2019,39(4):38-45. 被引量:29
2李超,王丽萍.矿物材料处理废水的研究进展[J].矿产保护与利用,2020,40(1):65-71. 被引量:8
3李博琦,谢贤,吕晋芳,朱辉,黎洁,康博文,宋强.粉煤灰资源化综合利用研究进展及展望[J].矿产保护与利用,2020,40(5):153-160. 被引量:26
4文朝璐,孙振华,李少鹏,马志斌,李会泉.LX-92树脂对硫酸体系低浓度镓离子的动态吸附[J].过程工程学报,2021,21(5):567-578. 被引量:3
5马晨,朱晓波,李望,张治国,张传祥.强化助浸回收煤矸石中镓的实验研究[J].稀有金属与硬质合金,2022,50(4):24-27. 被引量:3
6郭文超,李望,朱晓波,张治国,张传祥.P507萃取煤矸石硫酸浸出液中镓的实验研究[J].稀有金属与硬质合金,2022,50(4):28-32. 被引量:2
7王丽萍,李超,常宁,曹坤,高桂梅,张云峰,洪雨,图亚,赵建强.煤矸石中有价元素回收技术研究进展[J].无机盐工业,2023,55(7):10-17.
1刘仓,金亮,陈航超,温智平.粉煤灰资源化提取研究进展[J].煤炭工程,2021,53(S01):127-133. 被引量:6
2杨冬升,吴福飞,凌静,黄和维,赵玉印.提高陈积粉煤灰加气混凝土性能的配比优化[J].新型建筑材料,2019,46(12):117-119. 被引量:3
3段德丹,廖洪强,候昱灼,唐明秀,申午艳.超微粉碎粉煤灰用于建筑外墙用腻子粉研究[J].非金属矿,2020,43(2):88-91. 被引量:5
4李超,王丽萍.矿物材料处理废水的研究进展[J].矿产保护与利用,2020,40(1):65-71. 被引量:8
5王丽萍,徐靓,王永旺,李超.粉煤灰基地质聚合物研究进展[J].矿产保护与利用,2020,40(3):90-94. 被引量:9
6刘树森,云治厚,其其格,白云松,柴静.我国粉煤灰消纳问题的解决对策——以内蒙古自治区为例[J].煤炭加工与综合利用,2020(8):92-96. 被引量:3
7顾成,李宇.煤基固废物综合利用研究进展[J].煤炭与化工,2020,43(9):98-101. 被引量:13
8李博琦,谢贤,吕晋芳,朱辉,黎洁,康博文,宋强.粉煤灰资源化综合利用研究进展及展望[J].矿产保护与利用,2020,40(5):153-160. 被引量:26
9桂乾.粉煤灰资源综合利用现状研究[J].砖瓦,2021(2):30-31. 被引量:3
10冯文丽,吕学斌,熊健,刘超,于志昊,张蕊.粉煤灰高附加值利用研究进展[J].无机盐工业,2021,53(4):25-31. 被引量:12
1辛连君,方郭志.微波消解-石墨炉原子吸收光谱法测定麦田土壤中的铅[J].中国石油和化工标准与质量,2018,38(18):31-32. 被引量:4
2李云辉.分子印迹法-高效液相色谱-串联质谱法检测牛奶中的氨基糖苷类抗生素[J].现代食品,2018,3(19):110-115. 被引量:7
3乔治忠,刘利波,曹艳军.长距离管状带式输送机在黑岱沟选煤厂的应用与分析[J].煤炭加工与综合利用,2019(2):9-11. 被引量:4
4董雁,张夏红.乙酰水杨酸印迹微球的制备及吸附性能[J].泉州师范学院学报,2018,36(6):7-13. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF843.1[冶金工程—有色金属冶金]
Citation Information:
The extraction and enrichment technologies of gallium in hydrochloric acid system were emphatically introduced,mainly including extraction,adsorption and molecular imprinting methods.The technical characteristics of the gallium extraction methods in hydrochloric acid system were analyzed.Finally,the problems and research and development directions of gallium extraction technology were pointed out,and reasonable suggestions were also proposed.
quote
| GB/T 7714-2015 | [1] LI Chao, WANG Li-ping, GUO Zhao-hua, et al. Research Progress on Gallium Extraction Technology in Hydrochloric Acid System[J]. Rare Metals and Cemented Carbides, 2019(1): 6-10. |
| MLA | [1] LI Chao, et al., "Research Progress on Gallium Extraction Technology in Hydrochloric Acid System." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 6-10. |
| APA | [1] LI Chao, WANG Li-ping, GUO Zhao-hua, WANG Yong-wang, & CHEN Dong. (2019). Research Progress on Gallium Extraction Technology in Hydrochloric Acid System. Rare Metals and Cemented Carbides(1), 6-10. |
| IEEE | [1] LI Chao, WANG Li-ping, GUO Zhao-hua, WANG Yong-wang, and CHEN Dong, "Research Progress on Gallium Extraction Technology in Hydrochloric Acid System," Rare Metals and Cemented Carbides, no. 1, pp. 6-10, 2019. keywords: {gallium;extraction technology;hydrochloric acid system;extraction;adsorption;research progress} |