Study on Interference of Coexisting Elements and its Elimination Methods during Cobalt Determination by Potentiometric Titration AITranslate

China Railway Resources Group Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Experimental study was made of interference effects of the coexisting elements including Mn, As, Cr and Fe on cobalt determination by potentiometric titration. The interference elimination methods are proposed,that is oxidizing low valence Cr (Ⅲ) ,Fe (Ⅱ ) and As (Ⅲ) to high valence Cr( Ⅵ) ,Fe (Ⅲ) and As (Ⅴ), and oxidizing Mn ( Ⅱ ) to MnO2 precipitate to be separated and removed. Otherwise, MnOe precip- itate is washed and reduced, and then its cobalt content is determined with flame atomic absorption spec trometry to equalize the measured value by potentiometric titration.

KeyWords AITranslate

cobalt determination potentiometric titration coexisting element interference

1李建雄.EDTA络合滴定法测钴含量误差分析[J].工业金刚石,1999(2):6-7. 被引量:1

2谢丽婷.草酸钴中钴的快速测定——电位滴定法[J].江西有色金属,2006,20(4):43-45. 被引量:11

3符斌.重金属冶金分析[M],北京:冶金工业出版社,1994,82.

4李君,杨玉萍,何明,等.电位滴定法测钴粉中钴含量[A].中国硅酸盐学会.全国第五届浮法玻璃及深加工玻璃技术研讨会论文集[C].2003.

1罗道成,罗铸.碳点荧光猝灭法测定粉煤灰中痕量钴[J].冶金分析,2015,35(9):62-67. 被引量:5

2黎金盛,王成刚,张广文,罗平,许晋,叶汝汉.原子吸收光谱法快速测定镍钴合金镀液中镍、钴的含量[J].广东化工,2016,43(18):164-165. 被引量:1

3王虹,魏秉炎,韩娟,张良.火焰原子吸收光谱法测定冰铜中钴[J].冶金分析,2018,38(7):68-72. 被引量:2

4明帮来,谢英豪,张学梅,钟敏方.电位滴定法测定锂离子电池废料中钴[J].广东化工,2022,49(12):110-112.

1祝艳,鲁应光,母昭,杨亚玲.硅掺杂碳点荧光猝灭法检测废水中钴离子[J].环境化学,2020(12):3517-3523. 被引量:3

2王蓓蓓,王丽,叶华,唐璐子.基于碳量子点的荧光猝灭法检测微量三价铁离子[J].分析试验室,2017,36(10):1146-1150. 被引量:5

3曾美云,邹棣华,李小丹,杨小丽.X射线荧光光谱法测定以镍和钴为主的多金属矿中主次成分[J].冶金分析,2018,38(4):51-56. 被引量:11

4张天磊,周奕华,曹晟.碳点荧光探针在农产品快速检测中的应用进展[J].包装工程,2020,41(3):82-91. 被引量:2

5张夏红,董雁,章丽燕,郑培洪,何立芳.4-硝基邻苯二胺缩水杨醛分光光度法测定水中微量钴(Ⅱ)[J].冶金分析,2020,40(9):82-86. 被引量:2

6陈杰祺,潘凯波,吕晓丹,黄嘉琳,周泽丽,龚诗楚,杨柏.碳点对重金属离子检测的研究进展[J].分子科学学报,2021,37(6):471-482. 被引量:2

7明帮来,谢英豪,张学梅,钟敏方.电位滴定法测定锂离子电池废料中钴[J].广东化工,2022,49(12):110-112.

8田锐,陈君雨,张生,万苏玲.基于牛血清白蛋白修饰的金纳米簇的荧光光谱法快速测定维生素B_(12)药片中Co^(2+)的含量[J].理化检验:化学分册,2023,59(5):527-531.

1何旭伦,卢平,梁勇,武耐英,徐茂田.零流电位法在酸碱滴定中的应用研究[J].化学研究与应用,2012,24(4):531-535. 被引量:7

2林翠芳.氢氧化钠滴定法测定湿法冶金的生物浸出液中硫酸[J].冶金分析,2007,27(8):54-57. 被引量:3

3陈立国,李岩华,刘程惠,朱靖博.尿素包合结合柱层析法制备大豆脱臭馏分中的维生素E[J].大连轻工业学院学报,2007,26(2):124-127. 被引量:6

4刘坤,宋新旺,祝仰文,韩玉贵.胶体滴定法测定P(AM-co-AMPSNa)中AMPSNa含量[J].应用化工,2015,44(11):2115-2119. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O655.2[理学—分析化学]

Citation Information:

Experimental study was made of interference effects of the coexisting elements including Mn, As, Cr and Fe on cobalt determination by potentiometric titration. The interference elimination methods are proposed,that is oxidizing low valence Cr (Ⅲ) ,Fe (Ⅱ ) and As (Ⅲ) to high valence Cr( Ⅵ) ,Fe (Ⅲ) and As (Ⅴ), and oxidizing Mn ( Ⅱ ) to MnO2 precipitate to be separated and removed. Otherwise, MnOe precip- itate is washed and reduced, and then its cobalt content is determined with flame atomic absorption spec trometry to equalize the measured value by potentiometric titration.

quote

GB/T 7714-2015 [1] SONG Hai-feng. Study on Interference of Coexisting Elements and its Elimination Methods during Cobalt Determination by Potentiometric Titration[J]. Rare Metals and Cemented Carbides, 2013(3): 61-64.
MLA [1] SONG Hai-feng. "Study on Interference of Coexisting Elements and its Elimination Methods during Cobalt Determination by Potentiometric Titration." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 61-64.
APA [1] SONG Hai-feng. (2013). Study on Interference of Coexisting Elements and its Elimination Methods during Cobalt Determination by Potentiometric Titration. Rare Metals and Cemented Carbides(3), 61-64.
IEEE [1] SONG Hai-feng, "Study on Interference of Coexisting Elements and its Elimination Methods during Cobalt Determination by Potentiometric Titration," Rare Metals and Cemented Carbides, no. 3, pp. 61-64, 2013. keywords: {cobalt determination;potentiometric titration;coexisting element;interference}