Analysis of Surface Concave Point of Cemented Carbides AITranslate
Abstract AITranslate
The surface concave point phenomenon of a sintered cemented carbide product is introduced. In- ternal microstructure of the concave point is observed by scanning electron microscopy (SEM) and the composition of some points are detected by energy spectrum analysis. The results show that the cause of the concave point is resulted from partial mixture with other material near alloy surface.
KeyWords AITranslate
1陈楚轩.硬质合金质量控制原理[R].湖南:中国钨业协会硬质合金分会.2007.c13-48.
2张立,王元杰,余贤旺,陈述,熊湘君.干混合对硬质合金组织结构的影响[J].硬质合金,2007,24(1):24-27. 被引量:18
3肖鹏,张波.硬质合金生产中的质量控制[J].湖南有色金属,2009,25(3):44-46. 被引量:4
4张颢.蜂窝结构硬质合金的微观组织、孔隙与强度[A].2009年全国粉末冶金学术会议论文集[C].2009.276-278.
1王新庆,孟飞,李栓才.钼产品生产工艺浅谈[J].中国钼业,2011,35(4):55-57. 被引量:2
2周娟,金海兵,胡楠楠.连铸板坯宽度控制生产实践[J].鄂钢科技,2014,0(2):24-26. 被引量:1
3辛海艳,史顺亮,吴翔,肖科.WC总碳含量对WC-9%Co硬质合金收缩系数影响的研究[J].稀有金属与硬质合金,2015,43(6):69-72. 被引量:2
4G.E. Morales - Espejel 马延波(译) 李继峰(校).了解和防止表面疲劳[J].国外轴承技术,2014(1):46-51.
5肖满斗,肖伟,江嘉鹭.WC-Co硬质合金的Co相结构[J].粉末冶金材料科学与工程,2010,15(6):611-614. 被引量:12
6龙建,刘阳,谭敦强,郭锐,陆德平,尹桦.去除废旧硬质合金表面TiN涂层的双氧水+草酸钾碱溶液配制研究[J].粉末冶金工业,2012,22(3):38-43. 被引量:3
7李佳,陈利,尹飞,李明锋.硬质合金表面覆钴状态的研究[J].硬质合金,2005,22(4):212-215.
8黄自谦,谢清连.WC-Ti(C,N)-Co硬质合金表面脱氮后的残余热应力分析[J].粉末冶金材料科学与工程,2014,19(5):671-674.
9李建英,邓翠青,张静,梅淑文.锌液中的合金元素对锌花外观质量影响机理研究[J].冶金标准化与质量,2010,48(6):10-12.
10官新波.山楂自动去核机器的设计[J].今日科苑,2008(13):136-136. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF135.5[冶金工程—冶金物理化学]
Citation Information:
The surface concave point phenomenon of a sintered cemented carbide product is introduced. In- ternal microstructure of the concave point is observed by scanning electron microscopy (SEM) and the composition of some points are detected by energy spectrum analysis. The results show that the cause of the concave point is resulted from partial mixture with other material near alloy surface.
quote
| GB/T 7714-2015 | [1] WU Xiang, SHI Min, MIN Zhao-yu. Analysis of Surface Concave Point of Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2013(3): 58-60. |
| MLA | [1] WU Xiang, et al., "Analysis of Surface Concave Point of Cemented Carbides." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 58-60. |
| APA | [1] WU Xiang, SHI Min, & MIN Zhao-yu. (2013). Analysis of Surface Concave Point of Cemented Carbides. Rare Metals and Cemented Carbides(3), 58-60. |
| IEEE | [1] WU Xiang, SHI Min, and MIN Zhao-yu, "Analysis of Surface Concave Point of Cemented Carbides," Rare Metals and Cemented Carbides, no. 3, pp. 58-60, 2013. keywords: {cemented carbide;surface defect;concave point;mixture;shrinkage coefficient} |