In Situ Transmission Electron Microsopy of Oxide Shell-Induced Pore Formation in (De)lithiated Silicon Nanowires AITranslate

The University of Texas at Austin; The University of Texas at Austin; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; The University of Texas at Austin
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Silicon (Si) nanowires with a silicon oxide (SiOx) shell undergoing lithiation and delithiation were examined by in situ transmission electron microscopy (TEM). Large pores formed in the nanowires during the delithiation cycle. We found that the oxide shell constrains the expansion of the Si nanowires during lithitation and then induces pore formation in the nanowires. We propose that the SiOx shell prevents the vacancies that result from the loss of lithium from escaping the Si core, leading to pore nucleation and growth. It is also possible that the difference in mechanical properties of the expanding and contracting Si nanowire and SiOx shell contribute to the observed pore formation. This in situ study reaffirms the need to directly observe structural changes that occur during cycling in battery materials, especially when modified by coatings.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01904

Chinese Library Classification Number:

Citation Information:

Silicon (Si) nanowires with a silicon oxide (SiOx) shell undergoing lithiation and delithiation were examined by in situ transmission electron microscopy (TEM). Large pores formed in the nanowires during the delithiation cycle. We found that the oxide shell constrains the expansion of the Si nanowires during lithitation and then induces pore formation in the nanowires. We propose that the SiOx shell prevents the vacancies that result from the loss of lithium from escaping the Si core, leading to pore nucleation and growth. It is also possible that the difference in mechanical properties of the expanding and contracting Si nanowire and SiOx shell contribute to the observed pore formation. This in situ study reaffirms the need to directly observe structural changes that occur during cycling in battery materials, especially when modified by coatings.

quote

GB/T 7714-2015 [1] Emily R. Adkins, Taizhi Jiang, Langli Luo, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01904.
MLA [1] Emily R. Adkins, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01904.
APA [1] Emily R. Adkins, Taizhi Jiang, Langli Luo, ChongMin Wang, & Brian A. Korgel. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01904
IEEE [1] Emily R. Adkins, Taizhi Jiang, Langli Luo, ChongMin Wang, and Brian A. Korgel, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01904.