daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High Rate, Selective, and Stable Electroreduction of CO2 to CO in Basic and Neutral Media AITranslate

University of Toronto; University of Toronto; University of Toronto; University of Toronto
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The electroreduction of carbon dioxide (CO2) to chemicals such as carbon monoxide (CO) shows great potential for renewable fuel and chemical production. Significant progress in individual performance metrics such as reaction rate, selectivity, and stability has been achieved, yet the simultaneous achievement of each of these key metrics within a single system, and in a wide range of operating conditions, has yet to be demonstrated. Here we report a composite multilayered porous electrode consisting of a polytetrafluoroethylene gas distribution layer, a conformal Ag catalyst, and a carbon current distributor. Separating the gas and current distribution functions provides endurance, and further reconstructing the catalyst to carbonate-derived Ag provides flexibility in terms of electrolyte. The resulting electrodes reduce CO2 to CO with a Faradaic efficiency over 90% at current densities above 150 mA/cm2, in both neutral and alkaline media for over 100 h of operation. This represents an important step toward the deployment of CO2 electroduction systems using electrolyzer technologies.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01734

Chinese Library Classification Number:

Citation Information:

The electroreduction of carbon dioxide (CO2) to chemicals such as carbon monoxide (CO) shows great potential for renewable fuel and chemical production. Significant progress in individual performance metrics such as reaction rate, selectivity, and stability has been achieved, yet the simultaneous achievement of each of these key metrics within a single system, and in a wide range of operating conditions, has yet to be demonstrated. Here we report a composite multilayered porous electrode consisting of a polytetrafluoroethylene gas distribution layer, a conformal Ag catalyst, and a carbon current distributor. Separating the gas and current distribution functions provides endurance, and further reconstructing the catalyst to carbonate-derived Ag provides flexibility in terms of electrolyte. The resulting electrodes reduce CO2 to CO with a Faradaic efficiency over 90% at current densities above 150 mA/cm2, in both neutral and alkaline media for over 100 h of operation. This represents an important step toward the deployment of CO2 electroduction systems using electrolyzer technologies.

quote

GB/T 7714-2015 [1] CaoThang Dinh, F. Pelayo García de Arquer, David Sinton, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01734.
MLA [1] CaoThang Dinh, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01734.
APA [1] CaoThang Dinh, F. Pelayo García de Arquer, David Sinton, & Edward H. Sargent. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01734