Composition and Surface Morphology Invariant High On–Off Ratio from an Organic Memristor AITranslate
Abstract AITranslate
Material composition plays a crucial role in the device performance; thus, nonvolatile memory devices from a small molecule named 5-mercapto-1-methyl tetrazole (MMT) in an insulating polymer matrix of poly(4-vinyl pyridine) (PVP) were fabricated. The composition of the active material in the device was varied to observe its influence on the device’s electronic properties. The device with a more or less weight ratio of MMT has a much smoother surface morphology, whereas when the contributions of MMT and PVP were equal, the average surface roughness increased. However, the maximum on–off current ratio for all the devices is 105, suggesting that the MMT molecule does not show any change in its characteristic properties when surrounded by an insulating material. When the device was fabricated without the polymer matrix, the surface morphology of the device completely changed as it was filled with large holes. These holes provide short-circuited pathways for the current by forming the direct metal contact between the top and bottom electrodes. The carrier transport through these devices follows various conduction mechanisms. Some of the dominating conduction mechanisms are direct tunneling and trap-free and trap-assisted space–charge-limited conduction.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c01234
Chinese Library Classification Number:
Citation Information:
Material composition plays a crucial role in the device performance; thus, nonvolatile memory devices from a small molecule named 5-mercapto-1-methyl tetrazole (MMT) in an insulating polymer matrix of poly(4-vinyl pyridine) (PVP) were fabricated. The composition of the active material in the device was varied to observe its influence on the device’s electronic properties. The device with a more or less weight ratio of MMT has a much smoother surface morphology, whereas when the contributions of MMT and PVP were equal, the average surface roughness increased. However, the maximum on–off current ratio for all the devices is 105, suggesting that the MMT molecule does not show any change in its characteristic properties when surrounded by an insulating material. When the device was fabricated without the polymer matrix, the surface morphology of the device completely changed as it was filled with large holes. These holes provide short-circuited pathways for the current by forming the direct metal contact between the top and bottom electrodes. The carrier transport through these devices follows various conduction mechanisms. Some of the dominating conduction mechanisms are direct tunneling and trap-free and trap-assisted space–charge-limited conduction.
quote
| GB/T 7714-2015 | [1] Atanu Betal, Jayanta Bera, Ashish Sharma, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01234. |
| MLA | [1] Atanu Betal, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01234. |
| APA | [1] Atanu Betal, Jayanta Bera, Ashish Sharma, Arup K. Rath, & Satyajit Sahu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01234 |
| IEEE | [1] Atanu Betal, Jayanta Bera, Ashish Sharma, Arup K. Rath, and Satyajit Sahu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01234. keywords: {Nonvolatile memory small molecule polymer tunneling space−charge} |