5d transition metal Pt is the canonical spin Hall material for efficient generation of spin–orbit torques (SOTs) in Pt/ferromagnetic layer (FM) heterostructures. However, for a long while with tremendous engineering endeavors, the damping-like SOT efficiencies (ξDL) of Pt and Pt alloys have still been limited to ξDL < 0.5. Here we present that with proper alloying elements, particularly 3d transition metals V and Cr, a high spin–orbital Hall conductivity (σSH ≈ 6.5 × 105 (ℏ/2e) Ω–1 m–1) can be developed. Especially for the Cr-doped case, an extremely high ξDL ≈ 0.9 in a Pt0.69Cr0.31/Co device can be achieved with a moderate Pt0.69Cr0.31 resistivity of ρxx ≈ 133 μΩ cm. A low critical SOT-driven switching current density of Jc ≈ 3.2 × 106 A cm–2 is also demonstrated. The damping constant (α) of the Pt0.69Cr0.31/FM structure is also found to be reduced to 0.052 from the pure Pt/FM case of 0.078. The overall high σSH, giant ξDL, moderate ρxx, and reduced α of such a Pt–Cr/FM heterostructure makes it promising for versatile extremely low power consumption SOT memory applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c01233
Chinese Library Classification Number:
Citation Information:
5d transition metal Pt is the canonical spin Hall material for efficient generation of spin–orbit torques (SOTs) in Pt/ferromagnetic layer (FM) heterostructures. However, for a long while with tremendous engineering endeavors, the damping-like SOT efficiencies (ξDL) of Pt and Pt alloys have still been limited to ξDL < 0.5. Here we present that with proper alloying elements, particularly 3d transition metals V and Cr, a high spin–orbital Hall conductivity (σSH ≈ 6.5 × 105 (ℏ/2e) Ω–1 m–1) can be developed. Especially for the Cr-doped case, an extremely high ξDL ≈ 0.9 in a Pt0.69Cr0.31/Co device can be achieved with a moderate Pt0.69Cr0.31 resistivity of ρxx ≈ 133 μΩ cm. A low critical SOT-driven switching current density of Jc ≈ 3.2 × 106 A cm–2 is also demonstrated. The damping constant (α) of the Pt0.69Cr0.31/FM structure is also found to be reduced to 0.052 from the pure Pt/FM case of 0.078. The overall high σSH, giant ξDL, moderate ρxx, and reduced α of such a Pt–Cr/FM heterostructure makes it promising for versatile extremely low power consumption SOT memory applications.
quote
| GB/T 7714-2015 | [1] ChenYu Hu, YuFang Chiu, ChiaChin Tsai, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01233. |
| MLA | [1] ChenYu Hu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01233. |
| APA | [1] ChenYu Hu, YuFang Chiu, ChiaChin Tsai, ChaoChung Huang, KuanHao Chen, ChengWei Peng, ChienMin Lee, MingYuan Song, YenLin Huang, ShyJay Lin, & ChiFeng Pai. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01233 |
| IEEE | [1] ChenYu Hu, YuFang Chiu, ChiaChin Tsai, ChaoChung Huang, KuanHao Chen, ChengWei Peng, ChienMin Lee, MingYuan Song, YenLin Huang, ShyJay Lin, and ChiFeng Pai, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01233. keywords: {spin−orbit torques spin Hall effects orbital Hall effects spintronics SOTMRAM magnetic materials} |