Poly(amidoamine) Dendrimers: An Excellent Intrinsic Flame Retardant and Curing Agent for Epoxy Resins AITranslate

Northwest Normal University; Northwest Normal University; Northwest Normal University; Northwest Normal University; Northwest Normal University; Northwest Normal University; Northwest Normal University; Northwest Normal University; Northwest Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Considerable efforts have been made to fabricate the intrinsic epoxy resin (EP) with excellent flame retardancy and mechanical properties. However, conventional single molecule flame retardants have met the bottleneck after the massive research studies of the past decade, and with the development of the polymer technology, dendritic flame retardants have been studied due to their versatility and more efficient flame retardancy. Herein, poly-amidoamine (PAMAM) dendrimer flame retardants of different generations were synthesized and utilized as a curing agent and a flame retardant to fabricate the intrinsic EP materials. Their impacts on integrated properties of an EP matrix were studied thoroughly. As expected, the thermal stability, the fire safety, and the flexural capacity of EP/PAMAM thermosets were highly strengthened. The results showed that with 20 wt % loading content of the third-generation PAMAM(G3) dendrimer in the EP matrix (named as EP/20G3), its limited oxygen index value reached up to 26.4% and passed the UL-94 V-0 level. The peak heat release rate and the total heat release data decreased by 51.1 and 60.3%, respectively. Furthermore, the values of Tg, flexural strength, and flexural modulus of EP/20G3 were also promoted comparing with that of the pure EP. At the same time, as an amino-abundant compound, PAMAM dendrimers with different generations can also be served as a curing agent for EP instead of the commonly used diethylenetriamine. It means that PAMAM dendrimers play a dual role in the preparation of flame retardant EP in this system.

KeyWords AITranslate

flame retardancy epoxy resin curing agent PAMAM dendrimer crosslink reaction
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00009

Chinese Library Classification Number:

Citation Information:

Considerable efforts have been made to fabricate the intrinsic epoxy resin (EP) with excellent flame retardancy and mechanical properties. However, conventional single molecule flame retardants have met the bottleneck after the massive research studies of the past decade, and with the development of the polymer technology, dendritic flame retardants have been studied due to their versatility and more efficient flame retardancy. Herein, poly-amidoamine (PAMAM) dendrimer flame retardants of different generations were synthesized and utilized as a curing agent and a flame retardant to fabricate the intrinsic EP materials. Their impacts on integrated properties of an EP matrix were studied thoroughly. As expected, the thermal stability, the fire safety, and the flexural capacity of EP/PAMAM thermosets were highly strengthened. The results showed that with 20 wt % loading content of the third-generation PAMAM(G3) dendrimer in the EP matrix (named as EP/20G3), its limited oxygen index value reached up to 26.4% and passed the UL-94 V-0 level. The peak heat release rate and the total heat release data decreased by 51.1 and 60.3%, respectively. Furthermore, the values of Tg, flexural strength, and flexural modulus of EP/20G3 were also promoted comparing with that of the pure EP. At the same time, as an amino-abundant compound, PAMAM dendrimers with different generations can also be served as a curing agent for EP instead of the commonly used diethylenetriamine. It means that PAMAM dendrimers play a dual role in the preparation of flame retardant EP in this system.

quote

GB/T 7714-2015 [1] Li Li, Hui Xi, Jing Yang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00009.
MLA [1] Li Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00009.
APA [1] Li Li, Hui Xi, Jing Yang, Ting Xiao, Rui Zuo, Xueqing Xu, Yaoxia Yang, Zhiwang Yang, & Ziqiang Lei. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00009
IEEE [1] Li Li, Hui Xi, Jing Yang, Ting Xiao, Rui Zuo, Xueqing Xu, Yaoxia Yang, Zhiwang Yang, and Ziqiang Lei, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00009. keywords: {flame retardancy;epoxy resin;curing agent;PAMAM dendrimer;crosslink reaction}