Self-Healable, Stretchable, and Super-Soft Bottlebrush Polyester Elastomers for Highly Sensitive Flexible Sensors AITranslate

Donghua University; Donghua University; Henan Normal University; Donghua University; Donghua University; Donghua University; Donghua University; Huanghe Science and Technology University; Henan Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

While much effort has been devoted to the creation of super-soft elastomers, there is a dearth of research aimed at self-healable and super-soft renewable elastomers. Herein, self-healing and super-soft renewable elastomers are developed based on bottlebrush architecture design and dynamic associative transesterification. The bottlebrush polymer precursors are generated by ring-opening metathesis polymerization (ROMP) of the norbornene-terminated macromonomer poly(ε-caprolactone-co-l-lactide) (PCLLA) (NB-PCLLA). After introducing alkyne groups onto the end of PCLLA side chains, the bottlebrush polymers are cross-linked to achieve elastomer networks via a UV-induced “click” thiol-yne reaction between the terminal alkyne groups and the dithiothreitol (DTT) additive. The resulting materials exhibit a shear modulus as low as 17 kPa, high stretchability with breaking strains as large as 315%, and a self-healing efficiency of 95.6% at an elevated temperature of 80 °C. Taking the super-softness advantage, flexible sensor devices are assembled based on the prepared elastomer, which are highly sensitive to deformation with a gauge factor of 0.347. This work demonstrates that high-performance biodegradable materials with unique properties that conventional linear polymers impossibly possess can be easily constructed by molecular architecture design using bottlebrush polymers as building blocks.

KeyWords AITranslate

bottlebrush polymer supersoft elastomer selfhealable biodegradable flexible sensors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00017

Chinese Library Classification Number:

Citation Information:

While much effort has been devoted to the creation of super-soft elastomers, there is a dearth of research aimed at self-healable and super-soft renewable elastomers. Herein, self-healing and super-soft renewable elastomers are developed based on bottlebrush architecture design and dynamic associative transesterification. The bottlebrush polymer precursors are generated by ring-opening metathesis polymerization (ROMP) of the norbornene-terminated macromonomer poly(ε-caprolactone-co-l-lactide) (PCLLA) (NB-PCLLA). After introducing alkyne groups onto the end of PCLLA side chains, the bottlebrush polymers are cross-linked to achieve elastomer networks via a UV-induced “click” thiol-yne reaction between the terminal alkyne groups and the dithiothreitol (DTT) additive. The resulting materials exhibit a shear modulus as low as 17 kPa, high stretchability with breaking strains as large as 315%, and a self-healing efficiency of 95.6% at an elevated temperature of 80 °C. Taking the super-softness advantage, flexible sensor devices are assembled based on the prepared elastomer, which are highly sensitive to deformation with a gauge factor of 0.347. This work demonstrates that high-performance biodegradable materials with unique properties that conventional linear polymers impossibly possess can be easily constructed by molecular architecture design using bottlebrush polymers as building blocks.

quote

GB/T 7714-2015 [1] Xiaohui Yu, Yufei Wang, Mengke Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00017.
MLA [1] Xiaohui Yu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00017.
APA [1] Xiaohui Yu, Yufei Wang, Mengke Li, Yingxin Zhang, Yufan Huang, Qi Qian, Yong Zheng, Qiaozhi Hou, & Xiaoshan Fan. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00017
IEEE [1] Xiaohui Yu, Yufei Wang, Mengke Li, Yingxin Zhang, Yufan Huang, Qi Qian, Yong Zheng, Qiaozhi Hou, and Xiaoshan Fan, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00017. keywords: {bottlebrush polymer;supersoft elastomer;selfhealable;biodegradable;flexible sensors}