Influence of Iron and Aluminum Impurities in Beryllium on Properties of Beryllium Materals AITranslate

Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper overviwed the influence of the iron and aluminum impurities in beryllium in various forms on properties of beryllium materials, and pointed out that the formation of AlFeBe 4 with iron and aluminum by specific high temperature ageing heat treatment can improve the properties of beryllium. It was shown that certain ratio of iron and aluminum is a necessary condition to form AlFeBe 4. Description is made of the preparation of Be raw meterial conforming to specific Fe/Al ratio can be produced by selecting beryllium pearls or controlling acid concentration.

KeyWords AITranslate

Be material hot brittleness high temperature ductility Fe/Al ratio AlFeBe 4

1HUNTM.SurprisingBeryllium[J].MaterEng,1988,(11):46.

2MARDERJM.9thEditionofMetalsHandBook,vol7[M].OhioUSA:AmericanSocietyforMetals,1984:755.

3FULLERTONRC.AReviewofPresentandFutureApplicationsofBeryllium[C].4thInterConfonBeryllium,London:TheRoyalSociety,1977:49.

4ODEGARDBC.SAND79—8292[S].1979:7.

5GELLESSH.ImpurityEffectsinBeryllium[Z].AD741896,1972-03.

6STONEHOUSEAJ.InfluenceofImpurityinBeryllium[J].BerylliumScienceandTechnology1979,1:181.

7FOOSRA.Micro-AlloyingRelationshipsinBeryuium[C].ProceedingsoftheBerylliumConf,1970-03:127.

8LONDONGL,etal.GrainSizeandOxideContentAffectBerylliumProperties[J].MetalsEng,1976(11):45.

9SHARMABP.InterConfonPowderMetallurgyandRelatedHighTemperatureMaterials[C].BombayIndia,1983.

10HANESHD,etal.TheProceedingof3thInterConfonIsostaticPressing[C]London,1982:13.

1张青来,A.B.Bondarev,V.A.Andreev,王粒粒,胡永学.时效处理对金属铍剩余电阻比的影响[J].中国有色金属学报,2007,17(7):1124-1128. 被引量:1

2张青来,Bondarev A B,Andreev V A,王粒粒,胡永学.不同纯度金属铍热处理时剩余电阻的变化[J].稀有金属材料与工程,2007,36(8):1354-1357.

3康慧灵,何力军,许德美,钟景明,王战宏,孙本双,刘霄霞.粉末冶金多晶态铍室温断裂行为的研究进展[J].材料导报,2013,27(15):94-97. 被引量:1

4钟景明,李志年,王战宏,王东新,李峰,李军义,张健康.惯性器件用铍材研究及其应用进展[J].粉末冶金工业,2018,28(1):1-6. 被引量:6

5刘柳辉.绿柱石浮选粉矿生产工业氧化铍的实践[J].稀有金属与硬质合金,2002,30(4):25-26. 被引量:7

1刘晓文,毛小西,刘庄,华燕莉.羟硅铍石型铍矿的工艺矿物学研究[J].矿物学报,2010,30(S1):61-63. 被引量:8

2全俊.提高工业氧化铍产品质量的工艺措施[J].稀有金属与硬质合金,2006,34(2):61-63. 被引量:6

3全俊.氟化法生产工业氧化铍工艺研究[J].湖南有色金属,2011,27(5):20-23. 被引量:2

4全俊.碱溶水解法生产工业氧化铍新工艺研究[J].稀有金属与硬质合金,2012,40(2):15-18. 被引量:2

5周民杰,罗炳池,李恺,张继成,李佳,吴卫东.Cu掺杂对Be薄膜微结构的影响(英文)[J].中国有色金属学报:英文版,2012,22(5):1151-1155.

6王清良,李中,李乾,胡鄂明,冯志刚,成泉辉.铍精矿浸出液中铍的回收工艺试验[J].稀有金属,2016,40(1):71-76. 被引量:2

7AMD半导体发表能有效提升晶片效能的双闸极式电晶体[J].电子工程师,2002,28(10):58-58.

8刘军,孙洪涛,李晖,王志萍,陈红,李娜.电感耦合等离子体原子发射光谱法测定铍中氧化铍的含量[J].理化检验:化学分册,2019,55(12):1452-1454. 被引量:3

9陈晓磊,王锐,邱增帅,严小军,刘建梅.铍材薄壁回转零件加工刀具磨损研究[J].工具技术,2020,54(7):20-23. 被引量:2

10于万洋,朱亮.电爆法制备钽微米粉[J].金属功能材料,2020,27(5):1-5.

1孙立权,马凯.Fe/Al 复合板点焊工艺研究[J].武汉水利电力大学(宜昌)学报,1998,20(1):38-41.

2陈昭运,薛伟.16Cr5NiMo钢的高温延性特点[J].大电机技术,1990(5):32-35.

3孙显俊,陶杰,郭训忠,张立伍.Fe/Al复合管液压胀形数值模拟及试验研究[J].锻压技术,2010,35(3):66-70. 被引量:12

4王新华,吴冬梅,刘新宇,王万军,费惠春,张立,叶锦渭.X-52管线钢连铸坯高温变形试样中碳、氮化物的析出和钢的高温延性[J].钢铁,1997,32(11):47-50. 被引量:1

5苗玉刚,曾阳,王腾,吴斌涛,封小松.基于BC-MIG焊的铝/钢异种金属增材制造工艺[J].焊接学报,2015,36(7):5-8. 被引量:17

6周燕岛,刘春明,安彦兼次,木村宏.高纯度Fe-0.15%C合金的高温延性及硫的影响[J].山东工业大学学报,1992,22(1):1-9. 被引量:1

7杨森,杨绍斌,董伟.钨精矿粉含量对激光自蔓延烧结Fe/Al合金组织及性能的影响[J].材料保护,2016,49(3):1-3. 被引量:1

8彭艳,周惦武,徐少华,彭平,刘金水.钢/铝异种金属激光焊接Fe/Al界面微合金化的第一性原理研究[J].稀有金属材料与工程,2012,41(S2):302-306. 被引量:9

9Maurizo,Vedani,韦菁(译).微合金化钢高温延性试验后的晶界析出特性[J].钢铁译文集,2009(2):23-28.

10韩炜,尹付成,苏旭平,王建华,徐琛.硅对Fe/Al固态扩散反应中Fe_2Al_5生长动力学的影响[J].材料热处理学报,2010,31(6):28-32. 被引量:19

Basic Information:

DOI:

Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料]

Citation Information:

The paper overviwed the influence of the iron and aluminum impurities in beryllium in various forms on properties of beryllium materials, and pointed out that the formation of AlFeBe 4 with iron and aluminum by specific high temperature ageing heat treatment can improve the properties of beryllium. It was shown that certain ratio of iron and aluminum is a necessary condition to form AlFeBe 4. Description is made of the preparation of Be raw meterial conforming to specific Fe/Al ratio can be produced by selecting beryllium pearls or controlling acid concentration.

quote

GB/T 7714-2015 [1] MIN Xue-ren, ZHONG Jing-ming. Influence of Iron and Aluminum Impurities in Beryllium on Properties of Beryllium Materals[J]. Rare Metals and Cemented Carbides, 2000(3): 45-49.
MLA [1] MIN Xue-ren, and ZHONG Jing-ming. "Influence of Iron and Aluminum Impurities in Beryllium on Properties of Beryllium Materals." Rare Metals and Cemented Carbides, no. 3, 2000, pp. 45-49.
APA [1] MIN Xue-ren, & ZHONG Jing-ming. (2000). Influence of Iron and Aluminum Impurities in Beryllium on Properties of Beryllium Materals. Rare Metals and Cemented Carbides(3), 45-49.
IEEE [1] MIN Xue-ren and ZHONG Jing-ming, "Influence of Iron and Aluminum Impurities in Beryllium on Properties of Beryllium Materals," Rare Metals and Cemented Carbides, no. 3, pp. 45-49, 2000. keywords: {Be material;hot brittleness;high temperature ductility;Fe/Al ratio;AlFeBe 4}