Research Information on Diamond-coated Hard Metals(Ⅱ) AITranslate

Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The principal and technology of diamond CVD, structure and properties of CVD film, its application prospect and market all are presented with focus on research of diamond CVD hard metals.

KeyWords AITranslate

diamond CVD film coating hard metals structure and property application and market

1DEUERLERF,etal.ProcessControlduringDiamondCoatingofTools[J].IntJRefractoryMetals&HardMaterials,1998,16:191.

2YUZ,etal.PressureDependenceofGrowthModeofHFCVDDiamond[J].DiamondandRelatedMaterials,1997,(6):81.

3YUZ,etal.Orientationof(1×1)-SurfaceFreeEnergiersofCrystals[J].SurfaceScience,1998,401:236.

4YUZ,etal.DiamondGrowthonTurbostracticCarbonbyHotFilamentChemicalVaporDeposition[J].JournalofAppliedPhysics,1993,74:7235.

5KLAGESCP,etal.DiamondCoatingsandCBNCoatingsforTools[J].IntJRefractoryMetals&HardMaterials,1998,16:171.

6DERYAGUMBV,etal.SciAmer,1975,233(5):102.

7FEDOSEEVDV,etal.RussChemRev(EngTransl),1984,53(5):435.

8DEUERLERF,etal.PretreatmentofSubstrateSurfaceforImprovedAdhesionofDiamondFilmsonHardMetalCuttingTools[J].DiamondandRelatedMaterials,1996,(5):1478.

9CAPPELLIE,etal.DiamondNucleationandGrowthonDifferentCuttingToolMaterials[J].DiamondandRelatedMaterials,1996,(5):292.

10OLESEJ,etal.TheNewDiamond-coatedCarbideCuttingTool[J].DiamondandRelatedMaterials,1996,(5):617.

1李丙才,李阳.刀具涂层材料的发展[J].机械制造,2012,50(3):37-39. 被引量:5

2郑虎春,周建华,蒋超,刘新儒,秦琳.WC-Co梯度结构硬质合金研究进展[J].超硬材料工程,2012,24(2):14-18. 被引量:4

3方勤方,周辉峰,李洵.用硼砂溶液及燃焰外焰对硬质合金基底表面进行预处理[J].现代地质,2003,17(1):115-118. 被引量:5

1李海波,余晓艳.硼砂在珠宝首饰加工中的应用[J].宝石和宝石学杂志,2004,6(4):39-41. 被引量:3

2李海波,余晓艳.金刚石在切磨过程中的损伤及相应的处理方法[J].宝石和宝石学杂志,2005,7(2):20-22. 被引量:1

3郭熙丽.石油物资计算机管理集成策略[J].中国石油企业,2005(10):96-97.

4朱晖朝,雷淑梅,陈丽凤,朱红梅,朱斌,匡同春.两步浸蚀法预处理对火焰法沉积金刚石膜形貌、结构和性能的影响[J].硬质合金,2009,26(3):148-151. 被引量:1

5王德山.医疗针灸针套管装配机的研制[J].装备制造技术,2013(3):58-59. 被引量:1

6张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:63

7唐思文,苏闯南,肖雄,陈宇强,李鹏南,刘德顺.微波辅助氮化烧结制备TiCN基功能梯度金属陶瓷的组织与性能[J].热加工工艺,2015,44(18):103-106. 被引量:1

8方勤方,高翔,彭强,姚薇,董娟.云南兰坪-思茅盆地勐野井矿区钾石盐的特征及其沉积环境[J].地质学报,2015,89(11):2108-2113. 被引量:5

9王佳.基于专利分析的我国刀具涂层技术发展现状与对策研究[J].情报探索,2015(12):26-31. 被引量:1

10李俊涛.切削刀具PVD涂层材料的研究进展[J].工具技术,2015,49(7):11-14. 被引量:6

1刘沙,易丹青,余志明,卢斌,王斌,李泳侠,邹丹.金刚石涂层硬质合金的研究动态(Ⅰ)[J].稀有金属与硬质合金,2000(2):53-57. 被引量:12

2张瑞华,胡荣华,聂大.新型萃取剂Cyanex 272在溶剂萃取稀土中的应用[J].稀有金属与硬质合金,1995,23(1):19-24. 被引量:1

3曹妙康.直流电弧炉底电极及其相关技术的发展[J].上海金属,1995,17(2):13-20.

4王辅忠,李荣华,费英.高密度钨合金中沉淀相的研究进展[J].稀有金属与硬质合金,2002,30(4):39-41. 被引量:1

5周辉峰,李洵,方勤方.金刚石薄膜涂层硬质合金的耐磨性试验研究[J].探矿工程,2000(5):22-24. 被引量:3

6朱立光,金山同.连铸保护渣研究动态述评[J].连铸,1997,0(5):38-42.

7张晨,刘世洲.去除废钢中的有色金属[J].钢铁研究,1998(3):60-63.

8王应群.金属萃取/湿法冶金的研究动向[J].世界有色金属,1992(4):9-13.

9高建祥,曲选辉,赵赛.金属粉末注射成形技术的最新研究动态与发展趋势[J].硬质合金,2003,20(1):56-60. 被引量:14

10蔡方寒,唐霞辉,秦应雄,李立波,朱国富.金刚石工具用预合金粉末的研究动态[J].金刚石与磨料磨具工程,2004,24(5):77-80. 被引量:25

Basic Information:

DOI:

Chinese Library Classification Number:TF125.34[冶金工程—粉末冶金]

Citation Information:

The principal and technology of diamond CVD, structure and properties of CVD film, its application prospect and market all are presented with focus on research of diamond CVD hard metals.

quote

GB/T 7714-2015 [1] LIU Sha, YI Dan-qing, YU Zhi-ming, et al. Research Information on Diamond-coated Hard Metals(Ⅱ)[J]. Rare Metals and Cemented Carbides, 2000(3): 36-44.
MLA [1] LIU Sha, et al., "Research Information on Diamond-coated Hard Metals(Ⅱ)." Rare Metals and Cemented Carbides, no. 3, 2000, pp. 36-44.
APA [1] LIU Sha, YI Dan-qing, YU Zhi-ming, LU Bin, WANG Bin, LI Yong-xia, & ZOU Dan. (2000). Research Information on Diamond-coated Hard Metals(Ⅱ). Rare Metals and Cemented Carbides(3), 36-44.
IEEE [1] LIU Sha, YI Dan-qing, YU Zhi-ming, LU Bin, WANG Bin, LI Yong-xia, and ZOU Dan, "Research Information on Diamond-coated Hard Metals(Ⅱ)," Rare Metals and Cemented Carbides, no. 3, pp. 36-44, 2000. keywords: {diamond CVD film;coating;hard metals;structure and property;application and market}