Study on Effect of Cerium-Lanthanum Ratio on the Properties of Cerium-based Polishing Powder AITranslate
Abstract AITranslate
The ratio of cerium to lanthanum is one of the key factors affecting the physical and chemical properties and performance of the cerium-based polishing powder.In this study,the polishing powders with different ratios of cerium to lanthanum were prepared with the precipitation method.The study results show that the cerium and lanthanum components form stable composite carbonate precursors,and form composite oxides with a single crystal phase after calcination.When the proportion of cerium in cerium and lanthanum is 95%,the primary particle size of the polishing powder is less than 100 nm,and the agglomeration effect is weak.The polishing powders with medium and low cerium proportion(≤85%)have obvious agglomeration effect and large average particle size,but they have stronger cutting force on K9 optical glass in a short time.The polishing powders with high cerium proportion(85%,95%)have more durable cutting force.Doping with a small amount of lanthanum is beneficial to improve the strength and durability of the cutting force of cerium-based polishing powder on K9 optical glass.
KeyWords AITranslate
1郭尧,李现常,王芳,殷美丽,牛永生,侯绍刚,李永绣.氟化碳酸镧铈煅烧过程的相态结构和颗粒特征变化[J].稀土,2015,36(6):74-79. 被引量:3
2杨国胜,崔凌霄,谢兵,吴文远.氟对铈基稀土抛光粉性能的影响研究[J].稀土,2016,37(6):80-85. 被引量:9
3王晶,金彦章,王振波.氟化物掺入对稀土抛光粉性能的影响[J].无机盐工业,2019,51(4):37-41. 被引量:3
4窦宁.2020年稀土抛光粉市场探求 疫情下5G时代的现状与挑战[J].稀土信息,2020(10):28-31. 被引量:1
5霍知节.话说稀土抛光材料[J].新材料产业,2019(6):72-77. 被引量:3
1杨小海,李安,宫慧勇,崔超,臧琰,赖丹.不同沉淀剂制备氧化铈抛光粉[J].铜业工程,2023(2):86-91.
1刘囿辰,马国鹭,赵涌,宋子军,胡亮子.组合式力热动态载荷光学窗口的光学特性研究[J].应用光学,2021,42(6):1122-1126. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TQ133.3[化学工程—无机化工]
Citation Information:
The ratio of cerium to lanthanum is one of the key factors affecting the physical and chemical properties and performance of the cerium-based polishing powder.In this study,the polishing powders with different ratios of cerium to lanthanum were prepared with the precipitation method.The study results show that the cerium and lanthanum components form stable composite carbonate precursors,and form composite oxides with a single crystal phase after calcination.When the proportion of cerium in cerium and lanthanum is 95%,the primary particle size of the polishing powder is less than 100 nm,and the agglomeration effect is weak.The polishing powders with medium and low cerium proportion(≤85%)have obvious agglomeration effect and large average particle size,but they have stronger cutting force on K9 optical glass in a short time.The polishing powders with high cerium proportion(85%,95%)have more durable cutting force.Doping with a small amount of lanthanum is beneficial to improve the strength and durability of the cutting force of cerium-based polishing powder on K9 optical glass.
quote
| GB/T 7714-2015 | [1] YANG Xiao hai, LIU Yun long, LI An. Study on Effect of Cerium-Lanthanum Ratio on the Properties of Cerium-based Polishing Powder[J]. Rare Metals and Cemented Carbides, 2022(4): 57-61. |
| MLA | [1] YANG Xiao hai, et al., "Study on Effect of Cerium-Lanthanum Ratio on the Properties of Cerium-based Polishing Powder." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 57-61. |
| APA | [1] YANG Xiao hai, LIU Yun long, & LI An. (2022). Study on Effect of Cerium-Lanthanum Ratio on the Properties of Cerium-based Polishing Powder. Rare Metals and Cemented Carbides(4), 57-61. |
| IEEE | [1] YANG Xiao hai, LIU Yun long, and LI An, "Study on Effect of Cerium-Lanthanum Ratio on the Properties of Cerium-based Polishing Powder," Rare Metals and Cemented Carbides, no. 4, pp. 57-61, 2022. keywords: {polishing powder;cerium oxide;lanthanum oxide;cerium-lanthanum ratio;precipitation method;cuttingforce;particle size} |