daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation and Characterization of LaB6Nanopowders by Calciothermic Reduction AITranslate

Hunan Research Institute for Rare Earth Metal Materials Co.,Ltd.;Hunan Research Institute for Rare Earth Metal Materials Co.,Ltd.;Hunan Research Institute for Rare Earth Metal Materials Co.,Ltd.;Hunan Research Institute for Rare Earth Metal Materials Co.,Ltd.;Hunan Research Institute for Rare Earth Metal Materials Co.,Ltd.;Hunan Research Institute for Rare Earth Metal Materials Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

LaB6 nanopowders were successfully prepared by calciothermic reduction method for the first time.The effects of reduction temperature on the phase composition,morphology and particle size of powder products were studied by X-ray diffractometer(XRD)and field emission scanning electron microscope(FE-SEM),and the optical absorption properties of nanopowders were characterized by UV/VIS/NIR spectrophotometer.The results show that the prepared LaB6 nanopowders have a simple cubic single-phase crystal structure,good crystallinity and nearly spherical particle morphology with an average grain size of(35±6)nm.With the increase of reaction temperature,the particle size of the powders increases and the particle morphology shifts to cubic shape.The absorption spectrum shows that the LaB6 nanopowder prepared at 800℃has strong absorption properties in the ultraviolet and near-infrared regions,and its maximum transmission light wavelength is 595 nm,which is essentially in agreement with the first-principles calculation results of LaBe6.

KeyWords AITranslate

lanthanum hexaboride nanopower calciothermic reduction optical absorption morphology particlesize

1潘晓剑,包黎红,宁军,赵凤岐,朝洛蒙,刘子忠.多元纳米稀土六硼化物Nd1-xEuxB6粉末的制备及光吸收研究[J].物理学报,2021,70(3):191-198. 被引量:1

2程大伟,包黎红,张红艳,潘晓剑,那仁格日乐,赵凤岐,特古斯,朝洛濛.蒸发冷凝法制备超细CeB6和SmB6纳米粉末及可见光穿透特性[J].物理学报,2019,68(24):221-228. 被引量:3

3包黎红,朝洛蒙,伟伟,特古斯.稀土硼化物LaxCe1-xB6亚微米粉的制备及光吸收研究[J].物理学报,2015,64(9):445-449. 被引量:6

4苏玉长,张鹏飞,肖立华,陈宏艳.微波固相合成纳米LaB_6的组织结构及其透光特性[J].中南大学学报:自然科学版,2011,42(10):3015-3019. 被引量:5

5王小菊,蒋亚东,林祖伦,祁康成,陈泽祥.单晶六硼化镧的制备及主要应用[J].材料导报:网络版,2006(2):13-15. 被引量:4

6张粹伟.六硼化镧阴极[J].光电子技术,1989,9(3):35-44. 被引量:5

1余茂林,孙皓,杨雨浛,邓安仲,罗盛,袁旺.反射型蓝色隔热节能涂层的制备及隔热性能[J].表面技术,2022,51(3):217-225. 被引量:2

2乔次仁,次旦多杰,仁乾龙珠,殷一珂.路用近红外反射涂层光热性能研究[J].运输经理世界,2021(14):102-104.

3王曾学,刘艳,赵盼,张训迪,阳一鸣,孙鹏,张秀云,冯玉,郑婷婷,陈辰,李伟.近红外光热转换剂氧缺陷二氧化钼的制备及其在光热治疗中的应用[J].无机化学学报,2022,38(9):1739-1751.

4管雪,金健,顾广瑞.射频磁控溅射制备的CdSe薄膜的光电学性质[J].延边大学学报:自然科学版,2022,48(2):138-142.

5许进博,董晓珠,孔存辉,赵英娜,王建省,曾雄丰.SrTiO_(3)/TiO_(2)复合薄膜的制备及其光电化学阴极保护性能[J].复合材料学报,2022,39(8):3922-3928. 被引量:2

6王广崎,吴邦昊,毕艺洋,张钰.CdS纳米线的溶剂热合成及其光催化产氢性能[J].吉林化工学院学报,2022,39(5):20-26. 被引量:2

7黄文君,李盼盼,魏香凤,刘节华.非卤离子溶剂热构筑高质量一维Sb_(2)S_(3)单晶[J].齐鲁工业大学学报,2022,36(4):1-7.

8Bechir Ouni,Tarek Larbi,Mosbah Amlouk.Vibrational, Electronic and Structural Study of Sprayed ZnO Thin Film Based on the IR-Raman Spectra and DFT Calculations[J].晶体结构理论与应用(英文),2022,11(2):23-38. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ133.3[化学工程—无机化工]

Citation Information:

LaB6 nanopowders were successfully prepared by calciothermic reduction method for the first time.The effects of reduction temperature on the phase composition,morphology and particle size of powder products were studied by X-ray diffractometer(XRD)and field emission scanning electron microscope(FE-SEM),and the optical absorption properties of nanopowders were characterized by UV/VIS/NIR spectrophotometer.The results show that the prepared LaB6 nanopowders have a simple cubic single-phase crystal structure,good crystallinity and nearly spherical particle morphology with an average grain size of(35±6)nm.With the increase of reaction temperature,the particle size of the powders increases and the particle morphology shifts to cubic shape.The absorption spectrum shows that the LaB6 nanopowder prepared at 800℃has strong absorption properties in the ultraviolet and near-infrared regions,and its maximum transmission light wavelength is 595 nm,which is essentially in agreement with the first-principles calculation results of LaBe6.

quote

GB/T 7714-2015 [1] LIU Hua, ZHAO Rui-shan, WEN Kang, et al. Preparation and Characterization of LaB6Nanopowders by Calciothermic Reduction[J]. Rare Metals and Cemented Carbides, 2022(4): 51-56.
MLA [1] LIU Hua, et al., "Preparation and Characterization of LaB6Nanopowders by Calciothermic Reduction." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 51-56.
APA [1] LIU Hua, ZHAO Rui-shan, WEN Kang, DENG Yue-hua, HUANG Mei-song, & YANG Lu-hui. (2022). Preparation and Characterization of LaB6Nanopowders by Calciothermic Reduction. Rare Metals and Cemented Carbides(4), 51-56.
IEEE [1] LIU Hua, ZHAO Rui-shan, WEN Kang, DENG Yue-hua, HUANG Mei-song, and YANG Lu-hui, "Preparation and Characterization of LaB6Nanopowders by Calciothermic Reduction," Rare Metals and Cemented Carbides, no. 4, pp. 51-56, 2022. keywords: {lanthanum hexaboride;nanopower;calciothermic reduction;optical absorption;morphology;particlesize}