Viscoelastic Properties and Sulfur Distribution at the Nanoscale in Binary Elastomeric Blends: Toward Phase-Specific Cross-Link Density Estimations AITranslate

Luxembourg Institute of Science and Technology (LIST);Luxembourg Institute of Science and Technology (LIST);Luxembourg Institute of Science and Technology (LIST);Luxembourg Institute of Science and Technology (LIST);Goodyear Innovation Center Luxembourg, Avenue Gordon Smith;Goodyear Innovation Center Luxembourg, Avenue Gordon Smith;Luxembourg Institute of Science and Technology (LIST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Immiscible blends of elastomers present high technological interest, and the selection of the vulcanization system is important for the optimization of properties for different technical applications. In particular, the effect of the curing agents on the distribution of cross-links in each phase is key for the full comprehension of the structure–property relationships. Aiming at the understanding of the phase-specific network structure in rubber blends, this work presents an innovative strategy for the quantitative characterization of the local viscoelastic properties of immiscible rubber blends by atomic force microscopy (AFM) measurements. A systematic study on the quantitative nanomechanical characterization by AFM of unfilled single natural rubber (NR) matrixes with different degrees of cross-link densities ultimately allows for the estimation of the phase-specific cross-link density of the NR phase in NR/butadiene rubber (BR) blends, prepared with varying vulcanization systems. Complementary chemical information by high-resolution secondary ion mass spectrometry imaging is able to reveal differences in sulfur contents in each elastomeric phase of the blends.

KeyWords AITranslate

rubber blend AFM nanomechanical properties crosslink density sulfur distribution SIMS imaging
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00032

Chinese Library Classification Number:

Citation Information:

Immiscible blends of elastomers present high technological interest, and the selection of the vulcanization system is important for the optimization of properties for different technical applications. In particular, the effect of the curing agents on the distribution of cross-links in each phase is key for the full comprehension of the structure–property relationships. Aiming at the understanding of the phase-specific network structure in rubber blends, this work presents an innovative strategy for the quantitative characterization of the local viscoelastic properties of immiscible rubber blends by atomic force microscopy (AFM) measurements. A systematic study on the quantitative nanomechanical characterization by AFM of unfilled single natural rubber (NR) matrixes with different degrees of cross-link densities ultimately allows for the estimation of the phase-specific cross-link density of the NR phase in NR/butadiene rubber (BR) blends, prepared with varying vulcanization systems. Complementary chemical information by high-resolution secondary ion mass spectrometry imaging is able to reveal differences in sulfur contents in each elastomeric phase of the blends.

quote

GB/T 7714-2015 [1] João P. Cosas Fernandes, Carlos E. Federico, Esther Lentzen, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00032.
MLA [1] João P. Cosas Fernandes, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00032.
APA [1] João P. Cosas Fernandes, Carlos E. Federico, Esther Lentzen, Nathalie Valle, Beatriz BasterraBeroiz, Marc Weydert, & Robert Quintana. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00032
IEEE [1] João P. Cosas Fernandes, Carlos E. Federico, Esther Lentzen, Nathalie Valle, Beatriz BasterraBeroiz, Marc Weydert, and Robert Quintana, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00032. keywords: {rubber blend;AFM;nanomechanical properties;crosslink density;sulfur distribution;SIMS imaging}