daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Frequency Swelling/Deswelling Oscillation of Poly(Oligoethylene Glycol) Methacrylate-Based Hydrogel Microspheres with a Tris(2,2′-bipyridyl)ruthenium Catalyst AITranslate

Shinshu University; Shinshu University; The University of Tokyo; Shinshu University; Shinshu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The swelling/deswelling oscillation of autonomously oscillating hydrogel microspheres (microgels) at a frequency close to that of the human heartbeat was accomplished. In this study, poly(oligoethylene glycol) methacrylate (pOEGMA)-based microgels that contain a tris(2,2′-bipyridyl)ruthenium catalyst were used to create oscillatory chemical systems via the Belousov–Zhabotinsky (BZ) reaction. The oscillating pOEGMA microgels can undergo the BZ reaction without irreversible aggregation at elevated temperatures or high substrate concentrations. By optimizing the chemical composition of the microgels and the BZ reaction conditions, a short swelling/deswelling oscillation period of ∼1.3 s was achieved in the dispersed state. Furthermore, in the assembled state, the microgels exhibited fast swelling/deswelling on the order of seconds (oscillation period: ∼6.2 s). The central concept of this study, that is, “high-frequency oscillation”, can be expected to benefit the development of advanced bioinspired actuators that imitate the human heartbeat.

KeyWords AITranslate

microgels redox reactions oscillation catalysts actuators
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00153

Chinese Library Classification Number:

Citation Information:

The swelling/deswelling oscillation of autonomously oscillating hydrogel microspheres (microgels) at a frequency close to that of the human heartbeat was accomplished. In this study, poly(oligoethylene glycol) methacrylate (pOEGMA)-based microgels that contain a tris(2,2′-bipyridyl)ruthenium catalyst were used to create oscillatory chemical systems via the Belousov–Zhabotinsky (BZ) reaction. The oscillating pOEGMA microgels can undergo the BZ reaction without irreversible aggregation at elevated temperatures or high substrate concentrations. By optimizing the chemical composition of the microgels and the BZ reaction conditions, a short swelling/deswelling oscillation period of ∼1.3 s was achieved in the dispersed state. Furthermore, in the assembled state, the microgels exhibited fast swelling/deswelling on the order of seconds (oscillation period: ∼6.2 s). The central concept of this study, that is, “high-frequency oscillation”, can be expected to benefit the development of advanced bioinspired actuators that imitate the human heartbeat.

quote

GB/T 7714-2015 [1] Kohei Inui, Ikuma Saito, Ryo Yoshida, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00153.
MLA [1] Kohei Inui, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00153.
APA [1] Kohei Inui, Ikuma Saito, Ryo Yoshida, Haruka Minato, & Daisuke Suzuki. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00153
IEEE [1] Kohei Inui, Ikuma Saito, Ryo Yoshida, Haruka Minato, and Daisuke Suzuki, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00153. keywords: {microgels;redox reactions;oscillation;catalysts;actuators}