Conducting 2D Nanosheets: Photo Driven Crystallinity in Self-Assembled Cu (II) Metalated Porphyrin-Bispyridylquinoxaline Conducting 2D Nanosheets: Photo Driven Crystallinity in Self-Assembled Cu (II) Metalated Porphyrin-Bispyridylquinoxaline AITranslate

CSIR-Indian Institute of Chemical Technology; CSIR-Indian Institute of Chemical Technology; CSIR-Indian Institute of Chemical Technology; CSIR-Indian Institute of Chemical Technology; CSIR-Indian Institute of Chemical Technology; CSIR-Indian Institute of Chemical Technology; CSIR-Indian Institute of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tuning the crystallinity in self-assembled nanostructures has a significant impact on the electronic properties. Although several approaches have been adopted for organic π-conjugated systems to generate the amorphous to crystalline structures, the bulky structure of extended macrocyclics is hitherto unknown. Herein, we have developed three symmetric freebase and metallo substituted porphyrin appended bispyridylquinoxalines (PFb-DPQ, PCu-DPQ and PZn-DPQ) in which copper metalated P-DPQ exhibits crystalline phase transitions under light stimuli. Notably, light irradiated P-DPQ derivatives undergo a protonation, demetalation, and anion binding mechanism, resulting in the formation of self-assembled open, closed 0D nanospheres together with 2D nanosheets via methanol vapor diffusion approach. Interestingly, light stimulation regulates the morphology from 0D nanosphere to 2D nanosheets in PCu-DPQ and H+[PCu-DPQ(Cl)]−, which promotes the amorphous to crystalline nature. Consequently, the bulk conductivity of 2D nanosheets exhibits ∼32 mS cm–1, and it is remarkably 102 times higher than 0D nanospheres. Thus, these results promote that the stimuli responsive metallo substituted macrocyclic systems is a significant initiative to manipulate the electronic properties in organic electronics.

KeyWords AITranslate

porphyrinbispyridylquinoxaline light stimuli anion binding 2D nanostructure conductivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00320

Chinese Library Classification Number:

Citation Information:

Tuning the crystallinity in self-assembled nanostructures has a significant impact on the electronic properties. Although several approaches have been adopted for organic π-conjugated systems to generate the amorphous to crystalline structures, the bulky structure of extended macrocyclics is hitherto unknown. Herein, we have developed three symmetric freebase and metallo substituted porphyrin appended bispyridylquinoxalines (PFb-DPQ, PCu-DPQ and PZn-DPQ) in which copper metalated P-DPQ exhibits crystalline phase transitions under light stimuli. Notably, light irradiated P-DPQ derivatives undergo a protonation, demetalation, and anion binding mechanism, resulting in the formation of self-assembled open, closed 0D nanospheres together with 2D nanosheets via methanol vapor diffusion approach. Interestingly, light stimulation regulates the morphology from 0D nanosphere to 2D nanosheets in PCu-DPQ and H+[PCu-DPQ(Cl)]−, which promotes the amorphous to crystalline nature. Consequently, the bulk conductivity of 2D nanosheets exhibits ∼32 mS cm–1, and it is remarkably 102 times higher than 0D nanospheres. Thus, these results promote that the stimuli responsive metallo substituted macrocyclic systems is a significant initiative to manipulate the electronic properties in organic electronics.

quote

GB/T 7714-2015 [1] Madarapu Naresh, Palivela Siva Gangadhar, Priti Kumari, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00320.
MLA [1] Madarapu Naresh, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00320.
APA [1] Madarapu Naresh, Palivela Siva Gangadhar, Priti Kumari, Nagadatta Pravallika, Yelukala Ramakrishna, Lingamallu Giribabu, & Seelam Prasanthkumar. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00320
IEEE [1] Madarapu Naresh, Palivela Siva Gangadhar, Priti Kumari, Nagadatta Pravallika, Yelukala Ramakrishna, Lingamallu Giribabu, and Seelam Prasanthkumar, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00320. keywords: {porphyrinbispyridylquinoxaline light stimuli anion binding 2D nanostructure conductivity}