daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress in Green and Low-Carbon Preparation of Metal Powders by High-Pressure Hydrogen Reduction AITranslate

Changsha Research Institute of Mining and Metallurgy Co.,Ltd.;Changsha Research Institute of Mining and Metallurgy Co.,Ltd.;Changsha Research Institute of Mining and Metallurgy Co.,Ltd.;Changsha Research Institute of Mining and Metallurgy Co.,Ltd.;Changsha Research Institute of Mining and Metallurgy Co.,Ltd.;Changsha Research Institute of Mining and Metallurgy Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High-pressure hydrogen reduction method has the advantages of being green and environmentally friendly,low energy consumption,high production efficiency and being easy to automate production.The theore-tical basis of high-pressure hydrogen reduction technology is introduced,the current research progress in the preparation of precious metals and heavy metals by high-pressure hydrogen reduction at home and abroad is reviewed,and the future development direction of this method is prospected.

KeyWords AITranslate

high-pressure hydrogen reduction metal powder hydrometallurgy green and low-carbon process

1聂宪生,陈景,谭庆麟.从盐酸介质中加压氢还原铱的动力学研究[J].贵金属,1990,11(3):1-12. 被引量:4

2陈景,聂宪生.加压氢还原法分离铑铱[J].贵金属,1992,13(2):7-12. 被引量:4

3昝林寒,杨滨,汪云华,赵家春,范兴祥.氢还原法制备超细钴粉[J].材料科学与工程学报,2010,28(4):571-575. 被引量:1

4喻克宁,梁焕珍.铜硫化物直接水浆氢还原制备铜粉[J].有色金属,2004,56(41):74-76. 被引量:5

5张冠东,张登君,李报厚.从氨浸电镀污泥产物中氢还原分离铜、镍、锌的研究[J].化工冶金,1996,17(3):214-219. 被引量:37

6赵强,宁顺明,佘宗华,王文娟,吴江华,吴杰.偏钒酸钠氢还原制备钒氧化物清洁冶金新过程的应用研究[J].矿冶工程,2014,34(3):94-96. 被引量:3

1翟永健,李志超,张德林.大数据在城市生活垃圾智能分类管理中的应用研究[J].中文科技期刊数据库(全文版)自然科学,2022(12):0019-0022.

2王维波,薛媛,高怡文,康宵瑜,赵丽,金志,王锰.微生物与化学驱/气驱协同提高采收率技术研究进展[J].应用化工,2023,52(5):1587-1592.

3邹昊.试析高层建筑桩基础静压桩施工技术的应用[J].建筑与装饰,2023(1):191-194.

4王海平,金燕.机械电子工程专业高职本科“4+0”联合培养模式的探索与实践[J].南方农机,2023,54(7):159-163.

5曹玉霞,孙景卫,周海静,黄雁,郝斌.超音速火焰喷涂NiCoCrAlY/Al_(2)O_(3)-10%B_(4)C涂层的制备及抗氧化性能研究[J].表面技术,2023,52(5):413-419.

6张海宝,骆贞江,孟祥龙,伏晓丹,张鹏.刚果(金)铜钴矿湿法冶金工程实例分析[J].有色冶金设计与研究,2023,44(3):9-14.

7谢苗,张鸿宇,任泽,杨志勇,周永利,刘治翔,李玉岐.煤矿井下锚固群组动力响应特性分析[J].振动与冲击,2023,42(10):278-288.

8徐旭龙,熊山,熊军,周石港,闫一峰,汪志远,宋剑,王仕琛,琚泽.精细单砂体刻画在油田开发中后期的应用[J].中外能源,2023,28(5):15-24.

Basic Information:

DOI:

Chinese Library Classification Number:TF123[冶金工程—粉末冶金]

Citation Information:

High-pressure hydrogen reduction method has the advantages of being green and environmentally friendly,low energy consumption,high production efficiency and being easy to automate production.The theore-tical basis of high-pressure hydrogen reduction technology is introduced,the current research progress in the preparation of precious metals and heavy metals by high-pressure hydrogen reduction at home and abroad is reviewed,and the future development direction of this method is prospected.

quote

GB/T 7714-2015 [1] ZHU An-yu, SHEN Yu-jun, PENG Jun, et al. Research Progress in Green and Low-Carbon Preparation of Metal Powders by High-Pressure Hydrogen Reduction[J]. Rare Metals and Cemented Carbides, 2023(3): 37-42.
MLA [1] ZHU An-yu, et al., "Research Progress in Green and Low-Carbon Preparation of Metal Powders by High-Pressure Hydrogen Reduction." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 37-42.
APA [1] ZHU An-yu, SHEN Yu-jun, PENG Jun, ZHOU Xiao-zhou, CAI Yun-zhuo, & SHEN Lin-chang. (2023). Research Progress in Green and Low-Carbon Preparation of Metal Powders by High-Pressure Hydrogen Reduction. Rare Metals and Cemented Carbides(3), 37-42.
IEEE [1] ZHU An-yu, SHEN Yu-jun, PENG Jun, ZHOU Xiao-zhou, CAI Yun-zhuo, and SHEN Lin-chang, "Research Progress in Green and Low-Carbon Preparation of Metal Powders by High-Pressure Hydrogen Reduction," Rare Metals and Cemented Carbides, no. 3, pp. 37-42, 2023. keywords: {high-pressure hydrogen reduction;metal powder;hydrometallurgy;green and low-carbon process}