Constructing High Performance Hydrogels with Strong Underwater Adhesion through a “Mussel Feet-Rock” Inspired Strategy AITranslate
Abstract AITranslate
In this study, high performance hydrogels with strong underwater adhesion were constructed through a “mussel feet-rock” inspired strategy, in which a random copolymer containing side-chain positive charges and catechol groups (PMD) simulated the adhesive proteins of mussel, and poly(acrylic acid) (PAA) mimicked the rocky surface. PMD and PAA chains could noncovalently cross-link together through hydrogen bonding, charge interaction, and chain entanglement. Catechol groups further provide the hydrogel strong adhesion ability. Taking advantage of this strategy, the obtained PAA/PMD hydrogels featured the best stretchability among reported hydrogels and intensive repeatable adhesion behavior, and further exhibited unusual wet-enhanced tensile and shear strength together with durable underwater adhesion. These findings are valuable for the development of mussel-inspired adhesives and high performance hydrogels.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00590
Chinese Library Classification Number:
Citation Information:
In this study, high performance hydrogels with strong underwater adhesion were constructed through a “mussel feet-rock” inspired strategy, in which a random copolymer containing side-chain positive charges and catechol groups (PMD) simulated the adhesive proteins of mussel, and poly(acrylic acid) (PAA) mimicked the rocky surface. PMD and PAA chains could noncovalently cross-link together through hydrogen bonding, charge interaction, and chain entanglement. Catechol groups further provide the hydrogel strong adhesion ability. Taking advantage of this strategy, the obtained PAA/PMD hydrogels featured the best stretchability among reported hydrogels and intensive repeatable adhesion behavior, and further exhibited unusual wet-enhanced tensile and shear strength together with durable underwater adhesion. These findings are valuable for the development of mussel-inspired adhesives and high performance hydrogels.
quote
| GB/T 7714-2015 | [1] Rui Zhang, Hongwei Peng, Tianxu Zhou, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00590. |
| MLA | [1] Rui Zhang, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00590. |
| APA | [1] Rui Zhang, Hongwei Peng, Tianxu Zhou, Yuan Yao, Xuedong Zhu, Bowei Bi, Xing Zhang, Binxiu Liu, Linyan Niu, & Wenqing Wang. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00590 |
| IEEE | [1] Rui Zhang, Hongwei Peng, Tianxu Zhou, Yuan Yao, Xuedong Zhu, Bowei Bi, Xing Zhang, Binxiu Liu, Linyan Niu, and Wenqing Wang, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00590. keywords: {hydrogel;musselinspired;high performance;underwater adhesion;noncovalent crosslink} |