High Throughput Screening of 3D Printable Resins: Adjusting the Surface and Catalytic Properties of Multifunctional Architectures AITranslate

Iowa State University; Iowa State University; Iowa State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Identification of 3D printable materials is crucial to expand the breadth of physical and chemical properties attainable by additive manufacturing. Stereolithography (SLA), a widespread 3D printing method based on resin photopolymerization, is ideally suited for exploring a large variety of monomers to produce functional three-dimensional solids of diverse properties. However, for most commercial SLA printers, screening monomers and resin compositions requires large volumes (∼150 mL) in each printing cycle, making the process costly and inefficient. Herein, a high throughput block (HTB) adaptor was developed to screen arrays of monomers and resin compositions, consuming lower volumes (<2 mL) and less time per print (<1/16 based on a 4 × 4 matrix) than using the original hardware. By use of this approach, a library of materials with different surface hydrophobicities were 3D printed by including long chain acrylates in the resins. In addition, several metal salts were dissolved in an acrylic acid-based resin, 3D printed, and screened as benzyl alcohol oxidation catalysts. Cu(II)-based resins produced the most active structures. Combinations of Cu(II) and long chain acrylate monomers were then used to 3D print complex catalytic architectures with varying degrees of hydrophobicity. Linear relationships were observed between 3D printed surface area, surface hydrophobicity, and catalyst performance. For a high surface Schwarz P topology ca. 60% enhancement in the catalytic activity of Cu(II) was attained by replacing the parent resin with one containing hydrophobic isodecyl groups, indicating that the immediate environment of the catalytic site affected its performance. The HTB enables fast screening of resins for 3D printing multifunctional architectures with intrinsic catalytic activity, tunable surface properties, and minimal waste.

KeyWords AITranslate

3D printing stereolithography high throughput surface hydrophobicity heterogeneous catalysis
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00598

Chinese Library Classification Number:

Citation Information:

Identification of 3D printable materials is crucial to expand the breadth of physical and chemical properties attainable by additive manufacturing. Stereolithography (SLA), a widespread 3D printing method based on resin photopolymerization, is ideally suited for exploring a large variety of monomers to produce functional three-dimensional solids of diverse properties. However, for most commercial SLA printers, screening monomers and resin compositions requires large volumes (∼150 mL) in each printing cycle, making the process costly and inefficient. Herein, a high throughput block (HTB) adaptor was developed to screen arrays of monomers and resin compositions, consuming lower volumes (<2 mL) and less time per print (<1/16 based on a 4 × 4 matrix) than using the original hardware. By use of this approach, a library of materials with different surface hydrophobicities were 3D printed by including long chain acrylates in the resins. In addition, several metal salts were dissolved in an acrylic acid-based resin, 3D printed, and screened as benzyl alcohol oxidation catalysts. Cu(II)-based resins produced the most active structures. Combinations of Cu(II) and long chain acrylate monomers were then used to 3D print complex catalytic architectures with varying degrees of hydrophobicity. Linear relationships were observed between 3D printed surface area, surface hydrophobicity, and catalyst performance. For a high surface Schwarz P topology ca. 60% enhancement in the catalytic activity of Cu(II) was attained by replacing the parent resin with one containing hydrophobic isodecyl groups, indicating that the immediate environment of the catalytic site affected its performance. The HTB enables fast screening of resins for 3D printing multifunctional architectures with intrinsic catalytic activity, tunable surface properties, and minimal waste.

quote

GB/T 7714-2015 [1] J. Sebastián Manzano, Hsin Wang, Igor I. Slowing. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00598.
MLA [1] J. Sebastián Manzano, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00598.
APA [1] J. Sebastián Manzano, Hsin Wang, & Igor I. Slowing. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00598
IEEE [1] J. Sebastián Manzano, Hsin Wang, and Igor I. Slowing, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00598. keywords: {3D printing;stereolithography;high throughput;surface hydrophobicity;heterogeneous catalysis}