Large-capacity H_2 Pressure Recovery Equipment from H_2-Reduction Furnance for W/Mo Production AITranslate
Abstract AITranslate
Brief description is made of the present status of equipment for excess H2 high-pressure and pressure recovery from reduction furnace.It focused on the operating process and characteristics of the first large capacity H2 pressure recovery equipment from reduction furnace.The said equipment is characterized by large capacity,advanced technology,PLC fully-automatic operation control.Through operating practice,the main technical specificatioms have met the design requirement.
KeyWords AITranslate
1王廉舫.水电解制氢氧[M].湖南:株洲钻石印刷厂,1995..
2陈霖新 等.氢气生产与纯化[M].哈尔滨:黑龙江科学技术出版社,1983..
1范启萍.一种新型节能装置——氢气回收装置[J].设备管理与维修,2008(2):54-55. 被引量:2
1梁静,李来平,张新.氨分解制氢在钼加工行业的应用进展[J].中国钼业,2011,35(1):46-48. 被引量:3
2王庆强,许云东,李丹柯.光亮退火炉氢气回收技术[J].中国仪器仪表,2017(2):34-37. 被引量:1
1陈平,彭科席,谭小木.变压吸附技术应用小结[J].化肥工业,2000,27(2):27-29. 被引量:4
2韩炜.含氟废水处理工程实例[J].中国科技博览,2009(10):284-284. 被引量:1
3赵海军,延凤英,高娃,王永刚.氯酸钠副产氢气回收利用工艺探讨[J].中国氯碱,2016(3):43-44.
4陈宇.江苏省含多氯联苯电力设备现状与环境管理对策[J].污染防治技术,2012,25(3):29-30. 被引量:3
5史利芳,潘利祥,李朝晖,赵良庆,李冬.含油污泥处理技术及相关设备现状[J].环境工程,2015,33(S1):526-529. 被引量:17
6李明.云南省电磁辐射设备现状与环境影响分析[J].环境科学导刊,2011,30(2):33-35.
7于洪波.探讨电除尘器技术与设备的现状[J].中国新技术新产品,2015(9):168-168.
8张金明,杨传遍,袁春林,段玖祥.粉煤灰分选设备综述及国产设备现状与研制方向[J].电力环境保护,1996,12(1):41-46. 被引量:1
9窦岩.炼厂催化干气氢气回收工艺选择[J].中国科技博览,2016,0(2):245-246.
10钱济明.气体膜分离技术的发展与应用概况[J].化工设计通讯,1996,22(1):20-21.
Basic Information:
DOI:
Chinese Library Classification Number:X756[环境科学与工程—环境工程]
Citation Information:
Brief description is made of the present status of equipment for excess H2 high-pressure and pressure recovery from reduction furnace.It focused on the operating process and characteristics of the first large capacity H2 pressure recovery equipment from reduction furnace.The said equipment is characterized by large capacity,advanced technology,PLC fully-automatic operation control.Through operating practice,the main technical specificatioms have met the design requirement.
quote
| GB/T 7714-2015 | [1] ZHU Tong-qing. Large-capacity H_2 Pressure Recovery Equipment from H_2-Reduction Furnance for W/Mo Production[J]. Rare Metals and Cemented Carbides, 2003(2): 42-44. |
| MLA | [1] ZHU Tong-qing. "Large-capacity H_2 Pressure Recovery Equipment from H_2-Reduction Furnance for W/Mo Production." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 42-44. |
| APA | [1] ZHU Tong-qing. (2003). Large-capacity H_2 Pressure Recovery Equipment from H_2-Reduction Furnance for W/Mo Production. Rare Metals and Cemented Carbides(2), 42-44. |
| IEEE | [1] ZHU Tong-qing, "Large-capacity H_2 Pressure Recovery Equipment from H_2-Reduction Furnance for W/Mo Production," Rare Metals and Cemented Carbides, no. 2, pp. 42-44, 2003. keywords: {H_2 reduction furnace excess;H_2;pressure recovery;H_2 reutilization} |