Improvement of Na Reduction Process of Low-oxide Ta Powder in Large Reactor AITranslate
Abstract AITranslate
The paper describes the study and improvement of Na reduction process of low-oxide Ta powder in D700mm large reactor.The results showed that the improved process has basically solved the problem of the control of process parameters and operation problem.The oxygen content in the resultant Ta powder can be controlled at about 1%.
KeyWords AITranslate
1潘伦桃 等.钠还原钽粉的显微结构[A]..昆明:稀有金属冶金学会1998年年会[C].,1998..
1苍大强,黄永强,张广兵,邓小明,唐庆广.南钢高炉煤气布袋除尘的应用[J].炼铁,2006,25(5):40-42.
2徐纪山,王红斌,何小平.太钢3号高炉提高煤比的实践[J].炼铁,2009(5):30-32. 被引量:3
3田欣,刘连继,宋润平,王沧,时越.唐钢炼铁厂(北区)提高烧结机利用系数的技术研究与实践[J].金属世界,2007(4):48-50.
4В.С.Игнатьев,张文成.硅锰铝铁生产工艺的研究与改进[J].铁合金,1989(6):53-54.
5倪满森.有关连铸高拉速中的工艺操作问题[J].连铸,2000(6):21-24. 被引量:2
6王运国.提高高炉喷煤比的研究与改进[J].本钢技术,2002(6):5-6.
7陈炽,李志伟,张宇.扒渣站系统的研究与改进[J].山西冶金,2009,32(2):52-54.
8刘小鸥,祁和平,张良忠,俞波.平炉供风工艺的研究与改进[J].武钢技术,1994,32(3):8-12. 被引量:3
9武钢二炼钢厂在线热换透气砖攻关成功[J].包钢科技,2006,32(2):66-66.
10耿继双,李泽林,朱晓雷,齐志宇,梅雪辉.高碳钢小方坯絮流原因及解决措施[J].辽宁科技大学学报,2014,37(3):257-260.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
The paper describes the study and improvement of Na reduction process of low-oxide Ta powder in D700mm large reactor.The results showed that the improved process has basically solved the problem of the control of process parameters and operation problem.The oxygen content in the resultant Ta powder can be controlled at about 1%.
quote
| GB/T 7714-2015 | [1] HE Xiao, FENG Jia-chun, YANG Yu-hai. Improvement of Na Reduction Process of Low-oxide Ta Powder in Large Reactor[J]. Rare Metals and Cemented Carbides, 2003(2): 39-41. |
| MLA | [1] HE Xiao, et al., "Improvement of Na Reduction Process of Low-oxide Ta Powder in Large Reactor." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 39-41. |
| APA | [1] HE Xiao, FENG Jia-chun, & YANG Yu-hai. (2003). Improvement of Na Reduction Process of Low-oxide Ta Powder in Large Reactor. Rare Metals and Cemented Carbides(2), 39-41. |
| IEEE | [1] HE Xiao, FENG Jia-chun, and YANG Yu-hai, "Improvement of Na Reduction Process of Low-oxide Ta Powder in Large Reactor," Rare Metals and Cemented Carbides, no. 2, pp. 39-41, 2003. keywords: {large reactor;Na reduction;low-oxide Ta powder} |