Study on Microstructure and Mechanical Properties of High Strength Titanium Alloy Cold-Rolled Tubes AITranslate

Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cold compression tests of Ti-1300 alloy were carried out by Gleeble—3800 simulated testing machine.The effects of extrusion temperature,cold rolling reduction and heat treatment on the microstructure and mechanical properties of Ti-1300 alloy cold-rolled tubes were investigated through tensile tests at room temperature and microstructure observation.The results show that the Ti-1300 alloy cold-rolled tubes with 30% reduction extruded at the transformation temperature have a good strength-plasticity match.After solid solution treatment,cold-rolled tubes have lower strength and better plasticity,and the α+β two-phase solid solution microstructure mainly consists of a large number of spherical or elongated α phase and resi-dual metastable β phase.The β phase solid solution microstructure is mainly composed of equiaxed β grains.The strength of cold-rolled tubes in aging state is significantly improved,and their microstructure is mainly composed of spherical or elongated primary α phase,acicular secondary α phase and β matrix.

KeyWords AITranslate

Ti-1300 titanium alloy extrusion temperature cold rolling reduction solid solution and aging microstructure mechanical property

1卢金文,葛鹏,赵永庆,李倩,周伟,洪权.热加工工艺对Ti-1300合金轧制棒材显微组织的影响[J].稀有金属材料与工程,2014,43(6):1441-1446. 被引量:4

2江志强,杨合,詹梅,许旭东,李光俊.钛合金管材研制及其在航空领域应用的现状与前景[J].塑性工程学报,2009,16(4):44-50. 被引量:91

3南莉,杨亚社,齐元昊,罗登超,杨永福,曲恒磊,杨建朝.航空用高强TA18钛合金管材的轧制工艺[J].稀有金属材料与工程,2013,42(1):166-170. 被引量:16

4席锦会,杨亚社,南莉,舒滢,曲恒磊,杨建朝.航空导管用TA18钛合金管材研制[J].钛工业进展,2011,28(5):34-37. 被引量:13

5廖强,曲恒磊,杨亚社,南莉,舒滢,李刚,杨建朝.冷轧道次变形率对TA18钛合金管材组织与拉伸性能的影响[J].钛工业进展,2012,29(1):26-28. 被引量:9

6雷江,马小菊,尉北玲,李明强.冷轧生产TA18钛合金小规格厚壁管材加工工艺研究[J].钛工业进展,2012,29(1):36-38. 被引量:6

7赵映辉,葛鹏,赵永庆,杨冠军,汶建宏.Ti-1300合金的热变形行为研究[J].稀有金属材料与工程,2009,38(1):46-49. 被引量:22

8万明攀,赵永庆,曾卫东,马瑞,边红岩.固溶温度对Ti-1300合金组织与性能的影响[J].稀有金属材料与工程,2015,44(5):1209-1213. 被引量:6

9侯红苗,黄朝文,赵恒章,张永强.挤压态Ti-1300合金管材高温变形行为及本构模型[J].热加工工艺,2017,46(20):100-103. 被引量:2

1邱岩,张俊杰,韩琛宜,段晓辉,王文波,傅开.热处理工艺对TA17钛合金棒材组织与性能的影响[J].锻造与冲压,2023(15):68-70.

2杨奇,惠松骁,叶文君,徐哲,代春,王俭,高颀.冷轧TA18钛合金管材退火织构的形成机制[J].稀有金属材料与工程,2023,52(3):899-910.

3冯欣雨,肖晖,李泉辉,梁朝阳,钟国海,刘峻溢,秦启雯.致密砂岩水力裂缝特征实验研究[J].非常规油气,2023,10(4):132-138.

4朱小勇,邢远,江健,王莹,栾佰峰.中间道次退火对Ti-3Al-2.5V管材组织和性能的影响[J].钢铁钒钛,2023,44(3):45-51.

5杨建东.钕钆变质镁铝基合金的固溶及时效行为[J].西安工程大学学报,2023,37(4):56-63.

6刘文俊,罗斌,武永.2A97铝锂合金三层空心结构件超塑成形/扩散连接工艺[J].锻压技术,2023,48(8):78-82.

7张元东,王晓巍,王德勇,张安,车安达.热处理温度和冷却方式对TC32合金组织和性能的影响[J].锻造与冲压,2023(15):52-58.

8张明达,史栋刚,胡春东,曹京霞,黄浩,黄旭.初生α相对Ti6242s合金在保载疲劳载荷作用下微区塑性变形的影响[J].稀有金属材料与工程,2023,52(7):2317-2325.

9王清曌.Q355B钢连续冷却转变曲线及电弧焊工艺优化[J].金属加工:热加工,2023(9):80-86.

10熊信发,王校培,王坤,彭锦峰,蔡登安,周光明.三维编织复合材料圆管轴向压缩性能及破坏机理[J].南京航空航天大学学报,2023,55(4):702-710.

Basic Information:

DOI:

Chinese Library Classification Number:TG337.6[金属学及工艺—金属压力加工]

Citation Information:

Cold compression tests of Ti-1300 alloy were carried out by Gleeble—3800 simulated testing machine.The effects of extrusion temperature,cold rolling reduction and heat treatment on the microstructure and mechanical properties of Ti-1300 alloy cold-rolled tubes were investigated through tensile tests at room temperature and microstructure observation.The results show that the Ti-1300 alloy cold-rolled tubes with 30% reduction extruded at the transformation temperature have a good strength-plasticity match.After solid solution treatment,cold-rolled tubes have lower strength and better plasticity,and the α+β two-phase solid solution microstructure mainly consists of a large number of spherical or elongated α phase and resi-dual metastable β phase.The β phase solid solution microstructure is mainly composed of equiaxed β grains.The strength of cold-rolled tubes in aging state is significantly improved,and their microstructure is mainly composed of spherical or elongated primary α phase,acicular secondary α phase and β matrix.

quote

GB/T 7714-2015 [1] QI Yun-lian, CAI Jian-hua, XIN She-wei, et al. Study on Microstructure and Mechanical Properties of High Strength Titanium Alloy Cold-Rolled Tubes[J]. Rare Metals and Cemented Carbides, 2023(4): 79-82.
MLA [1] QI Yun-lian, et al., "Study on Microstructure and Mechanical Properties of High Strength Titanium Alloy Cold-Rolled Tubes." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 79-82.
APA [1] QI Yun-lian, CAI Jian-hua, XIN She-wei, SUN Hua-mei, ZENG Li-ying, & ZHANG Si-yuan. (2023). Study on Microstructure and Mechanical Properties of High Strength Titanium Alloy Cold-Rolled Tubes. Rare Metals and Cemented Carbides(4), 79-82.
IEEE [1] QI Yun-lian, CAI Jian-hua, XIN She-wei, SUN Hua-mei, ZENG Li-ying, and ZHANG Si-yuan, "Study on Microstructure and Mechanical Properties of High Strength Titanium Alloy Cold-Rolled Tubes," Rare Metals and Cemented Carbides, no. 4, pp. 79-82, 2023. keywords: {Ti-1300 titanium alloy;extrusion temperature;cold rolling reduction;solid solution and aging;microstructure;mechanical property}