Effects of Antimony on Grains and Eutectic Si of Hypoeutectic Al-Si Alloy under Gravity Sand Casting Conditions AITranslate
Abstract AITranslate
The effects of antimony(Sb) on grains and eutectic Si of hypoeutectic Al-Si alloy under gravity sand casting conditions were investigated by solidification temperature-time curves,polarized light microscope(PLM),scanning electron microscope(SEM),electron backscattered diffraction(EBSD),transmission electron microscope(TEM),and energy disperse spectroscope(EDS).The results show that the addition of Sb to the Al-7Si alloy results in a decrease in the nucleation temperature of primary α-Al grains and eutectic Si.The nucleation of primary α-Al grains becomes more difficult,and their average size increases from 319 μm to 353 μm.The mechanism of Sb modifying eutectic Si is that with Sb addition,the nucleation temperature of eutectic Si decreases,the solid solubility of Si in α-Al decreases,the chemical potential increases,the velocity of Si atoms discharging from α-Al increases,the growth rate of eutectic Si increases,and finally the eutectic Si becomes shorter and narrower.Sb does not play its role of modification by acting on the nucleation cores and twins of eutectic Si.
KeyWords AITranslate
1曾友云,杨立斌.Al-Si合金活塞性能实验研究[J].国外金属热处理,2005,26(2):19-22. 被引量:4
2习仲萍,曹建英,周晓亚.内燃机活塞用稀土共晶Al-Si合金中稀土加入量的试验研究[J].现代机械,2013(2):71-73. 被引量:3
3吴振平,廖恒成,姜云峰,陈洁,孙国雄.Sr对Al-15.5Si合金共晶团大小的影响[J].特种铸造及有色合金,2005,25(4):193-195. 被引量:8
4亓效刚,陈俊华,江旭彪.锑变质共晶硅的异质形核[J].特种铸造及有色合金,2000(1):13-15. 被引量:13
1许志鹏,周鹏飞,孙瑜.Al-9Si合金中共晶Si生长机制研究[J].铸造,2023,72(4):388-393.
2马小红,徐亚军,陈长科,陈诚诚,田冬梅,王向杰.微量元素对ADC12铝合金组织及热分析结果的影响[J].轻合金加工技术,2023,51(6):8-14.
3郝春来,李振,赫丽杰,王晓民,包鑫磊,张家铭.浇注工艺对AlSi9Cu3合金凝固组织及力学性能的影响[J].铸造,2023,72(6):688-692.
4王金龙,陈卉.基于石墨烯的双频可调太赫兹吸波器[J].石化技术,2023,30(9):57-59.
5王令兆,李建委,宋栋.高硅Al-Si合金活塞材料的研究进展[J].模具制造,2023,23(8):150-152.
6寇东旭,陈重毅,陈正宗,李永清,麻永林,李一鸣.焊接热循环及峰值温度对C-HRA-2镍基合金组织演变的影响[J].稀有金属材料与工程,2023,52(7):2377-2384.
7郭皓,樊晨康,孙旭兵,杨树峰,刘威.35MnVS非调质钢针状铁素体形核原位观察[J].重型机械,2023(4):78-83.
8徐永朝,李天庆,万永杰,李远航,王凯.双相不锈钢2205激光焊接接头组织和性能研究[J].精密成形工程,2023,15(9):90-98.
9李涵,李昭东,曹杰,张可,曹燕光,雍岐龙.冷拔小口径16MnNiV无缝钢管的显微组织与力学性能演变规律[J].材料工程,2023,51(9):117-127.
10张文静,周立山,杨文博,周柄男,韩恩山,何艳贞.有机蒙脱石复合降凝剂的制备与防蜡降凝作用机理研究[J].无机盐工业,2023,55(9):81-87.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]
Citation Information:
The effects of antimony(Sb) on grains and eutectic Si of hypoeutectic Al-Si alloy under gravity sand casting conditions were investigated by solidification temperature-time curves,polarized light microscope(PLM),scanning electron microscope(SEM),electron backscattered diffraction(EBSD),transmission electron microscope(TEM),and energy disperse spectroscope(EDS).The results show that the addition of Sb to the Al-7Si alloy results in a decrease in the nucleation temperature of primary α-Al grains and eutectic Si.The nucleation of primary α-Al grains becomes more difficult,and their average size increases from 319 μm to 353 μm.The mechanism of Sb modifying eutectic Si is that with Sb addition,the nucleation temperature of eutectic Si decreases,the solid solubility of Si in α-Al decreases,the chemical potential increases,the velocity of Si atoms discharging from α-Al increases,the growth rate of eutectic Si increases,and finally the eutectic Si becomes shorter and narrower.Sb does not play its role of modification by acting on the nucleation cores and twins of eutectic Si.
quote
| GB/T 7714-2015 | [1] MAO Guo-ling, PU Bo-wen, WANG Gen-quan, et al. Effects of Antimony on Grains and Eutectic Si of Hypoeutectic Al-Si Alloy under Gravity Sand Casting Conditions[J]. Rare Metals and Cemented Carbides, 2023(4): 83-87. |
| MLA | [1] MAO Guo-ling, et al., "Effects of Antimony on Grains and Eutectic Si of Hypoeutectic Al-Si Alloy under Gravity Sand Casting Conditions." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 83-87. |
| APA | [1] MAO Guo-ling, PU Bo-wen, WANG Gen-quan, YANG Chen-fan, ZHOU Hai-tao, & HE Xiao-dong. (2023). Effects of Antimony on Grains and Eutectic Si of Hypoeutectic Al-Si Alloy under Gravity Sand Casting Conditions. Rare Metals and Cemented Carbides(4), 83-87. |
| IEEE | [1] MAO Guo-ling, PU Bo-wen, WANG Gen-quan, YANG Chen-fan, ZHOU Hai-tao, and HE Xiao-dong, "Effects of Antimony on Grains and Eutectic Si of Hypoeutectic Al-Si Alloy under Gravity Sand Casting Conditions," Rare Metals and Cemented Carbides, no. 4, pp. 83-87, 2023. keywords: {gravity sand casting;Al-Si alloy;Sb modification;primaryα-Al grain;eutectic Si} |