Study on Leaching Process of Flotation Concentrate of Vanadium-containing Carbonaceous Shale AITranslate
Abstract AITranslate
Vanadium-containing carbonaceous shale concentrate was obtained by pre-flotation of Hubei high calcium and magnesium mica carbonaceous shale containing vanadium,and then the concentrate was used as raw material for leaching experiments.The results indicate that high vanadium leaching rate of 86.18%can be obtained under the following conditions:H2SO4concentration of 30%,liquid to solid ratio of 4∶1,leaching temperature of 90 ℃,sodium fluorosilicate dosage of 16% and leaching time of 12 h.
KeyWords AITranslate
1王学文,王明玉.石煤提钒工艺现状及发展趋势[J].钢铁钒钛,2012,33(1):8-14. 被引量:36
2李昌林,周云峰,费海霞,周向阳,李劼.石煤提钒工艺研究及应用现状[J].稀有金属与硬质合金,2012,40(6):9-14. 被引量:12
3向平,冯其明,钮因健,潘安新.选矿富集阿克苏石煤钒矿中的钒[J].材料研究与应用,2010,4(1):65-70. 被引量:26
4孙伟,王丽,曹学锋,刘润清,徐龙华,韩海生.石煤提钒的浮选工艺及吸附机理[J].中国有色金属学报,2012,22(7):2069-2074. 被引量:34
5姚金江,吴海国,李婕.高钙低品位石煤提取五氧化二钒新工艺[J].湖南有色金属,2009,25(6):21-23. 被引量:18
6徐懋,黄宪法,桂林.低品位石煤浮选及提钒工艺研究[J].山西冶金,2013,36(6):6-9. 被引量:4
7武宝新,王晖,符剑刚,林清泉,王重庆.湖南某石煤钒矿选煤选钒的探索试验[J].稀有金属与硬质合金,2014,42(3):1-6. 被引量:7
8田学达,杨康,杨用龙,谢畅.添加剂SMTV01对石煤酸浸提钒的影响[J].湿法冶金,2009,28(4):218-221. 被引量:6
9吴海鹰,戴子林,谷利君,李桂英.含氟助浸剂对钒矿的硫酸浸出和萃钒的影响研究[J].矿冶工程,2010,30(2):83-84. 被引量:18
10梁泰然,戴子林,郝文彬.助浸剂对石煤提钒的作用[J].矿冶工程,2010,30(6):69-71. 被引量:14
1胡洋,何东升,王梦涛,谢志豪,张可成,朱志伟.含钒云母在硫酸溶液中的溶解行为[J].矿冶工程,2019,39(4):102-105. 被引量:4
2亢选雄,叶国华,朱思琴,梁雪崟.从含钒页岩中提取五氧化二钒的研究进展[J].钢铁钒钛,2022,43(2):25-34. 被引量:4
3王淼,温建康,李文娟,杨鑫龙,赖永传,杨洪英.选冶联合回收石煤中伴生战略金属钒镍钼的研究进展[J].稀有金属,2023,47(6):881-892.
1李望,王雯博,段理哲,朱晓波.伯胺7101萃取分离钒及有机相乳化分析[J].矿冶工程,2021,41(4):76-78.
2金永朋,李艳军,袁帅,刘杰.新疆某难处理含钒石煤焙烧—酸浸提钒试验研究[J].金属矿山,2021(9):96-101. 被引量:1
3徐旭,孙永升,靳建平,李艳军.含钒云母悬浮氧化焙烧-酸浸提钒试验研究[J].矿冶工程,2021,41(5):111-115.
4荣一阳,叶国华,亢选雄,朱思琴,梁雪崟,项新月,张云,宋昌溆.用富钒液制取V_(2)O_(5)的研究进展[J].矿冶,2023,32(3):78-86.
5张云,叶国华,梁雪崟,项新月,荣一阳,宋昌溆.页岩钒矿直接酸浸提钒的强化与活化研究进展[J].钢铁钒钛,2023,44(2):1-8.
6亢选雄,叶国华,朱思琴,梁雪崟,荣一阳,宋昌溆,项新月,张云.含钒页岩提钒尾渣资源化利用研究进展[J].现代化工,2023,43(6):67-73.
7王淼,温建康,李文娟,杨鑫龙,赖永传,杨洪英.选冶联合回收石煤中伴生战略金属钒镍钼的研究进展[J].稀有金属,2023,47(6):881-892.
8蔡俊,高峰,颜文斌,华骏.浓硫酸熟化浸出提取湘西石煤中的钒[J].稀有金属与硬质合金,2023,51(4):24-27.
1周新泉.用氟硅酸钠、硫酸铝、食盐为主要原料合成冰晶石[J].轻金属,1989(4):21-23. 被引量:5
2刘玉强.氟硅酸钠生产高分子比冰晶石[J].轻金属,1998(4):21-24. 被引量:2
3马克印,李莹.含氟烟气中氟的回收利用小型动态试验[J].包钢科技,1991,0(4):63-67.
4胡忠.在“三废”治理中开发新产品[J].湖南有色金属,1992(4):251-253.
5专利题录和文摘[J].中国钨业,1989(4):33-34.
6经济信息[J].云南冶金,1993(10):65-66.
7金专.专利文献信息[J].特种铸造及有色合金,2014(4).
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Vanadium-containing carbonaceous shale concentrate was obtained by pre-flotation of Hubei high calcium and magnesium mica carbonaceous shale containing vanadium,and then the concentrate was used as raw material for leaching experiments.The results indicate that high vanadium leaching rate of 86.18%can be obtained under the following conditions:H2SO4concentration of 30%,liquid to solid ratio of 4∶1,leaching temperature of 90 ℃,sodium fluorosilicate dosage of 16% and leaching time of 12 h.
quote
| GB/T 7714-2015 | [1] HE Dong-sheng, LI Qiao-shuang, ZHANG Jian-gang, et al. Study on Leaching Process of Flotation Concentrate of Vanadium-containing Carbonaceous Shale[J]. Rare Metals and Cemented Carbides, 2016(6): 7-9. |
| MLA | [1] HE Dong-sheng, et al., "Study on Leaching Process of Flotation Concentrate of Vanadium-containing Carbonaceous Shale." Rare Metals and Cemented Carbides, no. 6, 2016, pp. 7-9. |
| APA | [1] HE Dong-sheng, LI Qiao-shuang, ZHANG Jian-gang, LIU Xing, ZOU Jian-jun, & QIN Fang. (2016). Study on Leaching Process of Flotation Concentrate of Vanadium-containing Carbonaceous Shale. Rare Metals and Cemented Carbides(6), 7-9. |
| IEEE | [1] HE Dong-sheng, LI Qiao-shuang, ZHANG Jian-gang, LIU Xing, ZOU Jian-jun, and QIN Fang, "Study on Leaching Process of Flotation Concentrate of Vanadium-containing Carbonaceous Shale," Rare Metals and Cemented Carbides, no. 6, pp. 7-9, 2016. keywords: {vanadium-containing carbonaceous shale;flotation concentrate;leaching;leaching assistant;vanadium} |