Study on Process of Nb and Ti Separation and Extraction from Nb and Ti Rich Sulfuric Acid Solution AITranslate
Abstract AITranslate
The process was studied of Nb and Ti separation and extraction from Nb and Ti rich sulfuric acid solution with 7.84g/L Nb2O5 and 47.40g/L TiO2.Titanium was precipitated from the Nb and Ti rich sulfuric acid solution by ammonium sulfate precipitation.When the enrichment ratio is 2.5,ammonium sulfate dosage is 450g/L,precipitation time is 90 min,calcination temperature is 900℃and time is 90 min,industrial titanium dioxide with more than 93.4% TiO2 is obtained,and Ti total recovery rate is more than 95.19%.Niobium was precipitated from the titanium-precipitated solution by calcium carbonate neutralization-ammonia precipitation.When the neutralized solution pH value is about 1.0,the niobium-precipitated solution pH value is about 5.0,calcination temperature is 800℃and time is 60 min,niobium oxide concentrate with an average Nb2O5 content of 30.51%is obtained,and Nb total recovery rate is over 98.9%.
KeyWords AITranslate
1杨武斌,罗勇,单强,牛贺才,于学元.内蒙古巴尔哲稀有稀土多金属矿床特征[J].矿物学报,2009,29(S1):266-266. 被引量:8
2特大型稀土稀有金属矿山在扎鲁特旗开工建设[J].稀土信息,2010,16(2):34-34. 被引量:5
3武建斌.山西省交口县赵家圪垛稀土 铌钽矿矿床特征[J].华北国土资源,2007(1):18-19. 被引量:7
4刘牡丹,刘勇,刘珍珍.复杂稀有金属伴生矿资源的综合利用现状[J].稀有金属与硬质合金,2015,43(6):24-27. 被引量:8
5刘牡丹,刘勇,李翔,刘珍珍.某复杂稀有金属伴生矿选矿试验研究[J].有色金属:选矿部分,2016(6):60-64. 被引量:8
6李翔,刘勇,李光辉,刘牡丹,刘珍珍.从低品位稀土铌铁粗精矿中分离回收铁和稀有金属的新工艺[J].材料研究与应用,2014,8(1):67-72. 被引量:7
7刘勇,刘牡丹,刘珍珍.复杂稀有金属伴生矿富集渣提取稀土和铌的工艺研究[J].稀有金属与硬质合金,2015,43(1):21-25. 被引量:10
1刘牡丹,刘勇,刘珍珍.添加剂对低品位稀土铌铁粗精矿还原焙烧过程微观分离机制的影响[J].稀有金属与硬质合金,2018,46(2):6-10.
1北京矿冶研究总院冶金研究设计所[J].矿冶,2008,17(4).
2刘牡丹,刘勇,刘珍珍.复杂稀有金属伴生矿资源的综合利用现状[J].稀有金属与硬质合金,2015,43(6):24-27. 被引量:8
3华东发,张之洁,周朝晖,汪晓东,丁芝虎.钼酸铵除铜工艺研究[J].湿法冶金,1998(1):11-13.
4刘予成.回转窑二次焙烧提高锌矿品位的工艺研究[J].文山学院学报,2016,29(3):28-30. 被引量:2
5张悦,王思佳,薛向欣.氨水沉淀法由含钛滤液提取二氧化钛[J].化工学报,2012,63(10):3345-3349. 被引量:10
6张爽,吕仁亮,王为国,马家玉,汪铁林,王存文.低温酸浸磷钾伴生矿提钾工艺研究[J].现代化工,2015,35(5):96-100. 被引量:6
7叶龙刚,李云,唐朝波,唐谟堂,张文海.铜钴伴生硫化矿火法冶炼过程钴的分配计算[J].有色金属:冶炼部分,2014(2):5-8. 被引量:5
8刘燕,李来平,张新,蒋丽娟,林小辉,杨健,李延超.钼铼分离富集技术的研究进展[J].中国钼业,2015,39(4):6-9. 被引量:2
9王艳,周春山.铅锌冶炼渣浸出液提取镓的研究[J].稀有金属与硬质合金,2001,29(4):7-9. 被引量:3
10杜学兰,马家玉,覃远航,吴再坤,王存文.表面活性剂对磷钾伴生矿提钾过程的影响[J].有色金属:冶炼部分,2016(5):13-16. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
The process was studied of Nb and Ti separation and extraction from Nb and Ti rich sulfuric acid solution with 7.84g/L Nb2O5 and 47.40g/L TiO2.Titanium was precipitated from the Nb and Ti rich sulfuric acid solution by ammonium sulfate precipitation.When the enrichment ratio is 2.5,ammonium sulfate dosage is 450g/L,precipitation time is 90 min,calcination temperature is 900℃and time is 90 min,industrial titanium dioxide with more than 93.4% TiO2 is obtained,and Ti total recovery rate is more than 95.19%.Niobium was precipitated from the titanium-precipitated solution by calcium carbonate neutralization-ammonia precipitation.When the neutralized solution pH value is about 1.0,the niobium-precipitated solution pH value is about 5.0,calcination temperature is 800℃and time is 60 min,niobium oxide concentrate with an average Nb2O5 content of 30.51%is obtained,and Nb total recovery rate is over 98.9%.
quote
| GB/T 7714-2015 | [1] LIU Mu-dan, LIU Yong, LIU Zhen-zhen, et al. Study on Process of Nb and Ti Separation and Extraction from Nb and Ti Rich Sulfuric Acid Solution[J]. Rare Metals and Cemented Carbides, 2016(6): 10-12. |
| MLA | [1] LIU Mu-dan, et al., "Study on Process of Nb and Ti Separation and Extraction from Nb and Ti Rich Sulfuric Acid Solution." Rare Metals and Cemented Carbides, no. 6, 2016, pp. 10-12. |
| APA | [1] LIU Mu-dan, LIU Yong, LIU Zhen-zhen, & ZHOU Ji-kui. (2016). Study on Process of Nb and Ti Separation and Extraction from Nb and Ti Rich Sulfuric Acid Solution. Rare Metals and Cemented Carbides(6), 10-12. |
| IEEE | [1] LIU Mu-dan, LIU Yong, LIU Zhen-zhen, and ZHOU Ji-kui, "Study on Process of Nb and Ti Separation and Extraction from Nb and Ti Rich Sulfuric Acid Solution," Rare Metals and Cemented Carbides, no. 6, pp. 10-12, 2016. keywords: {niobium;titanium;separation;extraction;sulfuric acid leaching solution;complex rare metal associated ore} |