Difficulties in PIM Process of Cemented Carbides and Their solution AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

PIM(powder injection molding) is an advanced forming technology and is drawing more and more attention.Powder injection molding of cemented carbides is a complicated process due to the materials'characteristics.There are still several big problems to be solved to improve the technology.In this Paper,defect control,carbon control,dimension precision control and its mechanical property improvement are discussed and some measures are proposed to solve the problems.

KeyWords AITranslate

cemented carbides powder injection molding carbon control dimension precision mechanical properties

1SUNG Hwan-jin,et al. Application of PIM for Manufacturing WC-Co Milling Inserts[J].Journal of the Japan Society of Powder and Powder Metallurgy,1999,46(8):887.

2曲选辉,颜寒松,黄伯云.金属粉末注射成形粘结剂的发展[J].粉末冶金技术,1997,15(1):61-65. 被引量:44

3LIN S T,et al.Extraction Debinding of Injection Molded Parts by Condensed Solvent[J].PMI,1989,21(5):19.

4LI Y,et al.Viscosity and Melt Rheology of Metal Injection Molding Feedstocks[J].Powder Metallurgy,1999,42(1):86.

5GERMAN R M.Powder Injection Molding[M].New Jersey:MPIF,1990.61.

6Li, Yimin, Huang, Baiyun, Qu, Xuanhui.IMPROVEMENT OF RHEOLOGICAL AND SHAPE RETENTION PROPERTIES OF WAX-BASED MIM BINDER BY MULTI-POLYMER COMPONENTS[J].中国有色金属学会会刊:英文版,1999,0(1):24-31. 被引量:7

7曲选辉,钟伟,李益民,张健,钟孝贤.硬质合金注射成形制品中的缺陷控制[J].稀有金属材料与工程,2000,29(5):332-335. 被引量:6

8MARTYN M T,et al.The Processing of Hardmetal Components by Powder Injection Moulding[J].Int J of Refractory Metals & Hard Materials 1993-1994,12:61.

9KISHOR M Kulkami.Factors Affecting Dimensional Precision of MIM Parts Under Production Condition[C]. Advances in Powder Metallurgy & Particulate Materials.New Jersey:MPIF,1994.157.

10BANKORIC D R,et al.Optimization of Debinding Cycles in Powder Injection Molding[C].Proceedings of the 1990 Powder Metallurgy Conference and Exhibition(Part 3).New Jerseg: MPIF,1990.223.

1林信平,曹顺华,李炯义.温压工艺在硬质合金制备中的应用[J].中国钼业,2004,28(3):29-33. 被引量:3

2李志希,范景莲,黄伯云,成会朝.超细WC-Co硬质合金注射成形技术的研究现状[J].粉末冶金工业,2004,14(3):23-28. 被引量:6

3李志希,范景莲,刘涛,肖琼.硬质合金注射工艺参数的研究[J].硬质合金,2005,22(1):32-35. 被引量:4

1范景莲,刘涛,成会朝.难熔钨合金与硬质合金的研究新动向[J].中国钨业,2005,20(3):17-20. 被引量:14

2范景莲,周红翠,成会朝,刘勋,刘涛,廖雪松.WC-10Co-1TaC硬质合金异形刀片注射成形与合金性能的研究[J].中国钨业,2006,21(2):20-24. 被引量:1

3于学勇,潘毅,华征潇,程凤军.超细粉末注射成型技术的研究进展[J].常熟理工学院学报,2006,20(6):70-73. 被引量:1

4于学勇,华征潇,程凤军.超细粉末注射成型技术研究的新进展[J].模具工业,2007,33(3):6-9.

5于学勇,华征潇,程凤军.MIM方法制备高硬度不锈钢剪刀的工艺研究[J].常熟理工学院学报,2007,21(2):63-66.

6范景莲,廖雪松,成会朝,刘涛,田家敏.“一步热脱脂+烧结”工艺对注射成形硬质合金显微结构与性能的影响[J].稀有金属材料与工程,2008,37(12):2236-2239. 被引量:4

7孙丹,张鹤年,孙卫权,李广生.一种新型超细硬质合金棒料挤压成形剂的设计[J].硬质合金,2009,26(3):176-179. 被引量:5

8谢兴铖,林晨光,贾成厂,曹瑞军,林中坤.超细WC-Co硬质合金注射成形的研究进展[J].材料导报,2012,26(23):99-103. 被引量:3

9何荣,胡业奇,许龙山.粉末冶金零件生坯切削加工性能研究进展[J].稀有金属与硬质合金,2013,41(1):60-65. 被引量:2

10周红翠,范景莲,成会朝,刘孙和.WC-Co硬质合金刀片注射成型参数优化研究[J].硬质合金,2013,30(4):210-216. 被引量:4

1祝宝军,曲选辉,秦明礼,肖平安.硬质合金注射成形过程中的难点问题及解决方法[J].粉末冶金材料科学与工程,2001,6(3):173-178.

2杨建国.3号高炉炉顶计算机控制系统[J].梅山科技,1996(4):50-53.

3Gille.,G,李学芳.WC粉末特性与钨钴硬质合金性能和烧结行为的关系[J].国外难熔金属与硬质材料,1996,12(2):12-23. 被引量:3

4娄宏达,黄志强.中高碳钢控碳技术[J].重钢技术,2015,58(1):1-6.

5胡顺遂,张立.碳化钨基硬质合金控碳问题探讨[J].稀有金属与硬质合金,1995,23(2):14-16. 被引量:4

6张利民,乔峥.65Mn钢控碳工艺调整[J].河北冶金,2014(10):43-44.

7范景莲,廖雪松,成会朝,刘涛,田家敏.“一步热脱脂+烧结”工艺对注射成形硬质合金显微结构与性能的影响[J].稀有金属材料与工程,2008,37(12):2236-2239. 被引量:4

8胡玫槐.提高中间罐连浇炉数有进展[J].连铸,1994,0(2):45-45.

9和宁波.溅渣护炉技术在我国的应用[J].河南冶金,1999(5):3-5. 被引量:2

10陈绍衣,赵秦生,张武城,黄珣,张俊熙.碳化钨粉分级和凿岩用硬质合金的制取[J].稀有金属与硬质合金,1992,20(3):12-15. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF124.39[冶金工程—粉末冶金]

Citation Information:

PIM(powder injection molding) is an advanced forming technology and is drawing more and more attention.Powder injection molding of cemented carbides is a complicated process due to the materials'characteristics.There are still several big problems to be solved to improve the technology.In this Paper,defect control,carbon control,dimension precision control and its mechanical property improvement are discussed and some measures are proposed to solve the problems.

quote

GB/T 7714-2015 [1] ZHU Bao-jun, QU Xuan-hui, QIN Ming-li, et al. Difficulties in PIM Process of Cemented Carbides and Their solution[J]. Rare Metals and Cemented Carbides, 2001(2): 20-24.
MLA [1] ZHU Bao-jun, et al., "Difficulties in PIM Process of Cemented Carbides and Their solution." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 20-24.
APA [1] ZHU Bao-jun, QU Xuan-hui, QIN Ming-li, & XIAO Ping-an. (2001). Difficulties in PIM Process of Cemented Carbides and Their solution. Rare Metals and Cemented Carbides(2), 20-24.
IEEE [1] ZHU Bao-jun, QU Xuan-hui, QIN Ming-li, and XIAO Ping-an, "Difficulties in PIM Process of Cemented Carbides and Their solution," Rare Metals and Cemented Carbides, no. 2, pp. 20-24, 2001. keywords: {cemented carbides;powder injection molding;carbon control;dimension precision;mechanical properties}