daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

General trends in the structural, electronic and elastic properties of the M3AlC2 phases (M = transition metal): A first-principle study AITranslate

Harbin Institute of Technology; Harbin Institute of Technology; Harbin Normal University; Harbin Institute of Technology; Harbin Institute of Technology; Drexel University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper, the first-principles pseudopotential total energy method is used to predict the structural, electronic and elastic properties of the M3AlC2 (MAX) phases, where M = 3d, 4d, and 5d early transition metals. Specifically, the effects of the valence electron concentrations (VEC) of Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W were examined. The lattice constants are a linear function of the atomic diameter of the M element. In general, M d–Al p hybridizations locate just below the Fermi level and are weaker than the M d–C p bonds, which are deeper in energy. The bulk moduli of the ternary carbides are found to be proportional to the bulk moduli of the corresponding binary carbides. Because the M–Al bonds are less stiff than the M–C bonds, the latter are mainly responsible for the high bulk moduli of the M3AlC2 phases. The M–Al bonds, on the other hand, play a critical role in decreasing the bulk moduli compared to the binary carbides.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.06.012

Chinese Library Classification Number:

Citation Information:

In this paper, the first-principles pseudopotential total energy method is used to predict the structural, electronic and elastic properties of the M3AlC2 (MAX) phases, where M = 3d, 4d, and 5d early transition metals. Specifically, the effects of the valence electron concentrations (VEC) of Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W were examined. The lattice constants are a linear function of the atomic diameter of the M element. In general, M d–Al p hybridizations locate just below the Fermi level and are weaker than the M d–C p bonds, which are deeper in energy. The bulk moduli of the ternary carbides are found to be proportional to the bulk moduli of the corresponding binary carbides. Because the M–Al bonds are less stiff than the M–C bonds, the latter are mainly responsible for the high bulk moduli of the M3AlC2 phases. The M–Al bonds, on the other hand, play a critical role in decreasing the bulk moduli compared to the binary carbides.

quote

GB/T 7714-2015 [1] Xiaodong He, Yuelei Bai, Chuncheng Zhu, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.06.012.
MLA [1] Xiaodong He, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.06.012.
APA [1] Xiaodong He, Yuelei Bai, Chuncheng Zhu, Yue Sun, Mingwei Li, & M.W. Barsoum. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.06.012
IEEE [1] Xiaodong He, Yuelei Bai, Chuncheng Zhu, Yue Sun, Mingwei Li, and M.W. Barsoum, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.06.012.