daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Easy to Pattern, Chemically Resistant One-Dimensional Polymer Photonic Crystals AITranslate

The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

One-dimensional photonic crystals (1D-PCs) are able to reflect certain wavelengths of light using periodic dielectric layers with mismatched refractive indices. Many polymer and inorganic systems exist for fabricating 1D-PCs, but challenges remain to create a 1D-PC that is stable under harsh chemical conditions. Furthermore, patterning 1D-PCs to provide spatial control of reflected light often requires complicated synthetic and/or processing steps. Herein, we demonstrate a relatively simple and scalable approach to fabricate chemically resistant 1D-PCs from two cheap and commercially available materials, poly(vinylidene fluoride-co-chlorotrifluoroethylene) (PVDF-CTFE) and phenolic resin (resol), in which the reflected wavelengths of the 1D-PC can be simply tuned by adjusting the substrate moving velocity during the dip coating process. The two layers have a naturally high refractive index contrast (Δn ≈ 0.24) and are able to exhibit high stability when exposed to various organic solvents and acidic and basic aqueous solutions. Moreover, significantly different hydrophobicity between the layers offers an easy-to-pattern approach by using a poly(dimethylsiloxane) pad to spatially control the wettability of PVDF-CTFE during a surface functionalization step, thus directing the deposition of the sequential resol layer. We believe this work provides a facile approach for patterning 1D-PCs with tunable reflecting behavior and excellent chemical stability.

KeyWords AITranslate

fluoropolymer resol dip coating thin films interfacial engineering
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00228

Chinese Library Classification Number:

Citation Information:

One-dimensional photonic crystals (1D-PCs) are able to reflect certain wavelengths of light using periodic dielectric layers with mismatched refractive indices. Many polymer and inorganic systems exist for fabricating 1D-PCs, but challenges remain to create a 1D-PC that is stable under harsh chemical conditions. Furthermore, patterning 1D-PCs to provide spatial control of reflected light often requires complicated synthetic and/or processing steps. Herein, we demonstrate a relatively simple and scalable approach to fabricate chemically resistant 1D-PCs from two cheap and commercially available materials, poly(vinylidene fluoride-co-chlorotrifluoroethylene) (PVDF-CTFE) and phenolic resin (resol), in which the reflected wavelengths of the 1D-PC can be simply tuned by adjusting the substrate moving velocity during the dip coating process. The two layers have a naturally high refractive index contrast (Δn ≈ 0.24) and are able to exhibit high stability when exposed to various organic solvents and acidic and basic aqueous solutions. Moreover, significantly different hydrophobicity between the layers offers an easy-to-pattern approach by using a poly(dimethylsiloxane) pad to spatially control the wettability of PVDF-CTFE during a surface functionalization step, thus directing the deposition of the sequential resol layer. We believe this work provides a facile approach for patterning 1D-PCs with tunable reflecting behavior and excellent chemical stability.

quote

GB/T 7714-2015 [1] Mark Robertson, Ashley Sanford, Zhe Qiang. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00228.
MLA [1] Mark Robertson, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00228.
APA [1] Mark Robertson, Ashley Sanford, & Zhe Qiang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00228