Near-Zero Azimuthal Anchoring of Liquid Crystals Assisted by Viscoelastic Bottlebrush Polymers AITranslate

Kyoto University; National Institute of Advanced Science and Technology (AIST); Japan Advanced Institute of Science and Technology; Kyoto University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this article, we revealed the mechanism of weak anchoring properties of liquid crystals (LCs) on cross-linked films of bottlebrushes consisting of poly(hexyl methacrylate) (PHMA) and poly(ethyl methacrylate) (PEMA). First, azimuthal anchoring coefficients, A2, of a LC were estimated using these two systems from the voltage–transmittance curves at different temperatures. The PHMA and PEMA systems showcased a temperature-dependent weak anchoring property, with A2 decreasing as the temperature was increased. Second, the degree of swelling of these two systems (with cross-linked films) by the LCs was determined and compared with the phase diagrams of the corresponding mixtures without cross-linking, suggesting that the relaxation dynamics of side chains of bottlebrushes was retained even after the cross-linking. Finally, rheological measurements were conducted for the LC/bottlebrush mixtures to discuss the dynamics of the LC-swollen cross-linked bottlebrush films, which clearly demonstrated the relaxation behavior of the side chains. Assuming the time scale for the determination of A2, the characteristic temperature corresponding to the side-chain motion was reasonably correlated with the decreasing temperature behavior of A2. As a consequence, weak anchoring could be explained by the polymer chain dynamics, which was revealed to be accelerated by the bottlebrush architecture as well as the swelling with LCs, depending on the affinity of the bottlebrush component with the target LC.

KeyWords AITranslate

zero anchoring mechanism liquid crystal polymerchain dynamics bottlebrush polymer interfacial interaction rheology Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00227

Chinese Library Classification Number:

Citation Information:

In this article, we revealed the mechanism of weak anchoring properties of liquid crystals (LCs) on cross-linked films of bottlebrushes consisting of poly(hexyl methacrylate) (PHMA) and poly(ethyl methacrylate) (PEMA). First, azimuthal anchoring coefficients, A2, of a LC were estimated using these two systems from the voltage–transmittance curves at different temperatures. The PHMA and PEMA systems showcased a temperature-dependent weak anchoring property, with A2 decreasing as the temperature was increased. Second, the degree of swelling of these two systems (with cross-linked films) by the LCs was determined and compared with the phase diagrams of the corresponding mixtures without cross-linking, suggesting that the relaxation dynamics of side chains of bottlebrushes was retained even after the cross-linking. Finally, rheological measurements were conducted for the LC/bottlebrush mixtures to discuss the dynamics of the LC-swollen cross-linked bottlebrush films, which clearly demonstrated the relaxation behavior of the side chains. Assuming the time scale for the determination of A2, the characteristic temperature corresponding to the side-chain motion was reasonably correlated with the decreasing temperature behavior of A2. As a consequence, weak anchoring could be explained by the polymer chain dynamics, which was revealed to be accelerated by the bottlebrush architecture as well as the swelling with LCs, depending on the affinity of the bottlebrush component with the target LC.

quote

GB/T 7714-2015 [1] Yuji Kinose, Keita Sakakibara, Osamu Sato, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00227.
MLA [1] Yuji Kinose, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00227.
APA [1] Yuji Kinose, Keita Sakakibara, Osamu Sato, & Yoshinobu Tsujii. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00227
IEEE [1] Yuji Kinose, Keita Sakakibara, Osamu Sato, and Yoshinobu Tsujii, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00227. keywords: {zero anchoring mechanism;liquid crystal;polymerchain dynamics;bottlebrush polymer;interfacial interaction;rheology;Show More}