Principles of Variable-Parameter Ion Exchange and its Application in Tungsten Metallurgy AITranslate
Abstract AITranslate
The distributing rules of adsorbed ions in exchange column and the influencing factors during dynamic ion exchange are acquired through theoretical analysis.On the above basis,a novel idea of variable-parameter ion exchange and its principles are presented.The application of the variable-parameter ion exchange process in tungsten metallurgy proves its advantages.
KeyWords AITranslate
1徐迎春,姜萍.关于提高201×7型树脂对钨交换容量的研究[J].中国钨业,2000,15(3):36-37. 被引量:9
2姜萍,徐迎春.离子交换解吸工艺的改进与实践[J].稀有金属与硬质合金,2001,29(1):47-49. 被引量:8
3孙培梅,谢武明,李洪桂,李运姣,赵中伟,霍广生,孙召明.Na_2WO_4溶液离子交换中WO_4^(2-)和SO_4^(2-)的吸附性能[J].中南工业大学学报,2002,33(3):238-241. 被引量:3
4李洪桂,李波,赵中伟.钨冶金离子交换新工艺研究[J].稀有金属与硬质合金,2007,35(1):1-4. 被引量:13
1王旭,廖春发.熔盐电解法制备金属钨粉的技术分析及发展前景[J].稀有金属,2011,35(4):587-592. 被引量:5
2刘峙嵘,王长福,赖毅,张寰,王云,周利民.偏钛酸型离子交换剂的制备及其对锂的富集性能[J].过程工程学报,2015,15(1):147-152. 被引量:2
1叶章根,陈松,李文良,吴延科,王力军.熔盐电解精炼铪的研究[J].稀有金属,2012,36(5):791-798. 被引量:13
2廖春发,房孟钊,王旭,汤浩,罗林生.NaCl-KCl-Na_2WO_4共融体系的方波伏安法分析[J].有色金属科学与工程,2015,6(4):6-9. 被引量:3
3张洁,欧阳云,邹海晶,冉敬文.失效离子筛型锂吸附剂的性能恢复[J].黄冈师范学院学报,2015,35(6):40-41. 被引量:1
4陈自正,沈卫华,陈立芳,成洪业,漆志文.纳米H_2TiO_3锂吸附剂的水热合成及其吸附性能[J].中国有色金属学报,2017,27(3):547-554. 被引量:6
5房孟钊,廖春发,王旭,王坤,焦芸芬,李伟,宁瑞,余珊.CaWO4在NaCl-CaCl2熔盐体系中溶解性能的研究[J].有色金属:冶炼部分,2018,0(12):33-36.
6李明辉.我国钨电极行业现状及未来发展趋势[J].世界有色金属,2019,0(15):140-141. 被引量:4
7喻相标,肖杰,郭少毓,肖义钰,廖春发,姜平国.蓝钨氢还原制备钨粉工艺研究[J].有色金属科学与工程,2021,12(3):35-41. 被引量:4
1李鹏,王新春.钢包底吹氩气变参数PID控制系统的实现[J].内蒙古科技与经济,2016(9):62-62.
2刘旭东,朱苗勇,邹俊苏,宋景欣,程乃良.连铸板坯凝固传热过程的计算机模拟[J].材料与冶金学报,2002,1(3):195-199. 被引量:12
3陈洲溪.离子交换法从钨酸盐溶液中除钼新工艺已通过鉴定[J].中国钨业,1993,0(1):35-35. 被引量:2
4闫金龙.PID变参数函数在高炉顶压以及TRT前压控制中的应用[J].金属世界,2010(4):45-47. 被引量:1
5薛玉权,周云,李阳,梁晨.铁浴法处理不锈钢粉尘的研究[J].安徽工业大学学报:自然科学版,2015,32(3):206-211.
6余腾海,王心灵,王华南,温永长.新型树脂201-W对钨的交换容量[J].中国钨业,1995,0(10):15-16. 被引量:2
7杨景明,王娜伟,张洪丰,车海军.自动厚度控制系统变参数自适应控制方法及其实现[J].冶金自动化,2004(z1):596-598.
8田玉红,毛文洁,刘正西,霍杰.锰矿尾矿去除水中Cu^(2+)的实验研究[J].广西工学院学报,2001,12(3):50-52. 被引量:4
9朱晓萍.201×7树脂在钨冶炼中的应用研究[J].云南冶金,2013,42(4):26-29. 被引量:3
10胡兆瑞.离子交换法冶炼钨工艺的诞生和发展[J].中国钨业,1997,0(Z1):42-44. 被引量:11
Basic Information:
DOI:
Chinese Library Classification Number:TF804.3[冶金工程—有色金属冶金]
Citation Information:
The distributing rules of adsorbed ions in exchange column and the influencing factors during dynamic ion exchange are acquired through theoretical analysis.On the above basis,a novel idea of variable-parameter ion exchange and its principles are presented.The application of the variable-parameter ion exchange process in tungsten metallurgy proves its advantages.
quote
| GB/T 7714-2015 | [1] ZHAO Zhong-wei, FANG Qi, LI Hong-gui, et al. Principles of Variable-Parameter Ion Exchange and its Application in Tungsten Metallurgy[J]. Rare Metals and Cemented Carbides, 2010(3): 38-42. |
| MLA | [1] ZHAO Zhong-wei, et al., "Principles of Variable-Parameter Ion Exchange and its Application in Tungsten Metallurgy." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 38-42. |
| APA | [1] ZHAO Zhong-wei, FANG Qi, LI Hong-gui, HUO Guang-sheng, & CHEN Ai-liang. (2010). Principles of Variable-Parameter Ion Exchange and its Application in Tungsten Metallurgy. Rare Metals and Cemented Carbides(3), 38-42. |
| IEEE | [1] ZHAO Zhong-wei, FANG Qi, LI Hong-gui, HUO Guang-sheng, and CHEN Ai-liang, "Principles of Variable-Parameter Ion Exchange and its Application in Tungsten Metallurgy," Rare Metals and Cemented Carbides, no. 3, pp. 38-42, 2010. keywords: {variable-parameter ion exchange;adsorption rule;tungsten metallurgy} |