Preparation of Tungsten Electrode Used in Rare Earth Fused Salt Electrolysis AITranslate

The 52nd Research Institute of China Ordnance Industry;The 52nd Research Institute of China Ordnance Industry;The 52nd Research Institute of China Ordnance Industry;The 52nd Research Institute of China Ordnance Industry;The 52nd Research Institute of China Ordnance Industry
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tungsten powders coated by nickel were prepared with proper nickel compound as the raw material and corresponding addition method.Trace nickel can be coated evenly on the surface of tungsten powders.The above tungsten powders were used to produce compact tungsten rods by activated sintering.The tungsten rods were applied in rare earth electrolysis as the cathode of better corrosion resistance than traditional molybdenum cathode.The compact tungsten electrode of a relative density over 90% can be prepared by activated sintering at a temperature below 1 500 ℃ and using the tungsten powders coated with 0.4% nickel.The above tungsten electrode preparation process has the advantages of short flow,low production cost,and stable product quality.

KeyWords AITranslate

tungsten electrode nickel coating activated sintering

1有色金属提取冶金手册编辑委员会.稀有高熔点金属[M].北京:冶金工业出版社,1999.

2范景莲,曲选辉,黄伯云,李益民.高密度合金强化烧结工艺的研究[J].稀有金属材料与工程,1999,28(5):313-316. 被引量:22

3黄宁,黄建忠.镍的添加方式对钨基高密度合金显微组织和性能的影响[J].矿冶工程,1997,17(3):69-71. 被引量:1

4黄培云.粉末冶金原理(第2版)[M].北京:冶金工业出版社,2008.

1薛娟琴,郭忠源,唐长斌,毕强,张桀.熔盐液面上钨阴极快速腐蚀研究[J].热加工工艺,2015,44(2):88-92. 被引量:3

2夏念念,肖赛君,华中胜,赵卓,干正强,储向峰.低温熔盐中Al^(3+)在钨钼电极上的阴极电化学行为研究[J].轻金属,2016(5):17-22.

1徐明钟,饶宁,苏严.10kA稀土电解炉钨阴极堆焊技术研究[J].铜业工程,2018(1):77-79.

2兰兰,高平,贺新民,李鹏,王冬生,张志伟.钨阴极表面激光熔覆Ni60A合金涂层及其抗氧化性能研究[J].兵器材料科学与工程,2018,41(2):67-72. 被引量:1

3王权,王玉峰,王供绿.不同温度下钨金属在NdF3-LiF熔盐环境中的腐蚀行为研究[J].稀土,2019,40(4):95-101.

1Li,C,彭运湘.化学活化烧结加工后钨的性能[J].钨钼材料,1992(2):58-68.

2李有观.钨材或含钨合金制造新工艺[J].中国钨业,1999,14(3):37-39. 被引量:1

3杨扬,周美玲,李汉广.稀土元素La,Y对钨材显微组织和性能的影响[J].中南矿冶学院学报,1993,24(1):69-76. 被引量:4

4Bria.,CL,林文松.钨棒的解理断裂[J].国外稀有金属,1992(5):32-38.

5胡定坤.一种简便快速的钨棒修磨法[J].东方锅炉,1990(1):37-38.

6彭春禺.钨棒的氩弧钎接[J].焊接,1994(10):21-21.

7孔涛,熊惟皓,张志力,李小峰.镍包覆Y_2O_3颗粒弥散强化镍基高温合金的抗热腐蚀性能[J].机械工程材料,2013,37(11):43-48. 被引量:5

8侯玉柏,曾克里,尹春雷,许根国.水热氢还原制备镍包金刚石[J].矿冶,2006,15(3):38-40. 被引量:3

9何德孚,殷德余,赵建国,贾凤明.铈钨棒的氧化铈含量及其电极使用性能[J].稀有金属材料与工程,2003,32(6):475-477. 被引量:5

10何建勇.添加超细镍粉对铁基齿轮烧结工艺及性能的影响[J].粉末冶金技术,2006,24(5):369-372.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

Tungsten powders coated by nickel were prepared with proper nickel compound as the raw material and corresponding addition method.Trace nickel can be coated evenly on the surface of tungsten powders.The above tungsten powders were used to produce compact tungsten rods by activated sintering.The tungsten rods were applied in rare earth electrolysis as the cathode of better corrosion resistance than traditional molybdenum cathode.The compact tungsten electrode of a relative density over 90% can be prepared by activated sintering at a temperature below 1 500 ℃ and using the tungsten powders coated with 0.4% nickel.The above tungsten electrode preparation process has the advantages of short flow,low production cost,and stable product quality.

quote

GB/T 7714-2015 [1] JIA Gen-gui, LI Chang-lin, SUN Dong-ya, et al. Preparation of Tungsten Electrode Used in Rare Earth Fused Salt Electrolysis[J]. Rare Metals and Cemented Carbides, 2010(3): 43-45.
MLA [1] JIA Gen-gui, et al., "Preparation of Tungsten Electrode Used in Rare Earth Fused Salt Electrolysis." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 43-45.
APA [1] JIA Gen-gui, LI Chang-lin, SUN Dong-ya, ZHANG Tai-kang, & LV Ying. (2010). Preparation of Tungsten Electrode Used in Rare Earth Fused Salt Electrolysis. Rare Metals and Cemented Carbides(3), 43-45.
IEEE [1] JIA Gen-gui, LI Chang-lin, SUN Dong-ya, ZHANG Tai-kang, and LV Ying, "Preparation of Tungsten Electrode Used in Rare Earth Fused Salt Electrolysis," Rare Metals and Cemented Carbides, no. 3, pp. 43-45, 2010. keywords: {tungsten electrode;nickel coating;activated sintering}