Screwy microstructure of hydroxyapatite sheets of shank bone AITranslate

Chongqing University; Chongqing University; University of Western Australia; Chongqing University; Chongqing University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Scanning electron microscope (SEM) observation shows that a shank bone is a kind of bioceramic composite consisting of inorganic hydroxyapatite and organic collagen protein. The hydroxyapatite possesses laminated microstructure and the each hydroxyapatite layer is composed of numerous long and thin hydroxyapatite sheets. The hydroxyapatite sheets in an arbitrary hydroxyapatite layer make an almost fixed angle with the hydroxyapatite sheets in their adjacent hydroxyapatite layers which compose a kind of particular screwy microstructure. The maximum pullout energy of the screwy microstructure, which is closely related to the fracture toughness of the bone, is theoretically investigated and compared with that of the parallel microstructure of the sheets. It shows that the maximum pullout energy of the screwy microstructure is markedly larger than that of the parallel microstructure, which is experimentally verified.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.01.036

Chinese Library Classification Number:

Citation Information:

Scanning electron microscope (SEM) observation shows that a shank bone is a kind of bioceramic composite consisting of inorganic hydroxyapatite and organic collagen protein. The hydroxyapatite possesses laminated microstructure and the each hydroxyapatite layer is composed of numerous long and thin hydroxyapatite sheets. The hydroxyapatite sheets in an arbitrary hydroxyapatite layer make an almost fixed angle with the hydroxyapatite sheets in their adjacent hydroxyapatite layers which compose a kind of particular screwy microstructure. The maximum pullout energy of the screwy microstructure, which is closely related to the fracture toughness of the bone, is theoretically investigated and compared with that of the parallel microstructure of the sheets. It shows that the maximum pullout energy of the screwy microstructure is markedly larger than that of the parallel microstructure, which is experimentally verified.

quote

GB/T 7714-2015 [1] B. Chen, Q. Yuan, J.G. Wang, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.01.036.
MLA [1] B. Chen, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.01.036.
APA [1] B. Chen, Q. Yuan, J.G. Wang, X.J. Liao, & S.T. Sun. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.01.036
IEEE [1] B. Chen, Q. Yuan, J.G. Wang, X.J. Liao, and S.T. Sun, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.01.036.