Study on Nd-rich Phase Distribution and the Effect of Ultrasonic Vibration in Hot-Deformed Nd-Fe-B Magnet AITranslate
Abstract AITranslate
The morphology and distribution of Nd-rich phase during conventionally hot pressing,hot deformation and ultrasonic vibration-assisted hot deformation of Nd-Fe-B magnets were studied by SEM analysis and magnetic property test,and the effect of ultrasonic vibration on the magnetic properties of Nd-Fe-B magnets was also studied.The results show that part of the Nd-rich phases in the melt-spun ribbon of the magnet are squeezed into the gap of the melt-spun ribbon during the hot pressing process,and as the hot pressing temperature increases,an obvious blocky Nd-rich phase appears.During the hot deformation process,the melt-spun ribbon in the hot-pressed magnet deforms under the combined action of pressure and high temperature.Some Nd-rich phases in the melt-spun ribbon are further squeezed to the outside of the melt-spun ribbon,and some Nd-rich phases are enriched inside the melt-spun ribbon under the effect of pressure.After adding a certain amount of ultrasonic vibration during the hot deformation process,it is found that the number and area fraction of the blocky Nd-rich phase in the magnet significantly reduce,and the distribution of the Nd-rich phase becomes more uniform.Ultrasonic vibration can promote the diffusion movement of liquid Nd-rich phase,making it more difficult to enrich to form blocky Nd-rich phase,and improving the coercivity of the magnet.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
The morphology and distribution of Nd-rich phase during conventionally hot pressing,hot deformation and ultrasonic vibration-assisted hot deformation of Nd-Fe-B magnets were studied by SEM analysis and magnetic property test,and the effect of ultrasonic vibration on the magnetic properties of Nd-Fe-B magnets was also studied.The results show that part of the Nd-rich phases in the melt-spun ribbon of the magnet are squeezed into the gap of the melt-spun ribbon during the hot pressing process,and as the hot pressing temperature increases,an obvious blocky Nd-rich phase appears.During the hot deformation process,the melt-spun ribbon in the hot-pressed magnet deforms under the combined action of pressure and high temperature.Some Nd-rich phases in the melt-spun ribbon are further squeezed to the outside of the melt-spun ribbon,and some Nd-rich phases are enriched inside the melt-spun ribbon under the effect of pressure.After adding a certain amount of ultrasonic vibration during the hot deformation process,it is found that the number and area fraction of the blocky Nd-rich phase in the magnet significantly reduce,and the distribution of the Nd-rich phase becomes more uniform.Ultrasonic vibration can promote the diffusion movement of liquid Nd-rich phase,making it more difficult to enrich to form blocky Nd-rich phase,and improving the coercivity of the magnet.
quote
| GB/T 7714-2015 | [1] ZHU Ning-yuan, AO Fu-qiang, LI Zhi-qi. Study on Nd-rich Phase Distribution and the Effect of Ultrasonic Vibration in Hot-Deformed Nd-Fe-B Magnet[J]. Rare Metals and Cemented Carbides, 2025(5): 59-64. |
| MLA | [1] ZHU Ning-yuan, et al., "Study on Nd-rich Phase Distribution and the Effect of Ultrasonic Vibration in Hot-Deformed Nd-Fe-B Magnet." Rare Metals and Cemented Carbides, no. 5, 2025, pp. 59-64. |
| APA | [1] ZHU Ning-yuan, AO Fu-qiang, & LI Zhi-qi. (2025). Study on Nd-rich Phase Distribution and the Effect of Ultrasonic Vibration in Hot-Deformed Nd-Fe-B Magnet. Rare Metals and Cemented Carbides(5), 59-64. |
| IEEE | [1] ZHU Ning-yuan, AO Fu-qiang, and LI Zhi-qi, "Study on Nd-rich Phase Distribution and the Effect of Ultrasonic Vibration in Hot-Deformed Nd-Fe-B Magnet," Rare Metals and Cemented Carbides, no. 5, pp. 59-64, 2025. keywords: {ultrasonic vibration;Nd-Fe-B;Nd-rich phase;hot pressing;hot deformation;magnetic property} |